CN1616353A - 一种制备硫酸铜的新工艺 - Google Patents
一种制备硫酸铜的新工艺 Download PDFInfo
- Publication number
- CN1616353A CN1616353A CN 200310105507 CN200310105507A CN1616353A CN 1616353 A CN1616353 A CN 1616353A CN 200310105507 CN200310105507 CN 200310105507 CN 200310105507 A CN200310105507 A CN 200310105507A CN 1616353 A CN1616353 A CN 1616353A
- Authority
- CN
- China
- Prior art keywords
- copper
- reaction
- copper sulfate
- sulfuric acid
- compound
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明属于无机化工领域,具体涉及一种新的硫酸铜制备工艺,提供了一种反应温底低、反应速度快,操作简单,能耗低,无环境污染的制备硫酸铜的新工艺。制备硫酸铜新工艺以紫铜或铜精矿及硫酸为原料,通过加热,在通入空气条件下,进行氧化生产硫酸铜,反应中加入了铜蚀助剂,反应液中铜蚀助剂的含量为0.01-5%;反应温度40-100℃;反应液硫酸含量2-30%;空气流速0.005-0.05%m/s。铜蚀助剂为对苯二酚或铜及钡化合物中的一种或几种配合。铜及钒的化合物包括其盐及氧化物。本发明原料利用率高,工艺流程短,设备投资少,生产成本明显低于其它工艺。
Description
一、技术领域:本发明属于无机化工领域,具体涉及一种新的硫酸铜制备工艺。
二、背景技术:硫酸铜是一种重要的无机化工产品,在石油、化工、印染、电镀、制革,尤其是农药等行业中有着广泛的应用。
目前,国内外以紫铜为主要原料制备硫酸铜的工艺基本上有三类:
1、高温焙烧氧化溶解工艺,该工艺是将紫铜经高温焙烧氧化生成氧化铜,然后与稀硫酸反应生成硫酸铜。该工艺缺点是能耗高,劳动强度大,设备投资和运转费用多。
2、氧化剂氧化溶解工艺:该工艺是将紫铜经氧化剂如浓硝酸、双氧水等氧化生成氧化铜,然后与稀硫酸反应生成硫酸铜。该工艺缺点是制备硫酸铜过程中,常伴有大量有害气体逸出如SO2、NOx等,造成严重的环境污染,增加原料消耗,提高了生产成本;
3、催化氧化法生产硫酸铜工艺:中国发明专利公开号CN1046145A提出一种以铁离子为催化剂,加热并鼓入空气进行催化反应制得硫酸铜,该工艺原理是利用三价铁离子的氧化性,将铜氧化生成硫酸铜。该工艺的缺点:一是反应速度慢,这是因为Fe2+在酸性条件下靠空气氧化成Fe3+速度很慢,是反应过程的控制步骤,故生成硫酸铜速度慢;二是滤液循环次数少。原材料消耗高,其原因是由于铜蚀助剂是由一种或几种对苯二酚及酮、钒化合物制造而成,铜化合物包括铜盐及铜的氧化物;钒化合物包括钒盐及钒的氧化物。
三、技术内容:本发明的目的在于提供一种反应温底低、反应速度快,操作简单,能耗低,无环境污染的制备硫酸铜的新工艺。
技术方案是:制备硫酸铜新工艺以紫铜或铜精矿及硫酸为原料,通过加热,在通入空气条件下,进行氧化生产硫酸铜,反应中加入了铜蚀助剂,反应液中铜蚀助剂的含量为0.01-5%;反应温度40-100℃;反应液硫酸含量2-30%;空气流速0.005-0.05%m/s。铜蚀助剂为对苯二酚或铜及钡化合物中的一种或几种配合。铜及钒的化合物包括其盐及氧化物。
有益效果:本发明具有反应温底低、反应速度快:母液全部循环利用,原料利用率高;工艺流程短,设备投资少,操作简单,能耗低,无环境污染等特点。生产成本明显低于其它工艺,具有很好的经济效益和社会效益。
四具体实施例:
将经过予处理的干净废紫铜放入反应塔中,然后加入含10%的硫酸,0.1%的铜蚀助剂的溶液,加热升温,使反应液达70℃±2℃,以0.02m/s流速通入空气进行反应,当反应液比重达34-35℃Be″时,即将此液放入结晶槽中降温结晶,待结晶完毕,用离心机分离出硫酸铅晶体,滤液返回反应塔,继续反应生成硫酸铜产品。
Claims (3)
1、一种制备硫酸铜新工艺、以紫铜或铜精矿及硫酸为原料,通过加热,在通入空气条件下,进行氧化生产硫酸铜,其特征在于:反应中加入了铜蚀助剂,反应液中铜蚀助剂的含量为0.01-5%;反应温度40-100℃;反应液硫酸含量2-30%;空气流速0.005-0.05%m/s。
2、根据权利要求1所述的制备硫酸铜新工艺,其特征在于:铜蚀助剂为对苯二酚或铜及钡化合物中的一种或几种配合。
3、根据权利要求1和2所述的制备硫酸铜新工艺,其特征在于:铜及钒的化合物包括其盐及氧化物。