CN100453875C - 一种不锈钢碳素钢复合管的加工方法 - Google Patents
一种不锈钢碳素钢复合管的加工方法 Download PDFInfo
- Publication number
- CN100453875C CN100453875C CNB2004100275180A CN200410027518A CN100453875C CN 100453875 C CN100453875 C CN 100453875C CN B2004100275180 A CNB2004100275180 A CN B2004100275180A CN 200410027518 A CN200410027518 A CN 200410027518A CN 100453875 C CN100453875 C CN 100453875C
- Authority
- CN
- China
- Prior art keywords
- pipe
- composite pipe
- stainless steel
- curved
- carbon steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明公开了一种不锈钢碳素钢复合管的加工方法,包括定尺锯断、锯口处理、弯管工艺、焊接工艺、表面处理,所述的弯管工艺是由穿芯工艺和模具制造工艺组成的。本发明的优点在于,由于采用的材料是不锈钢碳素钢复合管,其表面的不锈钢很薄,所以相对于纯不锈钢管、电镀的碳素钢管来说,成本降低;又对环境无污染。所采用的工艺特殊,不会在弯曲处产生皱折,外观漂亮。
Description
【技术领域】
本发明涉及一种管材的加工方法,特别涉及一种不锈钢碳素钢复合管的加工方法。
【背景技术】
当前机械加工领域所使用的管材,大多数是经过化学电镀处理后的普通的碳素钢管。加工这种钢管的加工工艺也是较为普通的:定尺锯断-锯口处理-弯管-焊接-表面处理。在其表面处理工艺中,对管制品要进行:抛光-酸洗-电镀,这种表面处理工艺不但工序繁琐,增加制造成本,而且会对公共环境造成极大的污染。此外,钢管的弯曲处容易产生皱折。
【发明内容】
为解决目前普通碳素钢管加工工艺中的成本高、环境污染严重、管材弯曲处容易产生皱折等问题,本发明所采用的技术方案是:一种不锈钢碳素钢复合管的加工办法,包括定尺锯断-锯口处理弯管工艺、焊接工艺、表面处理,所述的弯管工艺包括弯芯工艺和模具制造工艺。
所述的穿芯工艺包括,根据待弯复合管的外径、厚度、毛刺存在情况,计算出芯珠的适用尺寸;根据待弯复合管的弯曲角度、弯曲半径,计算出芯珠的连接片尺寸及连接后的芯珠串深入到弯曲部位的尺寸;根据弯管的拉力、摩擦力,计算出能承受弯管的拉力和摩擦力的芯珠的连接片尺寸。
所述的模具制造工艺包括,根据待弯复合管的尺寸、弯曲角度、弯曲半径,采用刨、磨、铣床加工出适合的带有精密R的主弯模;紧密地与主弯模相配合的带有精密R的前、后夹模。
所述的前、后夹模中的后夹模,贴近主弯模的一块是用磷青铜材料制成的。
本发明的优点在于,由于采用的材料是不锈钢碳素钢复合管,其表面的不锈钢很薄,所以相对于纯不锈钢管、电镀的碳素钢管来说,成本低;又无环境污染的问题;所采用的工艺特殊,不会在弯管处产生皱折,外观漂亮。
【具体实施方式】
下面对本发明的技术方案进行具体的描述:
工艺流程:定尺锯断-锯口处理-弯管-焊接-表面处理。
将不锈钢碳素钢复合管管材,用无毛刺切割机按所需尺寸锯断;用打磨机打磨,或用机床等机械处理;采用半自动单头弯管机以穿芯工艺和模具制造工艺对管材进行弯曲;使得高镍焊丝进行焊接,它可以使得碳素钢管的分子结构和化学成分改变到与不锈钢的基本相同,达到表面美观、不易生锈的目的;采用抛光机进行表面抛光。
其中的穿芯工艺:根据待弯复合管的外径尺寸、厚度、毛刺存在情况,计算出芯珠的适用尺寸;根据待弯复合管的弯曲角度、弯曲半径,计算出芯珠的连接片尺寸及连接后的芯珠串深入到弯曲部位的尺寸;根据弯管的拉力、摩擦力,计算出能承受所述弯管的拉力和摩擦力的芯珠的连接片尺寸。
其中的模具制造工艺:根据待弯复合管的尺寸、弯曲角度、弯曲半径,采用刨、磨、铣床加工出适合的带有紧密R的主弯模;紧密地与主弯模相配合地带有精密R的前、后夹模。两块前后夹模均为铁制的,而后夹模中贴近主弯模的一块是用磷青铜材料制成的。
Claims (2)
1、一种不锈钢碳素钢复合管的加工方法,包括定尺锯断、锯口处理、弯管工艺、焊接工艺、表面处理,其特征在于:所述的弯管工艺包括穿芯工艺和模具制造工艺;所述的穿芯工艺包括,根据待弯复合管的外径尺寸、厚度、毛刺存在情况,计算出芯珠的适用尺寸;根据待弯复合管的弯曲角度、弯曲半径,计算出芯珠的连接片尺寸及连接后的芯珠串深入到弯曲部位的尺寸;根据弯管的拉力、摩擦力,计算出能承受所述弯管的拉力和摩擦力的芯珠的连接片尺寸;所述的模具制造工艺包括,根据待弯复合管的尺寸、弯曲角度、弯曲半径,采用刨、磨、铣床加工出适合的带有精密R的主弯模;紧密地与主弯模相配合地带有精密R的前、后夹模。
2、如权利要求1所述的不锈钢碳素钢复合管的加工方法,其特征在于:所述的前、后夹模中的后夹模,贴近主弯模的一块是用磷青铜材料制成的。