Prior art keywords
steel pipe
roller
process furnace
model
utility
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2007200953224U
Other languages
English (en)
Inventor
李玉平
王凤臣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin Seri Machinery Equipment Corp Ltd
Original Assignee
Tianjin Seri Machinery Equipment Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin Seri Machinery Equipment Corp Ltd filed Critical Tianjin Seri Machinery Equipment Corp Ltd
Priority to CNU2007200953224U priority Critical patent/CN201033793Y/zh
Application granted granted Critical
Publication of CN201033793Y publication Critical patent/CN201033793Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Heat Treatment Of Articles (AREA)

Abstract

本实用新型涉及一种钢管水淬出加热炉倾斜式辊道。本实用新型属于钢管制备技术领域。钢管水淬出加热炉倾斜式辊道,包括驱动机构和V形辊,驱动机构驱动连接V形辊,其特点是:V形辊安装保持辊轴轴向与钢管水淬出加热炉的运动方向非垂直倾斜位置。本实用新型不但降低了热钢管对V形辊产生的变形,同时也降低了钢管在运输过程中产生的变形;具有结构简单,安装方便,便于检修,可使钢管质量更高等优点。

Description

钢管水淬出加热炉倾斜式辊道
技术领域
本实用新型属于钢管制备技术领域,特别涉及一种钢管水淬出加热炉倾斜式辊道。
背景技术
目前,在钢管工业生产中,水淬设计出加热炉的辊道均采用Q235A材质的V形辊,V形辊的摆放位置与钢管运动方面垂直,钢管温度在900-1000摄氏度,由于长时间的钢管运输,会导致V形辊变形,而且钢管在运输过程中,也会发生微小的变形,影响钢管的质量,导致钢管不能合格出厂,影响产品质量等。
发明内容
本实用新型为解决公知技术中存在的技术问题,而提供了一种钢管水淬出加热炉倾斜式辊道。
本实用新型的目的是提供一种结构简单、安装方便、便于检修、成本低廉的钢管水淬出加热炉倾斜式辊道。
为实现上述目的,本实用新型设计采用的技术方案是将V形辊的摆放采用倾斜放置。辊道通常摆放是与钢管运输方向成90度角,对于冷钢管是可以的。但使钢管与V形辊所成的角度在一定范围时,对于900-1000摄氏度的钢管,在运输过程中使之产生旋转,这样不但降低了热钢管对V形辊产生的变形,同时也会降低钢管在运输过程中产生的变形。
本实用新型采取如下技术方案:
钢管水淬出加热炉倾斜式辊道,包括驱动机构和V形辊,驱动机构驱动连接V形辊,其特点是:V形辊安装保持辊轴轴向与钢管水淬出加热炉的运动方向非垂直倾斜位置。
本实用新型还可以采用如下技术措施:
所述的钢管水淬出加热炉倾斜式辊道,其特点是:辊轴轴向与钢管水淬出加热炉的运动方向夹角为90-100度。
所述的钢管水淬出加热炉倾斜式辊道,其特点是:V形辊安装在底座上,驱动机构由电机和联轴器构成,电机经联轴器驱动连接V形辊。
本实用新型具有的优点和积极效果:
钢管水淬出加热炉倾斜式辊道采用了全新的技术方案,在保持原辊道形式不变的情况下,解决了上述两个问题。不但降低了热钢管对V形辊产生的变形,同时也降低了钢管在运输过程中产生的变形。本实用新型具有结构简单,安装方便,便于检修,可使钢管质量更高等优点。
附图说明
图1是本实用新型的主视图;
图2为图1的俯视图;
图3为图1的局部I放大结构示意图。
图中,1-电机,2-联轴器,3-轴承座,4-V形辊,5-底座。
具体实施方式
为能进一步了解本实用新型的内容、特点及功效,兹例举以下实施例,并配合附图详细说明如下:
请参阅图1、图2、图3。
钢管水淬出加热炉倾斜式辊道,包括驱动机构和V形辊4,驱动机构由电机1和联轴器2构成,联轴器2安装在轴承座3上,电机经联轴器驱动连接V形辊。V形辊4安装在底座5上,V形辊4安装保持辊轴轴向与钢管水淬出加热炉的运动方向夹角θ为95度。
本钢管水淬出加热炉倾斜式辊道采用的技术方案是将V形辊的摆放采用倾斜放置。使钢管与V形辊成一定角度,保证900-1000摄氏度的钢管,在运输过程中使之产生旋转,这样不但降低了热钢管对V形辊产生的变形,同时也会降低钢管在运输过程中产生的变形,达到了一举两得的目的。

Claims (3)

1.钢管水淬出加热炉倾斜式辊道,包括驱动机构和V形辊,驱动机构驱动连接V形辊,其特征是:V形辊安装保持辊轴轴向与钢管水淬出加热炉的运动方向非垂直倾斜位置。
2.根据权利要求1所述的钢管水淬出加热炉倾斜式辊道,其特征是:辊轴轴向与钢管水淬出加热炉的运动方向夹角为90-100度。
3.根据权利要求1或2所述的钢管水淬出加热炉倾斜式辊道,其特征是:V形辊安装在底座上,驱动机构由电机和联轴器构成,电机经联轴器驱动连接V形辊。
CNU2007200953224U 2007-02-16 2007-02-16 钢管水淬出加热炉倾斜式辊道 Expired - Fee Related CN201033793Y (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNU2007200953224U CN201033793Y (zh) 2007-02-16 2007-02-16 钢管水淬出加热炉倾斜式辊道

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNU2007200953224U CN201033793Y (zh) 2007-02-16 2007-02-16 钢管水淬出加热炉倾斜式辊道

Publications (1)

Publication Number Publication Date
CN201033793Y true CN201033793Y (zh) 2008-03-12

Family

ID=39194685

Family Applications (1)

Application Number Title Priority Date Filing Date
CNU2007200953224U Expired - Fee Related CN201033793Y (zh) 2007-02-16 2007-02-16 钢管水淬出加热炉倾斜式辊道

Country Status (1)

Country Link
CN (1) CN201033793Y (zh)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102898009A (zh) * 2012-11-01 2013-01-30 山东力诺新材料有限公司 玻璃管退火炉
CN104495201A (zh) * 2014-12-20 2015-04-08 济南洁瑞热能科技有限公司 半自动生产线
CN105253518A (zh) * 2015-08-31 2016-01-20 中国海洋石油总公司 V型辊调节托架
CN105600274A (zh) * 2016-03-03 2016-05-25 马鞍山纽泽科技服务有限公司 钢管导出装置

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102898009A (zh) * 2012-11-01 2013-01-30 山东力诺新材料有限公司 玻璃管退火炉
CN104495201A (zh) * 2014-12-20 2015-04-08 济南洁瑞热能科技有限公司 半自动生产线
CN105253518A (zh) * 2015-08-31 2016-01-20 中国海洋石油总公司 V型辊调节托架
CN105600274A (zh) * 2016-03-03 2016-05-25 马鞍山纽泽科技服务有限公司 钢管导出装置

Similar Documents

Publication Publication Date Title
CN201033793Y (zh) 钢管水淬出加热炉倾斜式辊道
CN204310364U (zh) 一种食品冷却传送装置
CN201704374U (zh) 无冷却炉辊装置
CN209322960U (zh) 一种锻造用高效淬火装置
CN106891462A (zh) 一种塑料薄膜加工设备中的冷却装置
CN209034274U (zh) 一种石油管道生产用便于上料的涂料搅拌装置
CN209597248U (zh) 一种大米加工用凉米仓
CN216764996U (zh) 一种用于铸管台车式退火炉的可调节挡辊装置
CN202061900U (zh) 冷床输入辊道
CN202547398U (zh) 一种真空熔炼炉用抽风机构
CN109278169B (zh) 一种软瓷产品冷却装置
CN202671639U (zh) 一种带钢连续热镀锌稳定传动装置
CN201817377U (zh) 快速对流加热炉
CN201581113U (zh) 节能型热轧无缝钢管燃气调质炉快速出炉装置
CN216947025U (zh) 一种微生物固定化发酵进料装置
CN219279862U (zh) 一种可调节罐内温度的发酵罐
CN221289320U (zh) 一种用于钢管高压水除磷的挡水装置
CN211516041U (zh) 一种金属硅浇铸用的快速冷却装置
CN221220773U (zh) 一种双缸双进料的节能柱塞泵
CN110746105B (zh) 薄玻璃钢化过渡装置及过渡方法
CN204058532U (zh) 大直径中频加热炉
CN102786212B (zh) 一种玻璃圆盆钢化冷却装置
CN220875453U (zh) 可拆卸式降温设备
CN221234553U (zh) 用于煤炭高温干馏的间歇式节能供料机构
CN221810920U (zh) 一种水泥磨循环风机固定底座

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C17 Cessation of patent right
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20080312

Termination date: 20110216