CN1956243A - 电池极片及含有该极片的锂离子二次电池的制备方法 - Google Patents
电池极片及含有该极片的锂离子二次电池的制备方法 Download PDFInfo
- Publication number
- CN1956243A CN1956243A CNA2005101143817A CN200510114381A CN1956243A CN 1956243 A CN1956243 A CN 1956243A CN A2005101143817 A CNA2005101143817 A CN A2005101143817A CN 200510114381 A CN200510114381 A CN 200510114381A CN 1956243 A CN1956243 A CN 1956243A
- Authority
- CN
- China
- Prior art keywords
- pole piece
- calendering
- pole
- active material
- thickness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
实施例(电池)编号 | Δd1/Δd(%) | Δd2/Δd(%) | 电池容量分布(mAh) | 容量平均值(mAh) | 循环次数 | ||||
实施例1A1-A3 | 10 | 90 | 752 | 756 | 757 | 755 | 410 | 415 | 416 |
实施例2A4-A6 | 20 | 80 | 753 | 756 | 759 | 756 | 413 | 415 | 419 |
实施例3A7-A9 | 30 | 70 | 756 | 758 | 760 | 758 | 415 | 418 | 420 |
实施例4A10-A12 | 40 | 60 | 750 | 754 | 755 | 753 | 409 | 413 | 414 |
实施例5A13-A15 | 50 | 50 | 750 | 751 | 753 | 752 | 409 | 410 | 412 |
对比例1AC1-AC2 | 100 | 0 | 730 | 739 | 750 | 740 | 366 | 375 | 408 |
Claims (9)