CN201394938Y - 锁紧式耐磨陶瓷衬板 - Google Patents

锁紧式耐磨陶瓷衬板 Download PDF

Info

Publication number
CN201394938Y
CN201394938Y CN2009200848369U CN200920084836U CN201394938Y CN 201394938 Y CN201394938 Y CN 201394938Y CN 2009200848369 U CN2009200848369 U CN 2009200848369U CN 200920084836 U CN200920084836 U CN 200920084836U CN 201394938 Y CN201394938 Y CN 201394938Y
Authority
CN
China
Prior art keywords
base plate
wear
plate
abrasion resistant
resistant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009200848369U
Other languages
English (en)
Inventor
许小龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009200848369U priority Critical patent/CN201394938Y/zh
Application granted granted Critical
Publication of CN201394938Y publication Critical patent/CN201394938Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种锁紧式耐磨陶瓷衬板,包括底板和胶合固定在底板上的耐磨陶瓷层,其底板上开有均布的孔,其耐磨陶瓷层由中部开有孔,周边设有公母凹凸槽的耐磨块相互咬合拼接,并由安置在耐磨块和底板的开孔中的固定栓锁紧固定而成,在固定栓上部的耐磨块的剩余孔中填塞有堵头,耐磨块为工业陶瓷制成。其中底板由普通钢板、铁板、不锈钢或锰合金板制成,厚度为2.5-16mm,耐磨块厚度为10-100mm,堵头为工业陶瓷制成,固定栓为平头、埋头、圆头或六角螺栓,材质为钢、不锈钢、铜或合金,所用胶合剂为有机胶合剂或无机胶合剂。本锁紧式耐磨陶瓷衬板耐磨、耐腐蚀,抗冲刷和抗冲击性强,使用寿命能达到八至十年,易于更换、维修,维护成本低。

Description

锁紧式耐磨陶瓷衬板
技术领域
本实用新型涉及耐磨衬板,特别涉及一种锁紧式耐磨衬板。
背景技术
耐磨衬板主要使用在冶金系统的渣系统中接收塔或称渣槽、导出管或称方箱、分配器、缓冲箱、布料溜槽以及料罐上,用于提高塔体及设备本体的耐磨性能,同时也可使用于运输设备的料仓、料斗及输料道等设备上。现有的耐磨衬板多采用耐磨喷涂料、粘连式陶瓷耐磨衬板、橡胶复合式陶瓷衬板、耐磨合金或稀土合金衬板。由于使用环境是渣水或矿料直接冲刷或冲击到衬板表面,陶瓷喷涂料、耐磨合金及稀土合金因耐冲刷性或耐冲击性不强而磨损快、粘连式陶瓷耐磨衬板耐剪切力不强而易脱落,复合式陶瓷衬板因抗高温性不强,因而现有的耐磨衬板使用寿命一般仅有几个月,最长的也只能达到两年,亟待改进。
发明内容
本实用新型旨在克服现有耐磨衬板的不足:提供一种锁紧式耐磨陶瓷衬板,该耐磨陶瓷衬板耐磨、耐冲刷、耐温、耐腐蚀,使用寿命长。
为解决上述技术问题,本实用新型的技术方案为:
一种锁紧式耐磨陶瓷衬板,包括底板和胶合固定在底板上的耐磨陶瓷层,其特征在于:底板上开有均布的孔,其耐磨陶瓷层由中部开有孔,周边设有公母凹凸槽的耐磨块相互咬合拼接,并由安置在耐磨块和底板的开孔中的固定栓锁紧固定而成,在固定栓上部的耐磨块的剩余孔中填塞有堵头,耐磨块为工业陶瓷制成。
所述的底板为普通钢板、铁板、不锈钢板或锰合金板制成,厚度为2.5-16mm。
所述的耐磨块为刚玉材料制成,厚度为10-100mm,形状为方形、长方形、弯月形、梯形、平行四边形、菱形或T形。
所述的固定栓为螺栓,大小为M2——M16。
所述的堵头与耐磨块材质相同,为工业陶瓷或刚玉材料制成,其样式可采用圆柱体、立方体或棱柱体。
所述的固定栓插入式或螺扣式安置在耐磨块和底板的开孔中锁紧耐磨块。
胶合所用的胶合剂根据实际使用条件采用有机胶合剂或无机胶合剂。
采用上述结构的锁紧式耐磨陶瓷衬板,由于耐磨层采用特种工业陶瓷刚玉,底板采用金属底板,不仅耐磨、耐腐蚀,且抗冲刷性强、抗冲击性强。由于耐磨块不仅胶合在底板上,而且采用榫铆和固定栓紧固的结构形式,其结构稳定、具有耐温、抗剪切力等优良性能,使用寿命可长达八至十年,从而降低了设备使用、维护和维修成本,且易更换。
附图说明
下面结合附图和具体实施方式对本实用新型作进一步详细说明。
图1为本实用新型的主视示图
图2为本实用新型的俯视示图
图3为本实用新型的结构图示意图
图中标号:1耐磨陶瓷层、2耐磨块、3堵头、4底板、5固定栓、6公母凹凸槽。
具体实施方式
参见图1至图3。本实用新型提供一种锁紧式耐磨陶瓷衬板,用于渣处理系统中接收塔或称接收槽、分配器、缓冲箱、导出管或称方箱的内衬。其锁紧式耐磨陶瓷衬板,包括底板4和胶合固定在底板上的耐磨陶瓷层1,其底板4上开有均布的孔,其耐磨陶瓷层1由中部开有孔,周边设有公母凹凸槽6的耐磨块2相互(榫铆)咬合拼接,并由安置在耐磨块和底板的开孔中的固定栓5锁紧固定而成,在固定栓上部的耐磨块的剩余孔中填塞有堵头3。其中底板4为普通钢板,厚度为2.5——16mm;耐磨块为特种工业陶瓷(AL2O3为主料经过高温烧结而成),厚度为10——100mm;固定栓为M2——M16的平头螺栓;堵头为Φ10*10cm至Φ12*25cm,材质与耐磨块相同。在渣水及矿料的冲刷过程中锁紧式耐磨陶瓷衬板附着于设备内衬与渣水、矿料直接摩擦,由于锁紧式耐磨陶瓷衬板的耐磨块采用特种工业陶瓷,硬度极高,仅次于金刚石,且表面加工后光滑平整,与渣水、物料的摩擦系数较低,故而非常耐磨且吸水率为零。耐酸碱腐蚀、抗冲击性强、抗剪切力强、耐温性能好,从而延长了使用寿命,降低了设备使用、维护及维修成本。
上述底板4也可使用铁板、铜板或不锈钢板,厚度一般宜为2.5——16mm;耐磨块2和堵头3也可采用硬质合金,厚度一般为10——100mm;固定栓5一般采用各类平头螺栓,大小为M2——M16,实际使用中可按需要调整,效果是一致的。本实用新型还可适用于料罐、布料溜槽、料斗及矿山码头的输料道等设备上。

Claims (6)

1、一种锁紧式耐磨陶瓷衬板,包括底板(4)和胶合固定在底板上的耐磨陶瓷层(1),其特征在于:底板上(4)开有均布的孔,其耐磨陶瓷层(1)由中部开有孔,周边设有公母凹凸槽(6)的耐磨块(2)相互咬合拼接,并由安置在耐磨块和底板的开孔中的固定栓(5)锁紧固定而成,在固定栓上部的耐磨块的剩余孔中填塞有堵头(3),耐磨块为工业陶瓷制成。
2、如权利要求1所述的锁紧式耐磨陶瓷衬板,其特征在于:所述的底板(4)为普通钢板、铁板、不锈钢板或锰合金板制成,厚度为2.5-16mm。
3、如权利要求1所述的锁紧式耐磨陶瓷衬板,其特征在于:所述的耐磨块(2)为刚玉材料制成,厚度为10-100mm,形状为方形、长方形、弯月形、梯形、平行四边形、菱形或T形。
4、如权利要求1所述的锁紧式耐磨陶瓷衬板,其特征在于:所述的固定栓(5)为螺栓,大小为M2--M16。
5、如权利要求1所述的锁紧式耐磨陶瓷衬板,其特征在于:所述的堵头(3)为工业陶瓷或刚玉材料制成,其样式为圆柱体、立方体或棱柱体。
6、如权利要求1所述的锁紧式耐磨陶瓷衬板,其特征在于:所述的固定栓插入式或螺扣式安置在耐磨块和底板的开孔中锁紧耐磨块。
CN2009200848369U 2009-04-10 2009-04-10 锁紧式耐磨陶瓷衬板 Expired - Fee Related CN201394938Y (zh)