CN114309280A - 一种加强联体铁架的冲压工艺 - Google Patents
一种加强联体铁架的冲压工艺 Download PDFInfo
- Publication number
- CN114309280A CN114309280A CN202011074286.XA CN202011074286A CN114309280A CN 114309280 A CN114309280 A CN 114309280A CN 202011074286 A CN202011074286 A CN 202011074286A CN 114309280 A CN114309280 A CN 114309280A
- Authority
- CN
- China
- Prior art keywords
- iron frame
- punching
- iron
- frame
- holes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种加强联体铁架的冲压工艺,它包括相邻位数铁架之间的加强筋冲制;铁架四周的的孔冲制;铁架内拉伸;铁架内孔两侧内孔冲制;相邻位数铁架之间切边,冲孔,压扁;相邻位数铁架之间孔冲制;铁架中部螺丝孔压花;铁架上下两侧边缘压扁;铁架上下两侧边缘压扁整形;铁架翻边内孔冲制,外形冲制;铁架四周圆孔倒角;架外形边缘倒角去毛刺;切断,完工落料等工艺;在一套模具上实现一到五位数联体铁架的制作节约了制作成本,提高了生产效率。
Description
技术领域
本发明属于家居金属件制造领域,具体讲就是涉及一种加强联体铁架的冲压工艺,能够利用一台模具制造出不同位数的加强联体铁架。
背景技术
智能家居是指以住宅为平台,利用综合布线技术、网络通信技术、安全防范技术、自动控制技术、音视频技术等将家居生活油管的设施集成后构建而成的住宅设施与家庭日程事务管理系统。与普通家居相比,智能家居不仅具有传统的居住功能,同时还兼备网络通信、信息家电、设备自动化等功能,可以提供全方位的信息交互。
智能插座,智能面板,智能显示屏是常见的智能家居设备,目前这些常见的智能家居设备包含金属零部件和塑料零部件,其中联体铁架是智能家居产品中常用到的一种金属件,联体铁架一般用来安装功能件,随着插座、面板的功能越来越来越多样话,传统的一位或两位联体铁架无法满足智能家居设备功能件安装的需要,目前发展到甚至需要五位联体铁架才能满足智能设备安装需要。
联体铁架传统上用工程模或连续模制作成型,但是不同位数的联体铁架需要制作不同的模具,成本高昂,生产效率低下,为了解决不同位数联体铁架需要制作不同模具的缺陷,目前设计了级进模来制作不同位数联体铁架,但是当位数达到5位数联体铁架时,常见的级进模具冲压工艺无法达到产品尺寸精度要求,尤其是产品翻边高度和精度无法达到要求。
发明内容
本发明的目的就是针对上述现有的多位数联体铁架制作制作高昂的技术缺陷,提供一种加强联体铁架的冲压工艺,能够在一套模具上实现一到五位数联体铁架的制作节约了制作成本,提高了生产效率。
技术方案
为了实现上述技术目的,本发明提供的一种加强联体铁架的冲压工艺,其特征在于,它包括以下几个步骤:
(1)相邻位数铁架之间的加强筋冲制;
(2)铁架四周的的孔冲制;
(3)铁架内拉伸;
(4)铁架内孔两侧内孔冲制;
(5)相邻位数铁架之间切边,冲孔,压扁;
(6)相邻位数铁架之间孔冲制;
(7)铁架中部螺丝孔压花;
(8)铁架上下两侧边缘压扁;
(9)铁架上下两侧边缘压扁整形;
(10)铁架翻边内孔冲制,外形冲制;
(11)铁架四周圆孔倒角;
(12)架外形边缘倒角去毛刺;
(13)切断,完工落料。
进一步地,它包括以下几个步骤:所述步骤(1)前进行logo冲制b。
进一步地,所述步骤(10)铁架翻边内孔冲制过程中左右两侧翻边高度大于前后两侧翻边高度至少0.1mm。
进一步地,所述进行logo冲制前进行定位工艺孔冲制a。
有益效果
本发明提供的一种加强联体铁架的冲压工艺,能够在一套模具上实现一到五位数联体铁架的制作节约了制作成本,提高了生产效率。
附图说明
附图1是本发明实施例五位联装铁架的产品图。
附图2是本发明实施例的冲压料带图。
具体实施方式
下面将结合本发明实施例中的附图,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有作出创造性劳动前提下所获得的所有其它实施例,都属于本发明保护的范围。
实施例
如附图2所示,一种加强联体铁架的冲压工艺,它包括以下几个步骤:
预冲工位a,定位工艺孔冲制;
预冲工位b,进行logo冲制;
第一工位,相邻位数铁架之间的加强筋冲制;
第二工位,铁架四周的的孔冲制;
第三工位,铁架内拉伸;
第四工位,铁架内孔两侧内孔冲制;
第五工位,相邻位数铁架之间切边,冲孔,压扁;
第六工位,相邻位数铁架之间孔冲制;
第七工位,铁架中部螺丝孔压花;
第八工位,铁架上下两侧边缘压扁;
第九工位,铁架上下两侧边缘压扁整形;
第十工位,铁架翻边内孔冲制,外形冲制;其中铁架翻边内孔冲制过程中左右两侧翻边高度大于前后两侧翻边高度至少0.1mm。
第十一工位,铁架四周圆孔倒角;
第十二工位,架外形边缘倒角去毛刺;
第十三工位,切断,完工落料得到如附图1所示产品。
在本说明书的描述中,参考术语“一个实施例”、“示例”、“具体示例”等的描述意指结合该实施例或示例描述的具体特征、结构、材料或者特点包含于本发明的至少一个实施例或示例中。在本说明书中,对上述术语的示意性表述不一定指的是相同的实施例或示例。而且,描述的具体特征、结构、材料或者特点可以在任何的一个或多个实施例或示例中以合适的方式结合。
以上公开的本发明优选实施例只是用于帮助阐述本发明。优选实施例并没有详尽叙述所有的细节,也不限制该发明仅为所述的具体实施方式。显然,根据本说明书的内容,可作很多的修改和变化。本说明书选取并具体描述这些实施例,是为了更好地解释本发明的原理和实际应用,从而使所属技术领域技术人员能很好地理解和利用本发明。本发明仅受权利要求书及其全部范围和等效物的限制。
Claims (4)
1.一种加强联体铁架的冲压工艺,其特征在于,它包括以下几个步骤:
(1)相邻位数铁架之间的加强筋冲制;
(2)铁架四周的的孔冲制;
(3)铁架内拉伸;
(4)铁架内孔两侧内孔冲制;
(5)相邻位数铁架之间切边,冲孔,压扁;
(6)相邻位数铁架之间孔冲制;
(7)铁架中部螺丝孔压花;
(8)铁架上下两侧边缘压扁;
(9)铁架上下两侧边缘压扁整形;
(10)铁架翻边内孔冲制,外形冲制;
(11)铁架四周圆孔倒角;
(12)架外形边缘倒角去毛刺;
(13)切断,完工落料。
2.如权利要求1所述的一种加强联体铁架的冲压工艺,其特征在于:所述步骤(1)前进行logo冲制(b)。
3.如权利要求1所述的一种加强联体铁架的冲压工艺,其特征在于:所述步骤(10)铁架翻边内孔冲制过程中左右两侧翻边高度大于前后两侧翻边高度至少0.1mm。
4.如权利要求2所述的一种加强联体铁架的冲压工艺,其特征在于:所述进行logo冲制前进行定位工艺孔冲制(a)。