DE357150C - Verfahren zur Herstellung eines Elektrolyten fuer Primaerelemente - Google Patents
Verfahren zur Herstellung eines Elektrolyten fuer PrimaerelementeInfo
- Publication number
- DE357150C DE357150C DEV15642D DEV0015642D DE357150C DE 357150 C DE357150 C DE 357150C DE V15642 D DEV15642 D DE V15642D DE V0015642 D DEV0015642 D DE V0015642D DE 357150 C DE357150 C DE 357150C
- Authority
- DE
- Germany
- Prior art keywords
- electrolyte
- primary elements
- production
- percent
- alum
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Herstellung eines Elektrolyten für Primärelemente. Es ist bereits ein Elektrolyt für Primärelemente bekannt, welcher aus einer Lösung von Steinsalz und Alaun besteht.
- Angestellte Versuche haben nun gezeigt, daß, wenn diesem Salzgemisch noch schwefelsaures Zink zugesetzt wird, eine länger andauernde und gleichmäßigere (weniger-abnehmende) Stromentwicklung erzielt wird.
- Der Elektrolytstoff nach der vorliegenden Erfindung besteht aus einem Gemisch von Steinsalz, Alaun und schwefelsaurem Zink, und zwar zweckmäßig nach der folgenden Zusammensetzung: 75 Prozent Steinsalz, 2o Prozent Alaun und 5 Prozent Zinksulfat. Diese Stoffe werden zerkleinert zusammengemischt und so in den Handel gebracht. Für den Gebrauch wird für ein gewöhnliches Element etwa ioo g des obigen Salzgemisches in 3/41 Wasser aufgelöst und in den Behälter des Elementes gefüllt. Nach Einfüllen der Lösung beginnt sofort die Stromentwicklung. Die Hauptvorteile des neuen Füllstoffes sind die folgenden Die Zinkstange wird nur langsam angegriffen, an der Außenseite des Elementes bilden sich keine Niederschläge, Klemmen und Leitungen angreifende Dämpfe werden nicht entwickelt, die Handhabung ist nicht gefährlich, und die Füllung ist sehr lange betriebsfähig.
Claims (2)
- PATENTANSPRÜCHE: i. Verfahren zur Herstellung eines Elektrolyten für Primärelemente; dadurch gekennzeichnet, daß dem bekannten Elektrolyten aus Steinsalz und Alaun schwefelsaures Zink zugesetzt wird.
- 2. Elektrolyt nach Anspruch i, bestehend aus 75 Prozent Steinsalz, 2o Prozent Alaun und 5 Prozent schwefelsaurem Zink.