CN102167577B - 一种高性能热敏陶瓷材料 - Google Patents

一种高性能热敏陶瓷材料 Download PDF

Info

Publication number
CN102167577B
CN102167577B CN201010603128.9A CN201010603128A CN102167577B CN 102167577 B CN102167577 B CN 102167577B CN 201010603128 A CN201010603128 A CN 201010603128A CN 102167577 B CN102167577 B CN 102167577B
Authority
CN
China
Prior art keywords
ceramic material
thermal sensitive
high performance
oxide
sensitive ceramic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201010603128.9A
Other languages
English (en)
Other versions
CN102167577A (zh
Inventor
费金华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wujiang Huacheng Composite Technology Co Ltd
Original Assignee
Wujiang Huacheng Composite Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wujiang Huacheng Composite Technology Co Ltd filed Critical Wujiang Huacheng Composite Technology Co Ltd
Priority to CN201010603128.9A priority Critical patent/CN102167577B/zh
Publication of CN102167577A publication Critical patent/CN102167577A/zh
Application granted granted Critical
Publication of CN102167577B publication Critical patent/CN102167577B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供一种高性能热敏陶瓷材料,由二氧化锰MnO280~84%、氧化镍NiO0.1-1%、四氧化三钴Co3O44-8%、三氧化二铁Fe2O38-10%、二氧化锌ZnO0.5-2%、氧化铜CuO3-5%组成的高压陶瓷电容器材料,采用本配方,就可以得到稳定度优于0.02度,β值误差≤±0.3%,零功率电阻值精度误差≤±0.08%等优良性能。

Description

一种高性能热敏陶瓷材料
技术领域
本发明涉及一种电容材料,尤其是高压陶瓷电容材料。
背景技术
目前的高压电容多数是-30度~65度的工作温度范围,目前广泛生产使用的高压陶瓷电容器材料的误差率高,电阻值变化大。
发明内容
本发明的目的提供一种误差率小,电阻值稳定的高压陶瓷电容材料。
一种高性能热敏陶瓷材料,其特征在于由二氧化锰MnO280~84%、氧化镍NiO0.1-1%、四氧化三钴Co3O44-8%、三氧化二铁Fe2O38-10%、二氧化锌ZnO0.5-2%、氧化铜CuO3-5%组成的高压陶瓷电容器材料。
采用本配方,就可以得到稳定度优于0.02度,β值误差≤±0.3%,零功率电阻值精度误差≤±0.08%等优良性能。
具体实施方式
具体实施时,我们将二氧化锰、氧化镍NiO、四氧化三钴Co3O4、三氧化二铁Fe2O3、二氧化锌ZnO、氧化铜CuO按配方比例混合后加入聚乙烯醇压制成型,然后在1250到1400摄氏度范围内烧结得到陶瓷电容。
将二氧化锰、氧化镍NiO、四氧化三钴Co3O4、三氧化二铁Fe2O3、二氧化锌ZnO、氧化铜CuO其余材料等按照配比搅拌球磨混合,用少量丙酮稀释,高速搅拌(7000r/min)20min,使无机材料充分分散,加入8%的聚乙烯醇进行喷雾造粒,然后置于130℃烘箱中1h,就可以得到本配方的电容器,其介电常数为3000,介质损耗小于0.0005,耐压强度大于16KV/mm,温度特性在-40,电容量变化不大于10%,在85度不小于-15%,且呈线性变化的高性能负温度系数陶瓷材料。

Claims (1)

1.一种高性能热敏陶瓷材料,其特征在于由二氧化锰MnO280~84%、氧化镍NiO0.1-1%、四氧化三钴Co3O44-8%、三氧化二铁Fe2O38-10%、氧化锌ZnO0.5-2%、氧化铜CuO3-5%组成的高性能热敏陶瓷材料,其制备方法为:将二氧化锰MnO2、氧化镍NiO、四氧化三钴Co3O4、三氧化二铁Fe2O3、氧化锌ZnO、氧化铜CuO按配比混合后加入聚乙烯醇压制成型,然后在1250到1400摄氏度范围内烧结得到高性能热敏陶瓷材料。
CN201010603128.9A 2010-12-24 2010-12-24 一种高性能热敏陶瓷材料 Expired - Fee Related CN102167577B (zh)