CN103526207A - 一种除锈浆料 - Google Patents
一种除锈浆料 Download PDFInfo
- Publication number
- CN103526207A CN103526207A CN201310434401.3A CN201310434401A CN103526207A CN 103526207 A CN103526207 A CN 103526207A CN 201310434401 A CN201310434401 A CN 201310434401A CN 103526207 A CN103526207 A CN 103526207A
- Authority
- CN
- China
- Prior art keywords
- slurry
- kilogram
- derusting
- aluminum oxide
- iron
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (3)