透水地材的制备方法 Download PDF

Info

Publication number
CN1597591A
CN1597591A CN 200410040425 CN200410040425A CN1597591A CN 1597591 A CN1597591 A CN 1597591A CN 200410040425 CN200410040425 CN 200410040425 CN 200410040425 A CN200410040425 A CN 200410040425A CN 1597591 A CN1597591 A CN 1597591A
Authority
CN
China
Prior art keywords
dankly
preparation
floor
permeable
raw material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200410040425
Other languages
English (en)
Other versions
CN1304321C (zh
Inventor
吴逢明
吴抗
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2004100404251A priority Critical patent/CN1304321C/zh
Publication of CN1597591A publication Critical patent/CN1597591A/zh
Application granted granted Critical
Publication of CN1304321C publication Critical patent/CN1304321C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种广泛取材于石材、玻璃、陶瓷,能够透水透气的透水地材的制备方法:a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的不规整颗粒,将其中的一种,或两种以上的颗粒混合作为主要原料备用;b)将粘结剂(环氧树脂或有机硅)和固化剂如3201等按照3∶1的比例(粘结剂为75%,固化剂为25%)配制、搅拌成胶合剂备用:c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂,自然冷却固化成型。

Description

透水地材的制备方法
技术领域
本发明涉及一种新建材产品的制造新方法,特别是一种能够透水透气的透水地材的制备方法。
背景技术
美丽的街心花园、街道或步行街、和步行广场,一场小雨,或一场大雨之后,由于混凝土地面不渗透雨水,积水使地面显得坑坑洼洼,行人在上面行走,坑坑洼洼的水凼凼,令人心烦,使得行人或游人的兴趣大减。
发明内容
本发明的目的在于公开了一种广泛取材于石材、玻璃、陶瓷,能够透水透气的透水地材的制备方法。
为达上述目的所采用的技术方案是
a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的不规整颗粒,将其中的一种,或两种以上(包括两种)的颗粒混合作为主要原料备用;
b)将粘结剂(树脂或有机硅)和固化剂如3201等按照3∶1的比例(粘结剂为75%,固化剂为25%)配制、搅拌成胶合剂备用;
c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂,自然冷却固化成型。有的是特殊用途的透水地板,如停车场等或其他需承重的地板,按上述用量标准,可增加或减少地板的厚度和胶合剂的用量。
根据用户或施工现场的需要,标准尺寸的透水地材,可在加工厂(或加工场)用模具大批量生产为成品,使用时直接拼装;非标准尺寸的透水地材,根据现场尺寸和形状,制成模具在其中浇铸成型拼装。
本发明的优点在于
1、透气、透水。由于透水和透气性能好,一场小雨,或一场大雨之后,地面透雨水,显得干净,不会积水也不会显得坑坑洼洼。行人在上面行走,令人心旷神怡,使得行人或游人的游兴大增。
2、易于拼凑安装。施工时,标准地材可以直接拼装,非标准地材根据安装地形制作模具现场浇铸拼装,由于地材的颗粒粗,拼装线细而不容易显露出来。
3、原料极易获得,石材、玻璃、陶瓷的三种原料遍地都是,取之不竭,用之不穷,可以满足任何量的需求。产品可以制造时,可以在粘合剂中,根据需要增加任何颜色,便于将地材拼装成大型图案和文字。
4、生产设备条件不高。由于工艺和程序科学而不复杂,所需制造厂房和设备都要求不会很高,易于生产,易于普及,从而制造成本也很低廉。
具体实施方式
a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的不规整颗粒,将其中的一种,或两种以上的颗粒混合作为主要原料备用;
b)将环氧树脂或和3201固化剂按照3∶1的比例(环氧树脂为75%,3201为25%)配制、搅拌成胶合剂备用:
c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂自然冷却固化成型。有的是特殊用途的透水地板,如停车场等或其它需承重的地板,可增加地板的厚度和胶合剂的用量。
根据用户或施工现场的需要,标准尺寸的透水地材,可在加工厂(或加工场)用模具大批量生产为成品,非标准尺寸的透水地材,根据现场尺寸和形状,可制成模具浇铸成型。

Claims (2)

1、一种广泛取材于石材、玻璃、陶瓷,能够透水透气的透水地材的制备方法,其特征在于其技术方案是
a)将石材、玻璃、陶瓷的三种原料粉碎成2-10mm3的颗粒,将其中的一种,或两种以上的颗粒混合作为主要原料备用;
b)将环氧树脂或有机硅和固化剂按照3∶1的比例配制、搅拌成胶合剂备用:
c)将上述a原料按照100×100×10mm,浇铸0.5-0.6Kg的上述b胶合剂,自然冷却固化成型;有的特殊用途的透水地板,如停车场或其它需承重的地板,可增加地板的厚度和胶合剂的用量。
2、根据权利要求1所述的透水地材的制备方法,其特征在于:
根据用户或施工现场的需要,标准尺寸的透水地材,可在加工厂用模具大批量生产,使用时直接拼装;非标准尺寸的透水地材,根据现场尺寸和形状,制成模具现场浇铸拼装。
CNB2004100404251A 2004-08-11 2004-08-11 透水地材的制备方法 Expired - Fee Related CN1304321C (zh)