CN104831525A - 斜纹桃皮绒面料的开纤减量处理工艺 - Google Patents
斜纹桃皮绒面料的开纤减量处理工艺 Download PDFInfo
- Publication number
- CN104831525A CN104831525A CN201510104976.8A CN201510104976A CN104831525A CN 104831525 A CN104831525 A CN 104831525A CN 201510104976 A CN201510104976 A CN 201510104976A CN 104831525 A CN104831525 A CN 104831525A
- Authority
- CN
- China
- Prior art keywords
- fibrillation
- weight reduction
- reduction treatment
- twilled
- face fabric
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种斜纹桃皮绒面料的开纤减量处理工艺,工艺难度低,制得的面料质量好,其中,所述斜纹桃皮绒面料在处理液中进行开纤减量处理,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂10-15g/L,渗透剂4-6g/L;开纤减量处理时浴比为1:10~15,时间为25-30min,温度为100-110℃,失重率18-20%。
Description
技术领域
本发明涉及一种斜纹桃皮绒面料的开纤减量处理工艺。
背景技术
桃皮绒是超细纤维织物一种新颖的薄型起绒织物,它是从人造麂皮中脱胎而来的,由于不经过聚氨酯湿法处理,所以质地更柔软。又因其绒更短,表面几乎看不出绒毛而皮肤却能感知,以至手感和外观更细腻而别致。桃皮绒经染整加工中精细的磨绒整理,使织物表面产生紧密覆盖约0.2毫米的短绒,犹如水蜜桃的表面,光泽柔和高雅,与人造麂皮相比,具有新颖而优雅的外观和舒适的手感,给消费者一种新奇感,适合了人们好奇的消费心理,从而受到人们的青睐,以致很快在国际市场上走红。现有技术中,由于桃皮绒织物成品要求有良好的手感、悬垂性、绒感,同时要保持一定的强力,所以染整工艺比较复杂,难度大。
发明内容
本发明所要解决的技术问题在于提供一种斜纹桃皮绒面料的开纤减量处理工艺,工艺难度低,制得的面料质量好。
为解决上述现有的技术问题,本发明采用如下方案:斜纹桃皮绒面料的开纤减量处理工艺,所述斜纹桃皮绒面料在处理液中进行开纤减量处理,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂10-15g/L,渗透剂4-6g/L;开纤减量处理时浴比为1:10~15,时间为25-30min,温度为100-110℃,失重率18-20%。
作为优选,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂10g/L,渗透剂4g/L;开纤减量处理时浴比为1:10,时间为25min,温度为110℃,失重率18%。
作为优选,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂15g/L,渗透剂6g/L;开纤减量处理时浴比为1:15,时间为30min,温度为100℃,失重率20%。
有益效果:
本发明采用上述技术方案提供的斜纹桃皮绒面料的开纤减量处理工艺,工艺难度低,有利于后续染色,可使制得的面料颜色更均匀、质量更好。
具体实施方式
实施例一:
斜纹桃皮绒面料的开纤减量处理工艺,所述斜纹桃皮绒面料在处理液中进行开纤减量处理,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂10g/L,渗透剂4g/L;开纤减量处理时浴比为1:10,时间为25min,温度为110℃,失重率18%。
实施例二:
与实施例一的不同之处在于,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂15g/L,渗透剂6g/L;开纤减量处理时浴比为1:15,时间为30min,温度为100℃,失重率20%。
实施例三:
斜纹桃皮绒面料,由坯布依次经染整工艺制得,所述染整工艺包括以下步骤:步骤一、开纤减量处理;步骤二、热定形;步骤三、磨毛;步骤四、染色;步骤五、拉幅后整理。
其中,所述斜纹桃皮绒面料在进行开纤减量处理时采用如实施例一或实施例二所述的斜纹桃皮绒面料的开纤减量处理工艺。
所述斜纹桃皮绒面料热定形温度155-160℃,时间25~30s,落布温度小于50℃。
所述斜纹桃皮绒面料在染液中染色,所述染液中各组分及其含量为:分散染料10-15%(owf)、酸性染料10-15%(owf)、NNO3g/L、匀染剂2g/L、固色剂1g/L;浴比50:1,用醋酸-醋酸钠的缓冲液调节染液pH值4.5-5;染色步骤为:染液在45℃入染,先保持染液45℃状态15分钟,然后染液以1℃/min的速度升温至80℃,再以3℃/min的速度升温至100℃,保持染液在100℃状态下25分钟,然后染液以1℃/min的速度升温至125℃,保持125℃状态40分钟,然后染液以2℃/min的速度降温至80℃,保持80℃状态15分钟,然后以1℃/min的速度降温至60℃进行水洗。
所述斜纹桃皮绒面料在整理液中进行拉幅后整理,整理液包括:防静电剂18g/L、非离子柔软剂25g/L,防雨剂20g/L;整理完成后先在80-85℃的温度下预烘45min,再在180-190℃的温度下烘焙15min。
Claims (3)
1.斜纹桃皮绒面料的开纤减量处理工艺,所述斜纹桃皮绒面料在处理液中进行开纤减量处理,其特征在于,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂10-15g/L,渗透剂4-6g/L;开纤减量处理时浴比为1:10~15,时间为25-30min,温度为100-110℃,失重率18-20%。
2.根据权利要求1所述的斜纹桃皮绒面料的开纤减量处理工艺,其特征在于,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂10g/L,渗透剂4g/L;开纤减量处理时浴比为1:10,时间为25min,温度为110℃,失重率18%。
3.根据权利要求1所述的斜纹桃皮绒面料的开纤减量处理工艺,其特征在于,所述处理液中各组分及其含量为:烧碱25g/L,保险粉10g/L,稳定剂15g/L,渗透剂6g/L;开纤减量处理时浴比为1:15,时间为30min,温度为100℃,失重率20%。