JP2007308353A - モルタルまたはコンクリートの処理方法およびセメント硬化体 - Google Patents
モルタルまたはコンクリートの処理方法およびセメント硬化体 Download PDFInfo
- Publication number
- JP2007308353A JP2007308353A JP2006141298A JP2006141298A JP2007308353A JP 2007308353 A JP2007308353 A JP 2007308353A JP 2006141298 A JP2006141298 A JP 2006141298A JP 2006141298 A JP2006141298 A JP 2006141298A JP 2007308353 A JP2007308353 A JP 2007308353A
- Authority
- JP
- Japan
- Prior art keywords
- concrete
- mortar
- curing agent
- treating
- film curing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】打設したモルタルまたはコンクリートが硬化した後、パラフィン系の塗膜養生剤を被覆するモルタルまたはコンクリートの処理方法であり、モルタルまたはコンクリートを打設した型枠を脱型する時に、パラフィン系の塗膜養生剤を被覆する前記処理方法であり、モルタルまたはコンクリートが高炉スラグを含有することが好ましく、パラフィン系の塗膜養生剤を1m2当たり50〜500g使用することが好ましい。さらに、前記コンクリートの処理方法で処理されたセメント硬化体である。
【選択図】なし
Description
また、本発明で云うセメント硬化体とは、モルタル、コンクリートの硬化体を総称したものである。
塗膜養生剤は、打設したモルタルまたはコンクリートが硬化した後に施すことが好ましい。従来の使用法のように、硬化前に塗布したのでは、本発明の効果、すなわち、中性化の抑制効果や塩化物イオンの浸透抑制効果は得られない。ここで、硬化とは、モルタルまたはコンクリートが凝結(JIS A 1147)した時点を意味する。
また、モルタルまたはコンクリートが凝結する前に塗膜養生剤を被覆した場合には、本発明のひび割れ低減効果は得られない。撒水などの水に関する養生が終了後、できるだけ早い時期に被覆することがひび割れ低減効果を得るために望ましい。モルタルまたはコンクリートを打設した型枠の脱型時に塗膜養生剤を塗膜すると、脱型作業の人手で並行して行うことができ新たな工数を必要とせず工事費の増加を抑えることができる他、型枠を脱型した直後に塗膜すれば乾燥収縮を最大限に抑制できる。
セメントA:市販の普通ポルトランドセメント
セメントB:市販の高炉セメントB種
細骨材:新潟県姫川産、比重2.62
塗膜養生剤A:ポゾリス物産社製商品名「マスターキュア」、パラフィン系
塗膜養生剤B:市販のEVA系塗膜養生剤
水:水道水
ひび割れ抵抗性試験:1m2当たり、2本を超えてひび割れが発生した場合は×、ひび割れが1〜2本発生した場合は△、ひび割れの発生がない場合は○とした。
中性化試験:材齢14日まで20℃の水中養生を行った後、30℃、相対湿度60%、CO2濃度5%の環境で4週間養生した。硬化体を切断し、断面にフェノールフタレインの1%アルコール溶液を噴霧して赤変しなかった部分を中性化部分と見なして中性化深さを測定した。
塩化物イオンの浸透抵抗性試験(JIS A 1171):材齢14日まで20℃の水中養生を行った後、擬似海水に4週間浸漬した。硬化体を切断し、硝酸銀-フルオロセイオン法によって塩化物イオンの浸透深さを測定した。
粗骨材:市販の粗骨材、Gmax25mm
Claims (5)
- 打設したモルタルまたはコンクリートが硬化した後、パラフィン系の塗膜養生剤を被覆することを特徴とするモルタルまたはコンクリートの処理方法。
- モルタルまたはコンクリートを打設した型枠を脱型する時に、パラフィン系の塗膜養生剤を被覆することを特徴とする請求項1記載のモルタルまたはコンクリートの処理方法。
- モルタルまたはコンクリートが高炉スラグを含有することを特徴とする請求項1または2に記載のモルタルまたはコンクリートの処理方法。
- パラフィン系の塗膜養生剤を1m2当たり50〜500g使用することを特徴とする請求項1〜3のいずれか1項に記載のモルタルまたはコンクリートの処理方法。
- 請求項1〜4のいずれか1項に記載のモルタルまたはコンクリートの処理方法で処理されたセメント硬化体。