CN1736673A - 环保型染色木材的生产方法 - Google Patents

环保型染色木材的生产方法 Download PDF

Info

Publication number
CN1736673A
CN1736673A CN 200510014863 CN200510014863A CN1736673A CN 1736673 A CN1736673 A CN 1736673A CN 200510014863 CN200510014863 CN 200510014863 CN 200510014863 A CN200510014863 A CN 200510014863A CN 1736673 A CN1736673 A CN 1736673A
Authority
CN
China
Prior art keywords
environment
wood
friendly type
production method
timber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510014863
Other languages
English (en)
Inventor
高峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TIANJIN GAOSHENG WOOD INDUSTRY Co Ltd
Original Assignee
TIANJIN GAOSHENG WOOD INDUSTRY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TIANJIN GAOSHENG WOOD INDUSTRY Co Ltd filed Critical TIANJIN GAOSHENG WOOD INDUSTRY Co Ltd
Priority to CN 200510014863 priority Critical patent/CN1736673A/zh
Publication of CN1736673A publication Critical patent/CN1736673A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种染色木材的生产方法。本发明的目的是这样实现的,第一步将环保型木材专用染色剂用热水溶解并搅拌均匀,第二步将选好的木材加到反应釜中,再用高效率真空泵抽真空2-3小时,第三步用专业泵体将染液压到反应釜中,然后将压力升到1.3-5MPa,同时将温度升到92-93摄氏度,并保压18-20小时即可完成。本发明与现有技术相比,由于利用环保型木材专用染色剂作为处理剂,只须加温加压就可实现,具有生产成本低、生产工艺简单、防止环境污染、将木材由低档变高档的特点,满足了不同消费者需求。

Description

环保型染色木材的生产方法
技术领域
本发明涉及一种染色木材的生产方法。
背景技术
目前,木材着色的方法主要是常温蒸煮,存在的缺点是工艺过程复杂,操作者劳动强度大,木材只能表面着色,着色效果不好,影响木制品的档次;同时蒸煮染色也会污染大气和水资源。
发明内容
本发明的目的是提供一种既对环境没有污染,又能生产高档木材的方法。
本发明的目的是这样实现的,第一步将环保型木材专用染色剂用热水溶解并搅拌均匀,第二步将选好的木材加到反应釜中,再用高效率真空泵抽真空2-3小时,第三步用专业泵体将染液压到反应釜中,然后将压力升到1.3-5Mpa,同时将温度升到92-93摄氏度,并保压18-20小时即可完成。
本发明与现有技术相比,由于利用环保型木材专用染色剂作为处理剂,只须加温加压就可实现,具有生产成本低、生产工艺简单、防止环境污染、将木材由低档变高档的的特点,满足了不同消费者需求。
附图说明
本发明无附图
具体实施方式
实施例1,本发明的目的是这样实现的,第一步将环保型木材专用染色剂用热水溶解并搅拌均匀,第二步将选好的木材加到反应釜中,再用高效率真空泵抽真空2-3小时,第三步用专业泵体将染液压到反应釜中,然后将压力升到1.3-5Mpa,同时将温度升到92-93摄氏度,并保压18-20小时即可完成木材染色。

Claims (1)

1、环保型染色木材的生产方法,其特征在于:第一步将环保型木材专用染色剂用热水溶解并搅拌均匀,第二步将选好的木材加到反应釜中,再用高效率真空泵抽真空2-3小时,第三步用专业泵体将染液压到反应釜中,然后将压力升到1.3-5Mpa,同时将温度升到92-93摄氏度,并保压18-20小时即可完成。
CN 200510014863 2005-08-25 2005-08-25 环保型染色木材的生产方法 Pending CN1736673A (zh)