CN103508535A - 一种脱硫废液的处理方法 - Google Patents

一种脱硫废液的处理方法 Download PDF

Info

Publication number
CN103508535A
CN103508535A CN201310475194.6A CN201310475194A CN103508535A CN 103508535 A CN103508535 A CN 103508535A CN 201310475194 A CN201310475194 A CN 201310475194A CN 103508535 A CN103508535 A CN 103508535A
Authority
CN
China
Prior art keywords
copper sulfate
scn
wastewater
liquid waste
removal liquid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310475194.6A
Other languages
English (en)
Inventor
王耀斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shaanxi Shengmai Petroleum Co Ltd
Original Assignee
Shaanxi Shengmai Petroleum Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shaanxi Shengmai Petroleum Co Ltd filed Critical Shaanxi Shengmai Petroleum Co Ltd
Priority to CN201310475194.6A priority Critical patent/CN103508535A/zh
Publication of CN103508535A publication Critical patent/CN103508535A/zh
Pending legal-status Critical Current

Abstract

本发明所述的一种脱硫废液的处理方法涉及一种废水的处理方法。其包括:在室温下,向废水中慢慢加入硫酸铜固体,边加入边搅拌,其中硫酸铜的加入量与废水中SCN-含量之比为(0.1~1):1,静置后过滤、洗涤、干燥即可。本发明所述的一种脱硫废液的处理方法,包括在室温下,向废水中慢慢加入硫酸铜固体,边加入边搅拌,其中硫酸铜的加入量与废水中SCN-含量之比为(0.1~1):1,静置后过滤、洗涤、干燥即可。本发明在含有SCN-、S2O3 2-的脱硫废液中加入适量硫酸铜固体,可形成单一物相的CuSCN沉淀,处理后SCN-浓度显著降低。

Description

一种脱硫废液的处理方法
技术领域
    本发明涉及一种废水的处理方法。
背景技术
湿法氧化脱硫通常以氨水或碳酸钠溶液吸收待处理气体中硫化氢,然后在催化剂作用下将硫化氢氧化为单质硫加以回收。湿法氧化脱硫具有脱硫效果好、常温常压下可操作、脱硫液可循环使用等优点,是国内化肥厂、焦化厂常采用的煤气、合成气和焦炉气脱硫技术。然而,硫化氢在催化氧化为单质硫的过程中会产生其他含硫副产物,如硫代硫酸盐、硫氰酸盐和硫酸盐等,并且随着脱硫液的循环使用而富集,导致脱硫效果大大降低,而其中盐浓度也远远超过了排放标准,因此脱硫废液已成为工厂生产和环境保护的双重难题。
发明内容
本发明旨在提供一种经济有效的脱硫废液的处理方法。
本发明所述的一种脱硫废液的处理方法,包括:在室温下,向废水中慢慢加入硫酸铜固体,边加入边搅拌,其中硫酸铜的加入量与废水中SCN-含量之比为(0.1~1):1,静置后过滤、洗涤、干燥即可。
本发明所述的一种脱硫废液的处理方法,包括在室温下,向废水中慢慢加入硫酸铜固体,边加入边搅拌,其中硫酸铜的加入量与废水中SCN-含量之比为(0.1~1):1,静置后过滤、洗涤、干燥即可。本发明在含有SCN-、S2O3 2-的脱硫废液中加入适量硫酸铜固体,可形成单一物相的CuSCN沉淀,处理后SCN-浓度显著降低,而S2O3 2-由于反应消耗和体系酸化而全部转化为硫酸盐,使得水体中Na2SO4。浓度接近或达到饱和值。因此,在采用低温结晶的方法或其他工业上可实现的方法除去大部分硫酸钠,最终水体盐浓度大大降低。可在补加碳酸钠固体后作为脱硫液使用或直接作为脱硫液补水。
具体实施方式
实施例一
量取100 mL实际脱硫废液于250 mL烧杯中,在室温、磁力搅拌条件下,多次少量加入一定量的硫酸铜固体,其中硫酸铜的加入量与脱硫废液样品中SCN-含量之比为(0.1~1):1。反应体系中产生的沉淀物经过滤、洗涤、干燥后称重,进行X射线衍射(XRD)和扫描电镜(SEM)表征;测定处理后水体pH、SCN-、S2O3 2-、S04 2-浓度以及Cu2+的剩余量。结果如下表:                                               
Figure 2013104751946100002DEST_PATH_IMAGE002

Claims (1)

1.一种脱硫废液的处理方法,其特征在于包括:在室温下,向废水中慢慢加入硫酸铜固体,边加入边搅拌,其中硫酸铜的加入量与废水中SCN-含量之比为(0.1~1):1,静置后过滤、洗涤、干燥即可。
CN201310475194.6A 2013-10-13 2013-10-13 一种脱硫废液的处理方法 Pending CN103508535A (zh)