CN108185503A - 一种用于干法再造烟叶的制备方法 - Google Patents
一种用于干法再造烟叶的制备方法 Download PDFInfo
- Publication number
- CN108185503A CN108185503A CN201711361115.3A CN201711361115A CN108185503A CN 108185503 A CN108185503 A CN 108185503A CN 201711361115 A CN201711361115 A CN 201711361115A CN 108185503 A CN108185503 A CN 108185503A
- Authority
- CN
- China
- Prior art keywords
- tobacco leaf
- dry process
- preparation
- process reproduction
- roll
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种用于干法再造烟叶的制备方法。本发明采用压光辊在一定条件下对干法再造烟叶进行压光处理,经压光处理后的干法再造烟叶的松厚度、抗张强度和抗张伸长率有明显提高,且烟雾量更大、感官质量也显著提高。
Description
技术领域
本发明属于烟草技术领域,具体涉及一种用于干法再造烟叶的制备方法。
背景技术
在控烟环境日趋严峻的背景下,传统烟草制品的销量在一些发达国家市场出现了停滞甚至下降的现象,这使得国内外烟草生产者把研究和开发下一代烟草制品或替代品作为了发展的重要目标和竞争焦点,进而使新型烟草制品的研发显得迫在眉睫。新型烟草制品主要包括加热不燃烧卷烟、电子烟和无烟气烟草制品。新型烟草制品是烟草行业的新兴战略性产品,发展新型烟草制品是事关行业未来发展的重大战略性课题。而在我国烟草市场上,除电子烟之外的其他新型烟草制品仍比较少见,所以持续加强新型烟草制品的研发是很有必要的。
在新型烟草制品的研发方面,国外起步较早,上世纪70年代,国外一些跨国烟草公司就开始做前期准备工作,投入了大量资金进行市场调研、产品研发、广告宣传,目前已取得了一定的成果。而国内发展相对滞后,并且三种主要类型的新型烟草制品发展差异较大、很不均衡,目前仅有电子烟产品占有了小量的市场份额。国内的加热不燃烧卷烟制品的研究尚处于萌芽状态,虽然一些中烟公司和科研机构在此方面已申请了一批专利,但在技术、工艺、设备等方面仍存在不足,目前尚未出现较为成熟的产品和大规模的工业化生产。在控烟环境日趋严峻的情况下,使得加热不燃烧卷烟的研发越来越受烟草生产者和科技工作者的重视,加热不燃烧卷烟的成功开发将具有较大的市场前景。
干法再造烟叶产品具有较好的填充值和较低的抗张强度,直接将未经前处理的干法再造烟叶用于聚拢工艺时,有一部分样品会出现断纸的情况;在发烟剂研究中,由于高用量的甘油使产品的物理性能降低较多,而对胶粘剂配方的调整可以使加热不燃烧用干法再造烟叶产品的物理性有所提高,但若要使加热不燃烧用干法再造烟叶产品能较好的适应聚拢工艺的加工要求,仅使用胶粘剂配方的调整则达不到要求。
发明内容
为了解决上述问题,本发明提供一种用于干法再造烟叶的制备方法用于进行干法再造烟叶聚拢前处理,使处理后的干法再造烟叶的拉伸强度、抗张伸长率等综合物理指标更稳定,便于后期处理。
本发明公开了一种用于干法再造烟叶的制备方法,包括以下步骤:
(1)将片状干法再造烟叶通过传送装置传送到压光辊;
(2)在压光辊表面的温度和压光辊表面的压力一定的情况下,并在压光辊的压光速度一定的情况下,用压光辊对片状干法再造烟叶进行压光处理;
(3)将步骤(2)压光处理后的干法再造烟叶冷却至室温即得到压光处理后的干法再造烟叶。
优选地,步骤(2)所述的压光辊表面的温度为25~120℃,所述压光辊表面的压力为0~10MPa。
优选地,步骤(2)所述的压光辊表面的温度为40~70℃,所述的压光辊表面的压力为0.3~0.45MPa。
优选地,步骤(2)所述的压光速度为5-20m/min。
优选地,所述压光辊为纸粕辊、金属辊或树脂辊中的一种或几种。
优选地,所述金属辊的辊筒表面镀有硬铬或辊筒表面套有铝层。
优选地,所述纸粕辊为棉浆辊、羊毛辊、无纺布辊、毛毯辊的一种或几种
本发明的有益效果:
(1)本发明的方法首次采用压光辊在一定条件下对干法再造烟叶进行压光处理,意外发现经压光处理后的干法再造烟叶的抗张强度和抗张伸长率有明显提高,且指标更稳定,使其能更好地满足后续聚拢工艺的加工要求;并且经压光处理后的干法再造烟叶孔隙率更高,在抽吸过程中烟雾量更大、烟气释放速率更快,香气香味更足,显著提高了感官质量。而传统的再造烟叶在后期聚拢处理时会出现断纸情况,影响产品的性能和后续的生产。
(2)本发明的制备方法工艺简单,普通设备就能满足要求,成本低廉。
具体实施方式
实施例1
选取干法再造烟叶(作为对照样),选取表面镀有硬铬的金属辊作为压光辊,压光辊表面的温度选为50℃,压光辊表面的压力选为0.40MPa的条件下,压光速度选为10m/min对干法再造烟叶(对照样)进行压光处理,得到本实施例压光处理后的干法再造烟叶。本实施例压光处理后的干法再造烟叶与未经压光处理的干法再造烟叶(对照样)的物理指标检测结果如表1所示:
表1物理指标检测
序号 | 抗张强度(KN/m) | 抗张伸长率(%) |
对照样 | 0.366 | 6.55 |
实施例1 | 0.528 | 10.84 |
由表1可以看出,经本发明的用于干法再造烟叶的制备方法压光处理后的干法再造烟叶的抗张强度和抗张伸长率有较大的提高。
实施例2:感官评价
对实施例1经压光处理后的干法再造烟叶与未经压光处理的干法再造烟叶 (对照样)进行感官质量评吸,评吸结果具体见表2。
表2感官质量评吸
由表2可知:经压光处理后的干法再造烟叶与未经压光处理的干法再造烟叶相比,烟雾量明显增加,香气香味也有明显提高。
Claims (7)
1.一种用于干法再造烟叶的制备方法,其特征在于,包括以下步骤:
(1)将片状干法再造烟叶通过传送装置传送到压光辊;
(2)在压光辊表面的温度和压光辊表面的压力一定的情况下,并在压光辊的压光速度一定的情况下,用压光辊对片状干法再造烟叶进行压光处理;
(3)将步骤(2)压光处理后的干法再造烟叶冷却至室温即得到压光处理后的干法再造烟叶。
2.根据权利要求1所述的制备方法,其特征在于,步骤(2)所述的压光辊表面的温度为25~120℃,所述压光辊表面的压力为0~10MPa。
3.根据权利要求1所述的制备方法,其特征在于,步骤(2)所述的压光辊表面的温度为40~70℃,所述压光辊表面的压力为0.3~0.45MPa。
4.根据权利要求1所述的制备方法,其特征在于,步骤(2)所述的压光速度为5-20m/min。
5.根据权利要求1所述的制备方法,其特征在于,所述的压光辊为纸粕辊、金属辊或树脂辊中的一种或几种。
6.根据权利要求5所述的制备方法,其特征在于,所述金属辊的辊筒表面镀有铬或辊筒表面套有铝层。
7.根据权利要求5所述的制备方法,其特征在于,所述纸粕辊为棉浆辊、羊毛辊、无纺布辊、毛毯辊的一种或几种。