CN1056337C - 聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法 - Google Patents
聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法 Download PDFInfo
- Publication number
- CN1056337C CN1056337C CN97113335A CN97113335A CN1056337C CN 1056337 C CN1056337 C CN 1056337C CN 97113335 A CN97113335 A CN 97113335A CN 97113335 A CN97113335 A CN 97113335A CN 1056337 C CN1056337 C CN 1056337C
- Authority
- CN
- China
- Prior art keywords
- plastic film
- vinyl acetate
- foaming body
- thermoplastic transparent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法,包括(一)用滚压机滚压方式在发泡体表面涂覆一层有机热熔胶;(二)制备热塑性透明印刷胶膜;(三)热贴合加工:将热塑性透明印刷涂膜置于发泡体表面涂覆的有机热熔胶上热压,使其上的有机热熔胶、热塑性透明印刷胶膜及其透明热熔胶同时产生软化热融粘性而牢固结合,实现了在聚乙烯醋酸乙烯酯发泡体的表面牢固结合热塑性透明印刷胶膜,使其具有美观、耐用、防水、容易清洗、实用广泛等多种功能。
Description
本发明涉及有机合成发泡体的加工方法,特指一种聚乙烯醋酸乙烯酯发泡体的凹凸表面与印刷胶膜的热贴合法。
目前聚乙烯醋酸乙烯酯发泡体已被广泛地应用于工业、商业、生活等各领域,参阅图5,常用的聚乙烯醋酸乙烯酯发泡体3的表面呈1凹凸不平,充满形状各异、大小不同的毛细孔2,且在其发泡成型过程中必须添加离型剂,使其表面1不易附着印刷油墨或塑胶膜,造成美观耐用性能欠佳,防水性能较差,不易清洗,影响其实用效果。
针对上述现有技术中的缺陷,本发明人经过多年的反复研究和试验,并经过多次的改进和完善,创造出本发明的技术方案。
本发明的目的在于提供一种聚乙烯醋酸乙烯酯发泡体的凹凸表面与印刷胶膜的热贴合法,能够将热塑性印刷胶膜贴合在聚乙烯醋酸乙烯酯发泡体的表面,达到美观、耐用、防水、容易清洗等多种功效。
本发明的目的是这样实现的:一种聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法,其特征在于该热贴合法包括:
(一)发泡体的表面处理:用滚压机滚压方式在聚乙烯醋酸乙烯酯发泡体表面涂覆一层有机液体热熔胶,使该有机液体热熔胶填入该聚乙烯醋酸乙烯酯发泡体的凹凸表层及毛细孔中,风干备用;
(二)制备热塑性透明印刷胶膜:在一张热塑性透明塑胶薄膜表面涂覆一层与其相同材质的透明热熔胶,再印刷至少一色的油墨图案,再涂覆一层所述有机液体热熔胶,风干,制成热塑性透明印刷胶膜备用;
(三)热贴合加工:将所述(二)制成的热塑性透明印刷胶膜置于所述(一)发泡体的处理表面上,送入热贴合机热压,使其上的所述有机热熔胶、热塑性透明印刷胶膜及其上涂覆的透明热熔胶同时产生软化热融粘性而牢固结合,其热压温度为80-150℃。
所述热塑性透明塑胶薄膜的材质包括聚乙烯、聚丙烯。
所述透明热熔胶的材质包括聚乙烯、聚丙烯。
本发明的主要优点是:
1、解决了在聚乙烯醋酸乙烯酯发泡体的表面不易贴合塑胶膜的困难,实现了能牢固地将热塑性印刷胶膜粘着在发泡体的凹凸表面,使其具有美观、耐用、防潮、防水、容易清洗、安全、实用广泛等多种功能。
2、本发明的工艺简单、加工容易、不需要特殊设备,加工成本低廉。
下面结合较佳实施例和附图对本发明进一步说明:
图1为本发明的制造工艺流程图;
图2为本发明的发泡体的表面处理的示意图;
图3为本发明的制备热塑性透明印刷胶膜的示意图;
图4为本发明的热贴合工艺的示意图;
图5为常用发泡体的外观及局部放大示意图。
参阅图1,本发明的聚乙烯醋酸乙烯酯发泡板材10的表面与印刷胶膜24热贴合法包括(一)发泡板材10的表面处理;(二)制备热塑性透明印刷胶膜24;(三)热贴合加工。
参阅图2,发泡板材10的表面处理:用滚压机12的滚压方式将有机液体热熔胶13从液体热熔胶贮槽14中涂覆在聚乙烯醋酸乙烯酯发泡板材10的表面,使有机液体热熔胶13填入发泡板材10的凹凸表层和毛细孔中,风干以后,在发泡板材10的表面形成有机热熔胶层11。
参阅图3,制备热塑性透明印刷胶膜24,在一张热塑性透明塑胶薄膜20表面涂覆一层聚丙烯或聚乙烯透明热熔胶21,再印刷一色或多色的油墨图案22,再涂覆一层与有机热熔胶层11相同材质的有机液体热熔胶23,风干后,制造成热塑性透明印刷胶膜24,备用。
参阅图4,热贴合加工:将上述制备的热塑性透明印刷胶膜24置于发泡板材10的有机热熔胶层11上,送入热贴合机30的热滚31热压,使有机热熔胶11、23和热塑性透明印刷胶膜20及其透明热熔胶21同时受热,产生软化热融粘性而牢固结合,其热压温度为80-150℃,视发泡板体10、热塑性透明印刷胶膜20的厚度,及透明热熔胶21的品种不同而变化合适的温度。
上述加工过程中滚压机的滚压方式、印刷一色或多色油墨图案、热贴合机热压操作均为现有技术,故不详述。其中所使用的有机热熔胶亦为常用的有机热熔胶,故不详述。
Claims (3)
1、一种聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法,其特征在于该热贴合法包括:
(一)发泡体的表面处理:用滚压机滚压方式在聚乙烯醋酸乙烯酯发泡体表面涂覆一层有机液体热熔胶,使该有机液体热熔胶填入该聚乙烯醋酸乙烯酯发泡体的凹凸表层及毛细孔中,风干备用;
(二)制备热塑性透明印刷胶膜:在一张热塑性透明塑胶薄膜表面涂覆一层与其相同材质的透明热熔胶,再印刷至少一色的油墨图案,再涂覆一层所述有机液体热熔胶,风干,制成热塑性透明印刷胶膜备用;
(三)热贴合加工:将所述(二)制成的热塑性透明印刷胶膜置于所述(一)发泡体的处理表面上,送入热贴合机热压,使其上的所述有机热熔胶、热塑性透明印刷胶膜及其上涂覆的透明热熔胶同时产生软化热融粘性而牢固结合,其热压温度为80-150℃。
2、如权利要求1所述的聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法,其特征在于所述热塑性透明塑胶薄膜的材质包括聚乙烯、聚丙烯。
3、如权利要求1所述的聚乙烯醋酸乙烯酯发泡体与印刷胶膜的热贴合法,其特征在于所述透明热熔胶的材质包括聚乙烯、聚丙烯。