CN103526207B - 一种除锈浆料 - Google Patents

一种除锈浆料 Download PDF

Info

Publication number
CN103526207B
CN103526207B CN201310434401.3A CN201310434401A CN103526207B CN 103526207 B CN103526207 B CN 103526207B CN 201310434401 A CN201310434401 A CN 201310434401A CN 103526207 B CN103526207 B CN 103526207B
Authority
CN
China
Prior art keywords
rust cleaning
cleaning slurry
kilogram
slurry
present
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310434401.3A
Other languages
English (en)
Other versions
CN103526207A (zh
Inventor
杨龙兴
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Top Drive Equipment Co., Ltd.
Original Assignee
Wuxi Yanggong Machinery Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuxi Yanggong Machinery Manufacturing Co Ltd filed Critical Wuxi Yanggong Machinery Manufacturing Co Ltd
Priority to CN201310434401.3A priority Critical patent/CN103526207B/zh
Publication of CN103526207A publication Critical patent/CN103526207A/zh
Application granted granted Critical
Publication of CN103526207B publication Critical patent/CN103526207B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明一种除锈浆料,该浆料含有10~30wt%的氧化铝抛光粉,1~3wt%的十八烷基三乙氧基硅烷,0.1~3wt%的硬脂酸,1~2wt%的丙三醇,0.1~1wt%的磷酸,0.1~1wt%的二氧化锰,0.1~0.5wt%表面活性剂,余量为水。采用本发明的除锈浆料在完成除去铁制器件表面的铁锈的同时,在表面能形成一层保护膜,从而阻止铁器重新生锈。

Description

一种除锈浆料
技术领域
本发明涉及一种用于金属表面抛光的浆料。
背景技术
铁制器件在与空气的长期接触过程中不可避免会发生一定程度氧化,特别是在潮湿环境下,使器件表面产生一层铁锈,现有除锈处理剂虽然能除去表面的铁锈,但除锈后的铁如不进行防腐处理,在表面很快会又被氧化而失去金属光泽,甚至重新产生铁锈。
发明内容
本发明的目的是提供了一种除锈浆料。
为了实现上述目的,本发明提供了如下的技术方案:
一种除锈浆料,含有10~30wt%的氧化铝抛光粉,1~3wt%的十八烷基三乙氧基硅烷,0.1~3wt%的硬脂酸,1~2wt%的丙三醇,0.1~1wt%的磷酸,0.1~1wt%的二氧化锰,0.1~0.5wt%表面活性剂,余量为水。
进一步,所述氧化铝抛光粉的粒径为4~50μm。
进一步,所述表面活性剂为十二烷基磺酸钠或壬基酚聚氧乙烯醚NP-10。
采用本发明的除锈浆料在完成除去铁制器件表面的铁锈的同时,在表面能形成一层保护膜,从而阻止铁器重新生锈。
具体实施方式
以下对本发明的优选实施例进行说明,应当理解,此处所描述的优选实施例仅用于说明和解释本发明,并不用于限定本发明。
实施例1
一种除锈浆料,由1公斤氧化铝抛光粉(粒径为4~15μm的α-Al2O3),0.3公斤的十八烷基三乙氧基硅烷(CAS:7399-00-0),0.2公斤的硬脂酸,0.1公斤的丙三醇,0.01公斤的磷酸,0.01公斤的二氧化锰,0.01公斤的十二烷基磺酸钠和8.37公斤的水,研磨混合均匀后得到。
实施例2
一种除锈浆料,由2公斤氧化铝抛光粉(粒径为10~25μm的α-Al2O3),0.2公斤的十八烷基三乙氧基硅烷,0.3公斤的硬脂酸,0.1公斤的丙三醇,0.1公斤的磷酸,0.1公斤的二氧化锰,0.05公斤的十二烷基磺酸钠和7.15公斤的水,研磨混合均匀后得到。
实施例3
一种除锈浆料,由3公斤氧化铝抛光粉(粒径为25~50μm的α-Al2O3),0.1公斤的十八烷基三乙氧基硅烷,0.01公斤的硬脂酸,0.2公斤的丙三醇,0.05公斤的磷酸,0.05公斤的二氧化锰,0.03公斤的壬基酚聚氧乙烯醚NP-10和6.56公斤的水,研磨混合均匀后得到。
该除锈浆料的使用:用打磨布沾上浆料,在铁制器具表面进行打磨,直至器具显出金属光泽后,然后放置10~20分钟,最后用水冲洗即可。
以上所述仅为本发明的优选实施例而已,并不用于限制本发明,尽管参照前述实施例对本发明进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。

Claims (3)

1.一种阻止铁器重新生锈的除锈浆料,含有10~30wt%的氧化铝抛光粉,1~3wt%的十八烷基三乙氧基硅烷,0.1~3wt%的硬脂酸,1~2wt%的丙三醇,0.1~1wt%的磷酸,0.1~1wt%的二氧化锰,0.1~0.5wt%表面活性剂,余量为水。
2.根据权利要求1所述的除锈浆料,其特征在于,所述氧化铝抛光粉的粒径为4~50μm。
3.根据权利要求1所述的除锈浆料,其特征在于,所述表面活性剂为十二烷基磺酸钠或壬基酚聚氧乙烯醚NP-10。
CN201310434401.3A 2013-09-23 2013-09-23 一种除锈浆料 Active CN103526207B (zh)