DE963472C - Verfahren zum Weichmachen von Polystyrol - Google Patents
Verfahren zum Weichmachen von PolystyrolInfo
- Publication number
- DE963472C DE963472C DES38930A DES0038930A DE963472C DE 963472 C DE963472 C DE 963472C DE S38930 A DES38930 A DE S38930A DE S0038930 A DES0038930 A DE S0038930A DE 963472 C DE963472 C DE 963472C
- Authority
- DE
- Germany
- Prior art keywords
- polystyrene
- plasticizing
- moles
- added
- orthosilicate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zum Weichmachen von Polystyrol Die Erfindung betrifft ein Verfahren zum Weichmachen von Polystyrol. Erfindungsgemäß werden zum Weichmachen Orthokieselsäureester verwendet, die pro Siliciumatom mindestens eine Cyclohexylphenoxygruppe enthalten.
- Die Erfindung wird an Hand von Beispielen erläutert.
- Beispiel I 150 g Polystyrol vom K-Werte 70 werden in 1000 g Trichloräthylen gelöst und 50 g o-Cyclohexylphenylorthosilikat zugegeben. Nach dessen Auflösung in dev Polystyrollösung ist die Mischung gebrauchsfertig. Sie kann zur Herstellung von Folien im Gießverfahren oder zur Herstellung geschmeidiger Schutzüberzüge dienen.
- Beispiel 2 150 g Polystyrol werden in 1000 g Trichloräthylen gelöst und dazu 30 g eines. Umesterungsproduktes gegeben, das aus 1 Mol Äthylorthosilikat und 3 Mol o-Cyclohexylphenol hergestellt wurde. Nach Auflösen des Umesterungsproduktes in der Polystyrollösung ist die Mischung gebrauchsfertig.
- Weichgemachtes Polystyrol kann in der gleichen Weise verwendet werden wie andere weichgemachte Polyplaste. Man kann sie für die Folienherstellung, zum Pressen, Spritzen, auch zur Faserlerstellung benutzen. Insbesondere eignet sich auch Polystyrol als Isolier- und Distanzstoff für elektrotechnische Zwecke. So kann man z. B. Bänder aus weichgemachter Polystyrolfolie zum Umspinnen von Drähten verwenden, oder man kann in sonstiger Weise Drähte in solche Folien einhüllen.
- Gegenüber einem bekannten Verfahren, bei dem Polykieselsäureester mit unterschiedlichen organischen Resten als Weichmacher für Vinylderivate verwendet werden, bietet die Erfindung den Vorteil, daß der Weichmachereffekt bei Orthoestern wesentlich größer ist als bei Polyestern, da letztere räumlich vernetzte Gebilde darstellen, auch lassen sich Orthoester leicht reproduzierbar als definierte Verbindungen herstellen, während dies bei Polyestern nicht möglich ist. Orthoester mit Cyclohexylphenoxygruppen sind auch wegen der Größe dieser Gruppen hydrolytisch nicht leicht spaltbar.
Claims (3)
- P A T E N T A N S P R Ü C H E: 1. Verfahren zum Weichmachen von Polystyrol, dadurch gekennzeichnet, daß als Weichmacher ein Orthokieselsäureester verwendet wird, der pro Siliciumatom mindestens eine Cydohexylpbenoxygruppe enthält.
- 2. Verfahren nach Anspruch I, dadurch gekennzeichnet, daß Polystyrol in gelöster Form etwa 25 Gewichtsprozent o-Cyclohexylphenylorthosilikat beigemischt wird.
- 3. Verfahren nach Anspruchs, dadurch gekennzeichnet, daß Polystyrol in gelöster Form etwa 20% eines Umesterungsproduktes beigemischt wird, das aus I Mol Äthylorthosilikat und 3 Mol o-Cyclohexylphenol hergestellt wird.In Betracht gezogene Druckschriften USA.-Patentschrift Nr. 2 507 422.