CN107032165A - 改善不锈钢冷退火酸洗线卷取折痕的装置及其使用方法 - Google Patents
改善不锈钢冷退火酸洗线卷取折痕的装置及其使用方法 Download PDFInfo
- Publication number
- CN107032165A CN107032165A CN201710289763.6A CN201710289763A CN107032165A CN 107032165 A CN107032165 A CN 107032165A CN 201710289763 A CN201710289763 A CN 201710289763A CN 107032165 A CN107032165 A CN 107032165A
- Authority
- CN
- China
- Prior art keywords
- paper
- corrugated paper
- auxiliary stand
- folding line
- stainless steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种改善不锈钢冷退火酸洗线卷取折痕的装置,在出口夹送辊支架上固定一个辅助支架,该辅助支架呈“L”形,一端连接固定在出口夹送辊支架上、另一端是自由端,瓦楞纸纸卷套在辅助支架自由端所在的那根横杆上,瓦楞纸纸卷的轴向与卷取机卷筒的轴向平行。该装置的使用方法是:将瓦楞纸纸卷套在辅助支架上,垫瓦楞纸作业时,把瓦楞纸纸卷的纸头引入带钢与卷取机卷筒之间,卷取机卷筒转动时,完成瓦楞纸垫纸。有益效果是:采用该装置可大幅提升瓦楞纸垫纸效率,避免了垫纸过程中的生产线降速。使用此技术改进可以降低作业过程对人工操作的依赖,避免人员因区域狭小还需要站在转动的卷取机后面作业而受到的伤害。
Description
技术领域
本发明属于不锈钢冷轧技术领域,涉及一种不锈钢冷退火酸洗线卷取区域瓦楞纸垫纸的辅助装置以及该装置的使用方法。
背景技术
不锈钢冷退火酸洗线出口卷取时,因为卷筒形状精度不够好或带钢自身头部的略微“上翘”都会产生横向的折痕,称之为卷取折痕。卷取折痕对于带钢表面质量影响较大,程度严重时会造成后续研磨后无法去除,最终导致材料无法应用到高端面板领域。
对于卷取折痕缺陷,一种方法是在带钢卷取前,先在卷筒外放一只套筒,带钢卷取时包裹在钢套筒上。这样做的优点就是用形状精度好的钢套筒来替代卷取机本身的卷筒,在卸卷时将钢套筒同钢卷一起卸下。但使用套筒的缺点是需要较多的钢套筒来周转,从而增加了成本,而且对于连续生产线来说,上套筒的时间会严重影响到生产线的连续性,因此该方法在连续性生产线上不可取。
防止卷取折痕的另一种方法是在带钢穿带过程中,在带钢头部与卷筒之间垫入瓦楞纸,来缓冲带钢头部“上翘”给后续带钢带来的折痕。根据经验,在卷取带钢时垫入一张长度为卷取机周长两倍的瓦楞纸可以有效的改善折痕缺陷。
由于连续生产线出口区域位置狭窄,一般人员都站在卷取机后方进行瓦楞纸作业,该作业存在如下几个风险:第一,垫入的瓦楞纸较长,人员不好控制,垫入过程中极易垫偏,影响到缓冲效果;第二,人员在狭小区域站在转动的卷取机后面作业,有一定的危险性;第三,为保证人员作业安全,整个垫纸过程中工艺降速,对连续性冷退火酸洗线工艺稳定性影响较大,造成产品力学性能的波动。
发明内容
本发明的目的在于利用一个辅助装置,提高瓦楞纸的垫纸效率,解决上述瓦楞纸垫纸作业中存在的问题。本发明提出一种改善不锈钢冷退火酸洗线卷取折痕的装置及其使用方法。
本发明所采用的技术方案是:一种改善不锈钢冷退火酸洗线卷取折痕的装置,在出口区域出口夹送辊支架上固定一个辅助支架,该辅助支架呈“L”形,一端连接固定在出口夹送辊支架上、另一端是自由端,瓦楞纸纸卷套在辅助支架自由端所在的那根横杆上,瓦楞纸纸卷的轴向与卷取机卷筒的轴向平行。
辅助支架与出口夹送辊支架的连接固定方式是焊接。
上述装置的使用方法是:将瓦楞纸纸卷套在辅助支架上,垫瓦楞纸作业时,把瓦楞纸纸卷的纸头引入带钢与卷取机卷筒之间,卷取机卷筒转动时,完成整个瓦楞纸的垫纸作业。
本发明取得的有益效果是:采用该装置可大幅提升瓦楞纸垫纸效率,避免了垫纸过程中的生产线降速。使用此技术改进可以降低作业过程对人工操作的依赖,避免人员因区域狭小还需要站在转动的卷取机后面作业而受到的伤害。
附图说明
图1是本发明装置的示意图;
图2是本发明装置的使用状态示意图;
图3是不锈钢冷退火酸洗线出口布置图;
图4是卷取折痕形成原理图。
具体实施方式
为更好的说明本发明,下面将结合说明书附图及较佳实例对本发明进行更详细的描述,本发明的保护范围不仅限于所举实例。
一种改善不锈钢冷退火酸洗线卷取折痕的装置,在出口区域出口夹送辊支架1上焊接一个辅助支架2,该辅助支架2呈“L”形,一端连接固定在出口夹送辊支架1上、另一端是自由端,瓦楞纸纸卷3套在辅助支架2自由端所在的那根横杆上,瓦楞纸纸卷3的轴向与卷取机卷筒4的轴向平行。
使用该装置时,将瓦楞纸纸卷3套在辅助支架2上,垫瓦楞纸作业时,把瓦楞纸纸卷3的纸头引入带钢5头部与卷取机卷筒4之间,卷取机卷筒4转动时,完成整个瓦楞纸的垫纸作业。一个钢卷卷曲所用的瓦楞纸长度大约是卷取机卷筒周长的两倍。带钢出速不降速或略降速的情况下,就可实现瓦楞纸垫纸,效率得以提升,同时也提高了工人的安全度。
Claims (3)
1.一种改善不锈钢冷退火酸洗线卷取折痕的装置,其特征在于:在出口区域出口夹送辊支架(1)上固定一个辅助支架(2),该辅助支架(2)呈“L”形,一端连接固定在出口夹送辊支架(1)上、另一端是自由端,瓦楞纸纸卷(3)套在辅助支架(2)自由端所在的那根横杆上,瓦楞纸纸卷(3)的轴向与卷取机卷筒(4)的轴向平行。
2.根据权利要求1所述的改善不锈钢冷退火酸洗线卷取折痕的装置,其特征在于:辅助支架(2)与出口夹送辊支架(1)的连接固定方式是焊接。
3.一种权利要求1或2所述的改善不锈钢冷退火酸洗线卷取折痕的装置的使用方法,其特征在于:将瓦楞纸纸卷(3)套在辅助支架(2)上,垫瓦楞纸作业时,把瓦楞纸纸卷(3)的纸头引入带钢(5)与卷取机卷筒(4)之间,卷取机卷筒(4)转动时,完成整个瓦楞纸的垫纸作业。