GB2178682A - Electric-resistance seam-welding method - Google Patents
Electric-resistance seam-welding methodInfo
- Publication number
- GB2178682A GB2178682A GB08612297A GB8612297A GB2178682A GB 2178682 A GB2178682 A GB 2178682A GB 08612297 A GB08612297 A GB 08612297A GB 8612297 A GB8612297 A GB 8612297A GB 2178682 A GB2178682 A GB 2178682A
- Authority
- GB
- United Kingdom
- Prior art keywords
- steel plate
- electric
- welding method
- resistance seam
- thickness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
This electric-resistance seam-welding method for welding difficult-to-weld steel plate suppresses the generation of burrs. The steel plate has coating layers of a metal harder than tin and an intermetallic compound. The thickness of the steel plate is not more than 0.5 mm. The overlap width of the steel plate is greater than 2.0 times the plate thickness, but is less than 2.4 times the plate thickness. The weldable current range of steel plate can be increased by this means.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP58103886A JPS59229290A (en) | 1983-06-10 | 1983-06-10 | Electric resistance seam welding method |
PCT/JP1984/000583 WO1986003442A1 (en) | 1983-06-10 | 1984-12-10 | Electric-resistance seam-welding method |
Publications (3)
Publication Number | Publication Date |
---|---|
GB8612297D0 GB8612297D0 (en) | 1986-06-25 |
GB2178682A true GB2178682A (en) | 1987-02-18 |
GB2178682B GB2178682B (en) | 1988-11-02 |
Family
ID=26425084
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB08612297A Expired GB2178682B (en) | 1983-06-10 | 1984-12-10 | Electric resistance seam welding method |
Country Status (5)
Country | Link |
---|---|
JP (1) | JPS59229290A (en) |
CH (1) | CH668930A5 (en) |
DE (1) | DE3490793T1 (en) |
GB (1) | GB2178682B (en) |
WO (1) | WO1986003442A1 (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0761368A1 (en) * | 1995-08-09 | 1997-03-12 | Elpatronic Ag | Welding method for coated sheets, especially tin-plated sheets |
EP0802011A2 (en) * | 1996-04-19 | 1997-10-22 | Elpatronic Ag | Method for joining two metal foils |
WO1998026897A1 (en) * | 1996-12-16 | 1998-06-25 | Carnaudmetalbox Plc | Measurement of welds |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6092088A (en) * | 1983-10-24 | 1985-05-23 | Nippon Kokan Kk <Nkk> | Electric resistance seam welding method |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB2056349A (en) * | 1979-08-06 | 1981-03-18 | Toyo Seikan Kaisha Ltd | Method and apparatus of making welded metallic can bodies and an improvement in welded can bodies |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE2532976B2 (en) * | 1975-03-19 | 1978-03-23 | Opprecht, Paul, Bergdietikon, Aargau (Schweiz) | Device for the semi or fully automatic electrical resistance longitudinal seam welding of can bodies |
JPS5623389A (en) * | 1979-08-06 | 1981-03-05 | Toyo Seikan Kaisha Ltd | Production of tin-free steel welded can barrel |
JPS57174468A (en) * | 1981-04-18 | 1982-10-27 | Hokkai Can Co Ltd | Welded can body |
-
1983
- 1983-06-10 JP JP58103886A patent/JPS59229290A/en active Granted
-
1984
- 1984-12-10 CH CH3144/86A patent/CH668930A5/en not_active IP Right Cessation
- 1984-12-10 DE DE19843490793 patent/DE3490793T1/de not_active Ceased
- 1984-12-10 GB GB08612297A patent/GB2178682B/en not_active Expired
- 1984-12-10 WO PCT/JP1984/000583 patent/WO1986003442A1/en active Application Filing
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB2056349A (en) * | 1979-08-06 | 1981-03-18 | Toyo Seikan Kaisha Ltd | Method and apparatus of making welded metallic can bodies and an improvement in welded can bodies |
Non-Patent Citations (1)
Title |
---|
JP, B2, 57-33110 * |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0761368A1 (en) * | 1995-08-09 | 1997-03-12 | Elpatronic Ag | Welding method for coated sheets, especially tin-plated sheets |
US5841094A (en) * | 1995-08-09 | 1998-11-24 | Elpatronic Ag | Method and apparatus for resistance welding coated sheet metal |
EP0802011A2 (en) * | 1996-04-19 | 1997-10-22 | Elpatronic Ag | Method for joining two metal foils |
EP0802011A3 (en) * | 1996-04-19 | 1998-02-04 | Elpatronic Ag | Method for joining two metal foils |
US6011236A (en) * | 1996-04-19 | 2000-01-04 | Elpatronic Ag | Method and apparatus for joining two metal foils together |
WO1998026897A1 (en) * | 1996-12-16 | 1998-06-25 | Carnaudmetalbox Plc | Measurement of welds |
Also Published As
Publication number | Publication date |
---|---|
JPS59229290A (en) | 1984-12-22 |
CH668930A5 (en) | 1989-02-15 |
GB8612297D0 (en) | 1986-06-25 |
DE3490793T1 (en) | 1987-01-29 |
GB2178682B (en) | 1988-11-02 |
WO1986003442A1 (en) | 1986-06-19 |
JPS6324795B2 (en) | 1988-05-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB2178682A (en) | Electric-resistance seam-welding method | |
JPS549132A (en) | Method of welding laminated sheed metals | |
KR840002679A (en) | Liner method and clad parts using clad parts | |
DE3362678D1 (en) | Method for the welding of internally clad cylindrical work pieces | |
JPS5548479A (en) | Arc welding method | |
JPS57149068A (en) | Mig welding method | |
JPS57181774A (en) | Welding method for copper or copper alloy clad steel plate | |
JPS5452648A (en) | Friction welding method for dissimilar metals | |
GB2012645A (en) | Improving spot weld penetration in metal sheets | |
JPS53106361A (en) | Submerged arc welding method for steel plate | |
GB2104428A (en) | Method of electric-arc welding of reservoirs for agressive mediums | |
JPS5794473A (en) | Arc spot welding method | |
JPS56105878A (en) | Production of corrosion-resistant welded can | |
JPS56158278A (en) | Vertical narrow groove welding of aluminum alloy thick plate | |
JPS57190786A (en) | Projection welding method | |
JPS5768289A (en) | Arc welding method | |
JPH09136161A (en) | Arc spot welding method | |
JPS574389A (en) | Welding method for aluminum material | |
JPS56158277A (en) | Vertical narrow groove welding for aluminum alloy thick plate | |
SEXTON et al. | THE SUBMERGED ARC, STRIP CLADDING OF MILD STEEL, WITH COPPER AND COPPER ALLOYS | |
JPS53138946A (en) | Sealing method by welding | |
JPS56131078A (en) | Method of arc welding between copper and carbon steel and coated arc welding bar used for this method | |
JPS54132448A (en) | Welding method for copper or copper alloy parts and ferro or nickel alloy parts | |
JPS57127580A (en) | Rust preventive method of seam weld zone | |
JPS5372751A (en) | Spot welding method of zinc plated steel plate |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PCNP | Patent ceased through non-payment of renewal fee |