CN1304321C - 透水地材的制备方法 - Google Patents
透水地材的制备方法 Download PDFInfo
- Publication number
- CN1304321C CN1304321C CNB2004100404251A CN200410040425A CN1304321C CN 1304321 C CN1304321 C CN 1304321C CN B2004100404251 A CNB2004100404251 A CN B2004100404251A CN 200410040425 A CN200410040425 A CN 200410040425A CN 1304321 C CN1304321 C CN 1304321C
- Authority
- CN
- China
- Prior art keywords
- dankly
- preparation
- agent
- glass
- raw material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种广泛取材于石材、玻璃、陶瓷,能够透水透气的透水地材的制备方法:a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的不规整颗粒,将其中的一种,或两种以上的颗粒混合作为主要原料备用;b)将粘结剂(环氧树脂或有机硅)和固化剂如3201等按照3∶1的比例(粘结剂为75%,固化剂为25%)配制、搅拌成胶合剂备用:c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂,自然冷却固化成型。
Description
技术领域
本发明涉及一种新建材产品的制造新方法,特别是一种能够透水透气的透水地材的制备方法。
背景技术
美丽的街心花园、街道或步行街、和步行广场,一场小雨,或一场大雨之后,由于混凝土地面不渗透雨水,积水使地面显得坑坑洼洼,行人在上面行走,坑坑洼洼的水凼凼,令人心烦,使得行人或游人的兴趣大减。
发明内容
本发明的目的在于公开了一种广泛取材于石材、玻璃、陶瓷,能够透水透气的透水地材的制备方法。
为达上述目的所采用的技术方案是
a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的不规整颗粒,将其中的一种,或两种以上(包括两种)的颗粒混合作为主要原料备用;
b)将粘结剂(树脂或有机硅)和固化剂如3201等按照3∶1的比例(粘结剂为75%,固化剂为25%)配制、搅拌成胶合剂备用;
c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂,自然冷却固化成型。有的是特殊用途的透水地板,如停车场等或其他需承重的地板,按上述用量标准,可增加或减少地板的厚度和胶合剂的用量。
根据用户或施工现场的需要,标准尺寸的透水地材,可在加工厂(或加工场)用模具大批量生产为成品,使用时直接拼装;非标准尺寸的透水地材,根据现场尺寸和形状,制成模具在其中浇铸成型拼装。
本发明的优点在于
1、透气、透水。由于透水和透气性能好,一场小雨,或一场大雨之后,地面透雨水,显得干净,不会积水也不会显得坑坑洼洼。行人在上面行走,令人心旷神怡,使得行人或游人的游兴大增。
2、易于拼凑安装。施工时,标准地材可以直接拼装,非标准地材根据安装地形制作模具现场浇铸拼装,由于地材的颗粒粗,拼装线细而不容易显露出来。
3、原料极易获得,石材、玻璃、陶瓷的三种原料遍地都是,取之不竭,用之不穷,可以满足任何量的需求。产品可以制造时,可以在粘合剂中,根据需要增加任何颜色,便于将地材拼装成大型图案和文字。
4、生产设备条件不高。由于工艺和程序科学而不复杂,所需制造厂房和设备都要求不会很高,易于生产,易于普及,从而制造成本也很低廉。
具体实施方式
a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的不规整颗粒,将其中的一种,或两种以上的颗粒混合作为主要原料备用;
b)将环氧树脂或和3201固化剂按照3∶1的比例(环氧树脂为75%,3201为25%)配制、搅拌成胶合剂备用:
c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂自然冷却固化成型。有的是特殊用途的透水地板,如停车场等或其它需承重的地板,可增加地板的厚度和胶合剂的用量。
根据用户或施工现场的需要,标准尺寸的透水地材,可在加工厂(或加工场)用模具大批量生产为成品,非标准尺寸的透水地材,根据现场尺寸和形状,可制成模具浇铸成型。
Claims (2)
1、一种广泛取材于石材、玻璃、陶瓷并能够透水透气的透水地材的制备方法,其特征在于其技术方案是:
a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的颗粒,将其中的一种,或两种以上的颗粒混合作为主要原料备用;
b)将环氧树脂或有机硅和固化剂按照3∶1的比例配制、搅拌成胶合剂备用;
c)将上述a)中制得的原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b)中制得的胶合剂,自然冷却固化成型。
2、根据权利要求1所述的透水地材的制备方法,其特征在于:
根据用户或施工现场的需要,标准尺寸的透水地材,在加工厂用模具大批量生产,使用时直接拼装;非标准尺寸的透水地材,根据现场尺寸和形状,制成模具现场浇铸拼装。