JP2000248391A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2000248391A5 JP2000248391A5 JP1999339125A JP33912599A JP2000248391A5 JP 2000248391 A5 JP2000248391 A5 JP 2000248391A5 JP 1999339125 A JP1999339125 A JP 1999339125A JP 33912599 A JP33912599 A JP 33912599A JP 2000248391 A5 JP2000248391 A5 JP 2000248391A5
- Authority
- JP
- Japan
- Prior art keywords
- metal surface
- caustic
- thermal barrier
- aqueous
- barrier coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000000034 method Methods 0.000 description 11
- 229910052751 metal Inorganic materials 0.000 description 9
- 239000002184 metal Substances 0.000 description 9
- 239000003518 caustics Substances 0.000 description 8
- 239000012720 thermal barrier coating Substances 0.000 description 7
- HEMHJVSKTPXQMS-UHFFFAOYSA-M Sodium hydroxide Chemical compound [OH-].[Na+] HEMHJVSKTPXQMS-UHFFFAOYSA-M 0.000 description 6
- 229910000907 nickel aluminide Inorganic materials 0.000 description 6
- 239000007864 aqueous solution Substances 0.000 description 4
- 239000000243 solution Substances 0.000 description 4
- NPXOKRUENSOPAO-UHFFFAOYSA-N Raney nickel Chemical compound [Al].[Ni] NPXOKRUENSOPAO-UHFFFAOYSA-N 0.000 description 3
- QVGXLLKOCUKJST-UHFFFAOYSA-N atomic oxygen Chemical compound [O] QVGXLLKOCUKJST-UHFFFAOYSA-N 0.000 description 3
- PCLURTMBFDTLSK-UHFFFAOYSA-N nickel platinum Chemical compound [Ni].[Pt] PCLURTMBFDTLSK-UHFFFAOYSA-N 0.000 description 3
- 239000001301 oxygen Substances 0.000 description 3
- 229910052760 oxygen Inorganic materials 0.000 description 3
- 239000011248 coating agent Substances 0.000 description 2
- 238000000576 coating method Methods 0.000 description 2
- 238000010438 heat treatment Methods 0.000 description 2
- 239000000203 mixture Substances 0.000 description 2
- 229910000951 Aluminide Inorganic materials 0.000 description 1
- 239000012300 argon atmosphere Substances 0.000 description 1
- 239000012298 atmosphere Substances 0.000 description 1
- 230000015572 biosynthetic process Effects 0.000 description 1
- 238000005524 ceramic coating Methods 0.000 description 1
- 239000012299 nitrogen atmosphere Substances 0.000 description 1
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US09/210,655 US6146692A (en) | 1998-12-14 | 1998-12-14 | Caustic process for replacing a thermal barrier coating |
| US09/210655 | 1998-12-14 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2000248391A JP2000248391A (ja) | 2000-09-12 |
| JP2000248391A5 true JP2000248391A5 (enExample) | 2007-01-18 |
| JP4954357B2 JP4954357B2 (ja) | 2012-06-13 |
Family
ID=22783734
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP33912599A Expired - Lifetime JP4954357B2 (ja) | 1998-12-14 | 1999-11-30 | 苛性アルカリプロセス |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US6146692A (enExample) |
| EP (1) | EP1010776B1 (enExample) |
| JP (1) | JP4954357B2 (enExample) |
| KR (1) | KR100652993B1 (enExample) |
| CZ (1) | CZ293386B6 (enExample) |
| DE (1) | DE69924590T2 (enExample) |
| TW (1) | TW548345B (enExample) |
Families Citing this family (30)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6203847B1 (en) * | 1998-12-22 | 2001-03-20 | General Electric Company | Coating of a discrete selective surface of an article |
| US6158957A (en) * | 1998-12-23 | 2000-12-12 | United Technologies Corporation | Thermal barrier removal process |
| US6243948B1 (en) * | 1999-11-18 | 2001-06-12 | General Electric Company | Modification and repair of film cooling holes in gas turbine engine components |
| US6305077B1 (en) * | 1999-11-18 | 2001-10-23 | General Electric Company | Repair of coated turbine components |
| KR20010062316A (ko) * | 1999-12-14 | 2001-07-07 | 제이 엘. 차스킨, 버나드 스나이더, 아더엠. 킹 | 금속 기판내의 통로 구멍으로부터 피복물을 제거하는방법, 및 이와 관련된 제품 |
| EP1251191B1 (en) | 2001-04-21 | 2004-06-02 | ALSTOM Technology Ltd | A method of repairing a ceramic coating |
| US6571472B2 (en) * | 2001-08-14 | 2003-06-03 | General Electric Company | Restoration of thickness to load-bearing gas turbine engine components |
| US20030101587A1 (en) * | 2001-10-22 | 2003-06-05 | Rigney Joseph David | Method for replacing a damaged TBC ceramic layer |
| US7090393B2 (en) * | 2002-12-13 | 2006-08-15 | General Electric Company | Using thermal imaging to prevent loss of steam turbine efficiency by detecting and correcting inadequate insulation at turbine startup |
| US20070023142A1 (en) * | 2002-12-19 | 2007-02-01 | Lagraff John R | Airfoil refurbishment method |
| US20050035086A1 (en) * | 2003-08-11 | 2005-02-17 | Chen Keng Nam | Upgrading aluminide coating on used turbine engine component |
| US20050127039A1 (en) * | 2003-12-16 | 2005-06-16 | General Electric Company | Process for removing adherent oxide particles from an aluminized surface |
| US6878215B1 (en) | 2004-05-27 | 2005-04-12 | General Electric Company | Chemical removal of a metal oxide coating from a superalloy article |
| US7666515B2 (en) * | 2005-03-31 | 2010-02-23 | General Electric Company | Turbine component other than airfoil having ceramic corrosion resistant coating and methods for making same |
| US20070039175A1 (en) * | 2005-07-19 | 2007-02-22 | General Electric Company | Methods for repairing turbine engine components |
| DE102005045839A1 (de) * | 2005-09-24 | 2007-04-12 | Mtu Aero Engines Gmbh | Verfahren zum Reinigen von Hohlräumen an Gasturbinenbauteilen |
| US8267662B2 (en) * | 2007-12-13 | 2012-09-18 | General Electric Company | Monolithic and bi-metallic turbine blade dampers and method of manufacture |
| US20100224602A1 (en) * | 2009-03-06 | 2010-09-09 | General Electric Company | Method and system for removing thermal barrier coating |
| TW201120249A (en) * | 2009-07-31 | 2011-06-16 | Sinryo Corp | Method for removal of hard coating film in superhard material, and method for production of superhard material |
| EP2524062B1 (en) * | 2010-01-11 | 2018-11-28 | Kolene Corporation | Metal surface scale conditioning method and apparatus thereof |
| US20120328445A1 (en) * | 2011-06-27 | 2012-12-27 | United Technologies Corporation | Grit blast free thermal barrier coating rework |
| US8956700B2 (en) | 2011-10-19 | 2015-02-17 | General Electric Company | Method for adhering a coating to a substrate structure |
| GB201318873D0 (en) * | 2013-10-25 | 2013-12-11 | Rolls Royce Plc | Thermal barrier coating removal process |
| US9334549B2 (en) | 2013-12-20 | 2016-05-10 | General Electric Company | Systems and methods for recovery of rare-earth constituents from environmental barrier coatings |
| US9409185B2 (en) | 2014-04-17 | 2016-08-09 | General Electric Company | Systems and methods for recovery of rare-earth constituents from environmental barrier coatings |
| CN105420744A (zh) * | 2015-11-20 | 2016-03-23 | 沈阳黎明航空发动机(集团)有限责任公司 | 一种涡轮叶片热障涂层陶瓷面层去除方法 |
| US9803139B1 (en) | 2016-06-24 | 2017-10-31 | General Electric Company | Process for removing aluminum-silicon coatings from metallic structures, and related processes for preparing magnetic components |
| GB201903484D0 (en) | 2019-03-14 | 2019-05-01 | Rolls Royce Plc | A method of removing a ceramic coating from a ceramic coated metallic article |
| US11926880B2 (en) | 2021-04-21 | 2024-03-12 | General Electric Company | Fabrication method for a component having magnetic and non-magnetic dual phases |
| US11661646B2 (en) | 2021-04-21 | 2023-05-30 | General Electric Comapny | Dual phase magnetic material component and method of its formation |
Family Cites Families (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3833414A (en) * | 1972-09-05 | 1974-09-03 | Gen Electric | Aluminide coating removal method |
| US4141781A (en) * | 1977-10-06 | 1979-02-27 | General Electric Company | Method for rapid removal of cores made of βAl2 O3 from directionally solidified eutectic and superalloy and superalloy materials |
| US4317685A (en) * | 1980-06-06 | 1982-03-02 | General Electric Company | Method for removing a scale from a superalloy surface |
| US4439241A (en) * | 1982-03-01 | 1984-03-27 | United Technologies Corporation | Cleaning process for internal passages of superalloy airfoils |
| US5507306A (en) * | 1993-12-23 | 1996-04-16 | Howmet Corporation | Cleaning apparatus and method for cleaning internal airfoil cooling passages |
| US5575858A (en) * | 1994-05-02 | 1996-11-19 | United Technologies Corporation | Effective cleaning method for turbine airfoils |
| US5678583A (en) * | 1995-05-22 | 1997-10-21 | Howmet Research Corporation | Removal of ceramic shell mold material from castings |
| DE69615517T2 (de) * | 1995-12-22 | 2002-05-16 | General Electric Co., Schenectady | Körper mit Hochtemperatur-Schutzschicht und Verfahren zum Beschichten |
| US5643474A (en) * | 1995-12-26 | 1997-07-01 | General Electric Company | Thermal barrier coating removal on flat and contoured surfaces |
| US5972424A (en) * | 1998-05-21 | 1999-10-26 | United Technologies Corporation | Repair of gas turbine engine component coated with a thermal barrier coating |
-
1998
- 1998-12-14 US US09/210,655 patent/US6146692A/en not_active Expired - Lifetime
-
1999
- 1999-11-05 DE DE69924590T patent/DE69924590T2/de not_active Expired - Lifetime
- 1999-11-05 EP EP99309006A patent/EP1010776B1/en not_active Expired - Lifetime
- 1999-11-30 JP JP33912599A patent/JP4954357B2/ja not_active Expired - Lifetime
- 1999-12-01 TW TW088121007A patent/TW548345B/zh not_active IP Right Cessation
- 1999-12-13 KR KR1019990057070A patent/KR100652993B1/ko not_active Expired - Fee Related
- 1999-12-14 CZ CZ19994541A patent/CZ293386B6/cs not_active IP Right Cessation
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2000248391A5 (enExample) | ||
| JP2002038283A5 (enExample) | ||
| JP2004525254A5 (enExample) | ||
| JP3027005B2 (ja) | 腐食した超合金または耐熱鋼製部材の再研磨方法および再研磨された部材 | |
| JP4954357B2 (ja) | 苛性アルカリプロセス | |
| US20070056709A1 (en) | Method for casting core removal | |
| CN113939095B (zh) | 一种陶瓷覆铜板及其制备方法 | |
| CA2370256A1 (en) | Method for refurbishing a coating including a thermally grown oxide | |
| EP1013798A3 (en) | Thermal barrier coating removal process | |
| CA2553857A1 (en) | A method of restoring catalytic activity of a spent hydroprocessing catalyst, a spent hydroprocessing catalyst having restored catalytic activity and a hydroprocessing process | |
| JP2007535697A5 (enExample) | ||
| AU2002311057A1 (en) | Method for obtaining pioglitazone as an antidiabetic agent | |
| JPS60500944A (ja) | 使用済み触媒溶液および付随洗浄水からのパラジウム−スズ系無電解めっき触媒の再生 | |
| DE59102130D1 (de) | Verfahren zur herstellung eines beschichteten hartmetallschneidkörpers. | |
| JP2003017837A5 (enExample) | ||
| JPS61136999A (ja) | 汚染アルミニウム含有ステンレススチールホイル上における酸化物ホイスカーの成長 | |
| JP4824163B2 (ja) | 硬質材層を除去するための方法 | |
| US4960647A (en) | Process for the reactive treating of palladium to form a protective coating and article | |
| CN110318061A (zh) | 铝合金氧化膜的去除方法 | |
| JPS60224792A (ja) | 加工材料上のアルミニウム分散層を化学的に除去する方法 | |
| JP2000176284A (ja) | アンモニア合成触媒の製造方法および同方法で得られた触媒 | |
| JPH05503320A (ja) | チタン化合物を基材金属から剥離するための剥離溶液及び方法 | |
| CN87101136A (zh) | 穿孔顶头的热处理方法 | |
| WO2007018158A1 (ja) | イオン窒化処理方法 | |
| CN114540806B (zh) | 一种铝合金钝化膜处理方法 |