ES351660A1 - Improved Sintered Alloys - Google Patents
Improved Sintered AlloysInfo
- Publication number
- ES351660A1 ES351660A1 ES351660A ES351660A ES351660A1 ES 351660 A1 ES351660 A1 ES 351660A1 ES 351660 A ES351660 A ES 351660A ES 351660 A ES351660 A ES 351660A ES 351660 A1 ES351660 A1 ES 351660A1
- Authority
- ES
- Spain
- Prior art keywords
- sintered alloys
- improved sintered
- alloys
- air
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
A sintered steel alloy comprises TiC 27 - 35% (containing less than 0À1% free carbon) Ni 4À8 - less than 26% Cr present up to 15À6%. such that Ni + Cr = 12-26% and Cr is up to 60% of Ni + Cr. N up to 0À04% B up to 0À01% and Zr up to 0À05% the balance, apart from impurities and incidental elements, being iron. The alloys may be solution treated at 820 - 860 C., air cooled, machined to final shape and aged at 480 C. followed by quenching in air.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE1966D0050371 DE1257440B (en) | 1966-06-23 | 1966-06-23 | Highly wear-resistant, machinable and hardenable sintered steel alloy and process for the production of this alloy |
DED0052539 | 1967-03-16 |
Publications (1)
Publication Number | Publication Date |
---|---|
ES351660A1 true ES351660A1 (en) | 1969-06-01 |
Family
ID=7054253
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES351660A Expired ES351660A1 (en) | 1966-06-23 | 1968-03-15 | Improved Sintered Alloys |
Country Status (5)
Country | Link |
---|---|
DE (1) | DE1558477B1 (en) |
ES (1) | ES351660A1 (en) |
FR (1) | FR93627E (en) |
GB (1) | GB1165491A (en) |
SE (1) | SE333250B (en) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE2652509C2 (en) * | 1976-11-18 | 1978-11-02 | Thyssen Edelstahlwerke Ag, 4000 Duesseldorf | Use of a hard alloy for tool and wear parts |
US4173471A (en) * | 1978-01-27 | 1979-11-06 | Chromalloy American Corporation | Age-hardenable titanium carbide tool steel |
JP6378717B2 (en) | 2016-05-19 | 2018-08-22 | 株式会社日本製鋼所 | Iron-based sintered alloy and method for producing the same |
-
1967
- 1967-03-16 DE DE19671558477 patent/DE1558477B1/en not_active Withdrawn
- 1967-12-07 FR FR131278A patent/FR93627E/en not_active Expired
- 1967-12-12 SE SE1706267A patent/SE333250B/en unknown
-
1968
- 1968-02-05 GB GB569368A patent/GB1165491A/en not_active Expired
- 1968-03-15 ES ES351660A patent/ES351660A1/en not_active Expired
Also Published As
Publication number | Publication date |
---|---|
GB1165491A (en) | 1969-10-01 |
DE1558477B1 (en) | 1970-04-23 |
FR93627E (en) | 1969-04-25 |
SE333250B (en) | 1971-03-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1157163A (en) | Copper-Zirconium Alloy | |
GB1301238A (en) | ||
GB1361055A (en) | Ioron-nickel-chromium alloys | |
GB1132990A (en) | Iron base alloy | |
GB1085715A (en) | Vehicle brake | |
GB1356734A (en) | Alpha-beta type titanium base alloys | |
GB1135003A (en) | Nickel-chromium-iron alloys | |
ES351660A1 (en) | Improved Sintered Alloys | |
GB911631A (en) | Alloys | |
GB1330543A (en) | Iron-cobalt-vanadium alloy | |
GB914770A (en) | Alloys | |
GB1320775A (en) | Nickel base alloys | |
GB1194568A (en) | Improvements in or relating to Magnetic Alloy Materials and Their Manufacture | |
GB1089934A (en) | High strength steel alloy composition | |
GB1095925A (en) | Hafnium alloys | |
GB1222385A (en) | Heat-treatment of ultra-high-tensile steel | |
GB1151178A (en) | Chromium-Iron-Nickel Alloys when used in Corrosive Atmospheres | |
GB1362209A (en) | Aluminium products | |
GB1029184A (en) | Improvements in or relating to high strength stainless steel | |
GB1317211A (en) | Heat treatable alloy | |
GB1020423A (en) | Improvements in or relating to free machining steel | |
GB1065863A (en) | Improvements in or relating to copper alloys | |
ES344725A1 (en) | Ultra hard cobalt-molybdenum-iron alloys | |
GB946642A (en) | Process for the production of nodular cast iron | |
ES300039A1 (en) | Ductile corrosion-resistant alloy |