CN102828413A - 防水西裤的制造方法 - Google Patents

防水西裤的制造方法 Download PDF

Info

Publication number
CN102828413A
CN102828413A CN2012103482153A CN201210348215A CN102828413A CN 102828413 A CN102828413 A CN 102828413A CN 2012103482153 A CN2012103482153 A CN 2012103482153A CN 201210348215 A CN201210348215 A CN 201210348215A CN 102828413 A CN102828413 A CN 102828413A
Authority
CN
China
Prior art keywords
waterproof
western
suit pants
parts
style trousers
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012103482153A
Other languages
English (en)
Inventor
解吉平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY
Original Assignee
KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY filed Critical KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY
Priority to CN2012103482153A priority Critical patent/CN102828413A/zh
Publication of CN102828413A publication Critical patent/CN102828413A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种防水西裤的制造方法,包括如下步骤:将西裤面料在含有防水剂的浸渍液中浸轧处理,压力2-2.5kg/cm2,带液率75-80%;将面料烘干处理,然后进行裁剪、制裤、熨烫定型;采用烘培定型机将熨烫定型后的西裤在140-150℃之间恒温0.5-2小时;所述防水剂由如下重量份的组分构成:聚醚酯弹性体60-70份、苯基异氰酸酯聚氨酯20-25份、硅烷偶联剂2-5份、聚丙烯酸钠分散剂0.5-1.2份,并加水配成质量浓度为15-45%的浸轧液。本发明防水西裤中防水剂与织物牢固结合,耐久性强,具有很好的防水性能,并且经多次洗涤后防水性能仍然出色。

Description

防水西裤的制造方法
技术领域
本发明涉及一种防水西裤的制造方法。
背景技术
随着人们生活水平的日益提高,消费者对服装服用性能的要求也愈来愈高。特别是休闲旅游等户外活动的着装必须具备防雨防风、保温耐寒、透湿、舒适、轻便等特殊功能。早期的防水性涂层加工是在织物表面涂有不透水、不溶于水的连续塑料薄膜,因而织物不透气、不透汗,穿着用这类织物做成的雨衣会使人感到气闷,故主要用于制作帐篷、雨伞等用品。人们希望织物能同时具备防水和透湿功能。
防水透湿织物是集防水、透湿、防风和保暖性能于一体的多功能织物。织物在一定的水压下不能被水润湿,但人体散发的汗液却能通过织物扩散或传递到外界,不在体表和织物之间积聚冷凝。具备这种透湿能力的织物,不仅能满足人们在特殊作业环境(如严寒、雨雪、大风天气,沙漠、雨林等恶劣环境)中活动时的穿着需要(如作战服、野外考察服等),也适用于人们在日常生活中对雨衣等防水衣物及各种高档服装面料的要求,具有广阔的发展前景。
中国专利CN1460068A公开了一种水蒸汽可渗透的防水复合材料织物,其采用聚醚酯弹性体粘合剂层层压到构成基材织物上的聚醚酯弹性体薄膜层,以解决原有材料具有一定毒性的技术缺陷。然而该聚醚酯弹性体粘合剂使用过程中需要使用到有机溶剂,同样不可避免的产生生产环节的有毒有害污染。并且耐水洗性还有待进一步提高。
发明内容
本发明要解决的技术问题是提供一种防水西裤的制造方法,以克服现有技术存在的上述缺陷。
为解决上述技术问题,本发明防水西裤的制造方法,包括如下步骤:
1)将西裤面料在含有防水剂的浸渍液中浸轧处理,压力2-2.5kg/cm2,带液率75-80%;
2)将面料烘干处理,然后进行裁剪、制裤、熨烫定型;
3)采用烘培定型机将熨烫定型后的西裤在140-150℃之间恒温0.5-2小时;
所述防水剂由如下重量份的组分构成:
聚醚酯弹性体          60-70份、
苯基异氰酸酯聚氨酯    20-25份、
硅烷偶联剂            2-5份、
聚丙烯酸钠分散剂      0.5-1.2份,
然后加水配成质量浓度为15-45%的浸轧液。
所述聚醚酯弹性体包含聚乙二醇残基、亚烷基二醇残基、和二羧酸残基,其中聚乙二醇残基占5-25wt%;
亚烷基二醇残基中包含乙二醇残基、丁二醇残基。
所述聚丙烯酸钠分散剂优选粘度200-30mPa·s。
本发明防水西裤中防水剂与织物牢固结合,耐久性强,具有很好的防水性能,并且经多次洗涤后防水性能仍然出色。
具体实施方式
实施例1
防水剂的制备:
聚醚酯弹性体          70份、
苯基异氰酸酯聚氨酯    20份、
硅烷偶联剂            2份、
聚丙烯酸钠分散剂    0.5份,
将上述组分混合后加水配成质量浓度为15%的浸轧液。
防水西裤的制造:
1)将西裤面料在含有防水剂的浸渍液中浸轧处理,压力2kg/cm2,带液率75%;
2)将面料烘干处理,然后进行裁剪、制裤、熨烫定型;
3)采用烘培定型机将熨烫定型后的西裤在140℃之间恒温2小时。
实施例2
防水剂的制备:
聚醚酯弹性体          60份、
苯基异氰酸酯聚氨酯    25份、
硅烷偶联剂            5份、
聚丙烯酸钠分散剂      1.2份,
将上述组分混合后加水配成质量浓度为45%的浸轧液。
防水西裤的制造:
1)将西裤面料在含有防水剂的浸渍液中浸轧处理,压力2.5kg/cm2,带液率80%;
2)将面料烘干处理,然后进行裁剪、制裤、熨烫定型;
3)采用烘培定型机将熨烫定型后的西裤在150℃之间恒温0.5小时。
应用实施例
防水性能
将本发明防水西裤按照标准ISO 4920-2012《纺织品织物耐表面湿润(喷雾试验)性的测定》的方法测定在不同洗涤条件下的防水性能,结果本发明在洗涤50次后,仍然具有优异的防水性能。

Claims (4)

1.一种防水西裤的制造方法,其特征在于,包含如下步骤:
1)将西裤面料在含有防水剂的浸渍液中浸轧处理,压力2-2.5kg/cm2,带液率75-80%;
2)将面料烘干处理,然后进行裁剪、制裤、熨烫定型;
3)采用烘培定型机将熨烫定型后的西裤在140-150℃之间恒温0.5-2小时;
所述防水剂由如下重量份的组分构成:
聚醚酯弹性体          60-70份、
苯基异氰酸酯聚氨酯    20-25份、
硅烷偶联剂            2-5份、
聚丙烯酸钠分散剂      0.5-1.2份,
并加水配成质量浓度为15-45%的浸轧液。
2.根据权利要求1所述的防水西裤的制造方法,其特征在于,所述聚醚酯弹性体包含聚乙二醇残基、亚烷基二醇残基、和二羧酸残基,其中聚乙二醇残基占5-25wt%。
3.根据权利要求2所述的防水西裤的制造方法,其特征在于,所述聚醚酯弹性体中亚烷基二醇残基中包含乙二醇残基、丁二醇残基。
4.根据权利要求1所述的防水西裤的制造方法,其特征在于,所述聚丙烯酸钠分散剂粘度为300-350mPa·s。
CN2012103482153A 2012-09-19 2012-09-19 防水西裤的制造方法 Pending CN102828413A (zh)