JP2006134761A - 二次電池 - Google Patents
二次電池 Download PDFInfo
- Publication number
- JP2006134761A JP2006134761A JP2004324000A JP2004324000A JP2006134761A JP 2006134761 A JP2006134761 A JP 2006134761A JP 2004324000 A JP2004324000 A JP 2004324000A JP 2004324000 A JP2004324000 A JP 2004324000A JP 2006134761 A JP2006134761 A JP 2006134761A
- Authority
- JP
- Japan
- Prior art keywords
- negative electrode
- active material
- electrode active
- positive electrode
- secondary battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
【解決手段】 帯状の正極と負極22とがセパレータを介して巻回されている。負極22は、負極集電体22Aが負極活物質層22Bで覆われた被覆領域22Cを有する。この被覆領域22Cの1回以上の充電を行った後の巻回方向における破断までの伸び率は、3%以上である。負極活物質の膨張により負極集電体22Aに亀裂や破断が生じることを防止し、サイクル特性を向上させる。被覆領域22Cの1回以上の充電を行った後の破断までの伸び率が16%以下であることが好ましい。
【選択図】 図3
Description
ディ.ラーチャー(D. Larcher)著「ジャーナル オブ ジ エレクトロケミカル ソサエティ(Journal of The Electrochemical Society)」、2000年、5巻、第147号、p1658-1662
上記実施の形態で説明した二次電池を作製した。まず、炭酸リチウム(Li2 CO3 )と炭酸コバルト(CoCO3 )とを、Li2 CO3 :CoCO3 =0.5:1(モル比)の割合で混合し、空気中において900℃で5時間焼成して、正極活物質としてのリチウム・コバルト複合酸化物(LiCoO2 )を得た。次いで、このリチウム・コバルト複合酸化物91質量部と、導電剤であるグラファイト6質量部と、結着剤であるポリフッ化ビニリデン3質量部とを混合して正極合剤を調整した。続いて、この正極合剤を溶剤であるN−メチル−2−ピロリドンに分散させて正極合剤スラリーとし、厚み20μmのアルミニウム箔よりなる正極集電体21Aの両面に均一に塗布して乾燥させ、ロールプレス機で圧縮成型して正極活物質層21Bを形成し正極21を作製した。続いて、正極集電体21Aの一端にアルミニウム製の正極リード25を取り付けた。
破断までの伸び率(%)=[(L−L0 )/L0 ]×100
(数1において、Lは標点間距離、L0 は破断する前の標点間距離をそれぞれ表す。)
負極活物質として、実施例2−1では実施例1−1〜1−4と同一の材料、実施例2−2ではCo0.44Sn0.56、実施例2−3ではMg2 Siを用いたことを除き、他は実施例1−2と同様にして二次電池を作製した。
Claims (4)
- 帯状の正極集電体の面上に正極活物質層を有する正極と、帯状の負極集電体の面上に負極活物質層を有する負極とを積層し、巻回した巻回体を備え、
前記負極は、電極反応物質を吸蔵および放出することが可能であり、構成元素として金属元素および半金属元素のうちの少なくとも1種を含む負極活物質を含み、
且つ、前記負極は、前記負極集電体が前記負極活物質層により覆われた被覆領域を有し、前記被覆領域の1回以上の充電を行った後の巻回方向における破断までの伸び率が3%以上である
ことを特徴とする二次電池。 - 前記被覆領域の破断までの伸び率が16%以下であることを特徴とする請求項1記載の二次電池。
- 前記負極は、前記負極活物質として、スズ(Sn)およびケイ素(Si)のうちの少なくとも一方を構成元素として含む材料を含むことを特徴とする請求項1記載の二次電池。
- 前記負極は、前記負極活物質として、スズと、コバルト(Co)と、炭素(C)とを構成元素として含み、炭素の含有量が9.9質量%以上29.7質量%以下であり、かつスズとコバルトとの合計に対するコバルトの割合が30質量%以上70質量%以下であるCoSnC含有材料を含むことを特徴とする請求項1記載の二次電池。