CN201900233U - 用于锂锭浇铸的速冷铸锭模具 - Google Patents

用于锂锭浇铸的速冷铸锭模具 Download PDF

Info

Publication number
CN201900233U
CN201900233U CN201020687323XU CN201020687323U CN201900233U CN 201900233 U CN201900233 U CN 201900233U CN 201020687323X U CN201020687323X U CN 201020687323XU CN 201020687323 U CN201020687323 U CN 201020687323U CN 201900233 U CN201900233 U CN 201900233U
Authority
CN
China
Prior art keywords
mould
cooling
lithium
ingot casting
ingot
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201020687323XU
Other languages
English (en)
Inventor
何卫东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Tianqi Lithium Industry Co., Ltd.
Original Assignee
Chongqing Kunyu Lithium Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Kunyu Lithium Co Ltd filed Critical Chongqing Kunyu Lithium Co Ltd
Priority to CN201020687323XU priority Critical patent/CN201900233U/zh
Application granted granted Critical
Publication of CN201900233U publication Critical patent/CN201900233U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型公开了一种用于锂锭浇铸的速冷铸锭模具,包括内部设有型腔的模体,所述模体的内壁与外壁之间设置有冷却腔,与冷却腔连通设置有冷却介质入口和冷却介质出口,使用时,通过冷却介质入口和冷却介质出口通入流动的冷却介质,减少锂水在模具中的冷却时间,防止其受到过多氧化而影响锂锭的质量,同时,也提高了锂锭浇铸的安全性。另外,本实用新型通过模具的分体设计,使锂锭脱模更方便快捷,有效提高脱模效率。

Description

用于锂锭浇铸的速冷铸锭模具
技术领域
本实用新型涉及一种浇铸模具,特别涉及一种用于锂锭浇铸的模具。
背景技术
金属锂是常用的制造蓄电池等产品的原材料,锂通常浇注成锂锭来存储和运输。
现有技术中,浇铸锂锭的过程是将熔融状态的锂水进行处理后,直接倒入铸锭模具内,待冷却凝固后,再进行脱模取出锂锭。该铸锭模具通常是由一体式结构的模体和型腔构成,在使用过程中存在以下两点不足:a.由于金属锂的化学性质非常活泼,极易与空气中的氧和水等成分发生氧化反应,尤其是处于高温状态时,反应更容易进行,加之锂水在模具中冷却需要较长的时间,因而会严重影响锂锭产品的质量,也存在较大的安全隐患,为解决该问题,可采取在正压型手套箱内浇铸的办法,但这样也增加了设备成本;b.采用现有的模具浇铸锂锭时,不便于脱模,影响生产效率。
针对上述不足,需对现有的铸锭模具进行改进,使高温锂水可迅速冷却,以保证锂锭质量、提高安全性,另外,也使脱模更加方便,提高生产效率。
发明内容
有鉴于此,本实用新型提供一种用于锂锭生产的速冷铸锭模具,该模具可通过冷却介质进行冷却,冷却速度快,极大减少高温锂水在模具中的冷却时间,达到提高锂锭质量和生产安全性的目的。
本实用新型的用于锂锭浇铸的速冷铸锭模具,包括内部设有型腔的模体,所述模体的内壁与外壁之间设置有冷却腔,与冷却腔连通设置有冷却介质入口和冷却介质出口。
进一步,所述模体由至少两个模瓣扣合而成,与模瓣一一对应设置有冷却腔;
进一步,所述模瓣上还一一对应设置有拉环;
进一步,所述冷却介质入口、冷却介质出口和拉环均设置于模瓣的外壁上;
进一步,所述冷却介质出口的位置高于冷却介质入口的位置。
本实用新型的有益效果:本实用新型的用于锂锭浇铸的速冷铸锭模具,包括内部设有型腔的模体,所述模体的内壁与外壁之间设置有冷却腔,与冷却腔连通设置有冷却介质入口和冷却介质出口,使用时,通过冷却介质入口和冷却介质出口通入流动的冷却介质,减少锂水在模具中的冷却时间,防止其受到过多氧化而影响锂锭的质量,同时,也提高了锂锭浇铸的安全性。另外,本实用新型通过模具的分体设计,使锂锭脱模更方便快捷,有效提高脱模效率。
附图说明
下面结合附图和实施例对本实用新型作进一步描述。
图1为本实用新型的结构示意图;
图2为图1的A-A剖视图。
具体实施方式
图1为本实用新型的结构示意图,图2为图1的A-A剖视图,如图所示:本实施例的用于锂锭浇铸的速冷铸锭模具,包括内部设有型腔1的模体2,所述模体2的内壁与外壁之间设置有冷却腔3,与冷却腔3连通设置有冷却介质入口4和冷却介质出口5,本实施例中,通过向冷却介质入口通入冷却水,冷却水在冷却腔中与高温锂水换热,再经冷却介质出口排出,有效减少锂水在模具中的冷却时间,防止其受到过多氧化而影响锂锭的质量,同时,也提高了锂锭浇铸的安全性。
本实施例中,所述模体2由至少两个模瓣2a扣合而成,与模瓣2a一一对应设置有冷却腔3,便于脱模,可有效提高生产效率,每个模瓣上均设置冷却腔,能保证型腔周边冷却均匀。
本实施例中,所述模瓣2a上还一一对应设置有拉环6,以便于进行脱模操作。
本实施例中,所述冷却介质入口4、冷却介质出口5和拉环6均设置于模瓣2a的外壁上,结构合理,便于操作。
本实施例中,所述冷却介质出口5的位置高于冷却介质入口4的位置,可提高冷却介质的换热效率。
最后说明的是,以上实施例仅用以说明本实用新型的技术方案而非限制,尽管参照较佳实施例对本实用新型进行了详细说明,本领域的普通技术人员应当理解,可以对本实用新型的技术方案进行修改或者等同替换,而不脱离本实用新型技术方案的宗旨和范围,其均应涵盖在本实用新型的权利要求范围当中。

Claims (5)

1.一种用于锂锭浇铸的速冷铸锭模具,包括内部设有型腔(1)的模体(2),其特征在于:所述模体(2)的内壁与外壁之间设置有冷却腔(3),与冷却腔(3)连通设置有冷却介质入口(4)和冷却介质出口(5)。
2.根据权利要求1所述的用于锂锭浇铸的速冷铸锭模具,其特征在于:所述模体(2)由至少两个模瓣(2a)扣合而成,与模瓣(2a)一一对应设置有冷却腔(3)。
3.根据权利要求2所述的用于锂锭浇铸的速冷铸锭模具,其特征在于:所述模瓣(2a)上还一一对应设置有拉环(6)。
4.根据权利要求1、2或3所述的用于锂锭浇铸的速冷铸锭模具,其特征在于:所述冷却介质入口(4)、冷却介质出口(5)和拉环(6)均设置于模瓣(2a)的外壁上。
5.根据权利要求4所述的用于锂锭浇铸的速冷铸锭模具,其特征在于:所述冷却介质出口(5)的位置高于冷却介质入口(4)的位置。
CN201020687323XU 2010-12-29 2010-12-29 用于锂锭浇铸的速冷铸锭模具 Expired - Lifetime CN201900233U (zh)