CN1884093A - 制备镉的硫族化合物纳米晶体的原料组份及制备方法 - Google Patents
制备镉的硫族化合物纳米晶体的原料组份及制备方法 Download PDFInfo
- Publication number
- CN1884093A CN1884093A CN 200610014587 CN200610014587A CN1884093A CN 1884093 A CN1884093 A CN 1884093A CN 200610014587 CN200610014587 CN 200610014587 CN 200610014587 A CN200610014587 A CN 200610014587A CN 1884093 A CN1884093 A CN 1884093A
- Authority
- CN
- China
- Prior art keywords
- cadmium
- solvent
- powder
- preparation
- solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (5)