CA1284930C - Methode de preparation d'un metal allant a la mise en forme a froid - Google Patents
Methode de preparation d'un metal allant a la mise en forme a froidInfo
- Publication number
- CA1284930C CA1284930C CA000509291A CA509291A CA1284930C CA 1284930 C CA1284930 C CA 1284930C CA 000509291 A CA000509291 A CA 000509291A CA 509291 A CA509291 A CA 509291A CA 1284930 C CA1284930 C CA 1284930C
- Authority
- CA
- Canada
- Prior art keywords
- zinc
- film
- metal
- treatment
- phosphate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C22/00—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C22/78—Pretreatment of the material to be coated
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C22/00—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C22/82—After-treatment
- C23C22/83—Chemical after-treatment
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C22/00—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C22/05—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions
- C23C22/06—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6
- C23C22/07—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6 containing phosphates
- C23C22/08—Orthophosphates
- C23C22/12—Orthophosphates containing zinc cations
Landscapes
- Chemical & Material Sciences (AREA)
- General Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Chemical Treatment Of Metals (AREA)
- Metal Extraction Processes (AREA)
- Lubricants (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
- Forging (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60111590A JPS61269929A (ja) | 1985-05-24 | 1985-05-24 | 金属材料の潤滑処理方法 |
JP60-111590 | 1985-05-24 |
Publications (1)
Publication Number | Publication Date |
---|---|
CA1284930C true CA1284930C (fr) | 1991-06-18 |
Family
ID=14565220
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CA000509291A Expired - Fee Related CA1284930C (fr) | 1985-05-24 | 1986-05-15 | Methode de preparation d'un metal allant a la mise en forme a froid |
Country Status (6)
Country | Link |
---|---|
JP (1) | JPS61269929A (fr) |
AU (1) | AU580408B2 (fr) |
BR (1) | BR8602325A (fr) |
CA (1) | CA1284930C (fr) |
GB (1) | GB2175611B (fr) |
NZ (1) | NZ215988A (fr) |
Families Citing this family (16)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6268647A (ja) * | 1985-09-21 | 1987-03-28 | Dowa Teppun Kogyo Kk | 塑性加工用金属材料における潤滑性金属被膜の製造方法 |
JPS6283477A (ja) * | 1985-10-08 | 1987-04-16 | Nippon Parkerizing Co Ltd | 鉄鋼材の表面処理方法 |
JPS63174748A (ja) * | 1987-01-14 | 1988-07-19 | Sumitomo Metal Ind Ltd | 冷間鍛造用Ti及びTi合金線材の連続伸線方法 |
JPS63190180A (ja) * | 1987-02-02 | 1988-08-05 | Sumitomo Metal Ind Ltd | ステンレス線材の連続伸線方法 |
JP2701277B2 (ja) * | 1987-12-09 | 1998-01-21 | 日産自動車株式会社 | ワーク加工方法 |
JPH03215684A (ja) * | 1990-01-18 | 1991-09-20 | Nippon Parkerizing Co Ltd | アルミニウムの潤滑皮膜処理法 |
US5277048A (en) * | 1992-11-20 | 1994-01-11 | Crs Holdings, Inc. | Process and apparatus for treating the surface of an elongated, steel alloy form to facilitate cold working thereof |
FR2790983B1 (fr) * | 1999-03-15 | 2001-06-22 | Dacral Sa | Procede de formage de pieces metalliques par deformation a froid |
JP4495325B2 (ja) * | 1999-12-20 | 2010-07-07 | 株式会社アーレスティ | エンジンブロックの製造方法 |
TW571000B (en) * | 2001-10-19 | 2004-01-11 | Nihon Parkerizing | Methods of preparing metal wires for plastic processing |
US9267184B2 (en) | 2010-02-05 | 2016-02-23 | Ati Properties, Inc. | Systems and methods for processing alloy ingots |
US8230899B2 (en) | 2010-02-05 | 2012-07-31 | Ati Properties, Inc. | Systems and methods for forming and processing alloy ingots |
US10207312B2 (en) | 2010-06-14 | 2019-02-19 | Ati Properties Llc | Lubrication processes for enhanced forgeability |
US8789254B2 (en) | 2011-01-17 | 2014-07-29 | Ati Properties, Inc. | Modifying hot workability of metal alloys via surface coating |
US9539636B2 (en) | 2013-03-15 | 2017-01-10 | Ati Properties Llc | Articles, systems, and methods for forging alloys |
EP3371346A4 (fr) * | 2015-11-05 | 2018-11-21 | Phosfan Ltd. | Revêtements composites au phosphate |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
AU426079B2 (en) * | 1968-02-09 | 1972-07-17 | Fuji Iron & Steel Company Limited | Surface treated steel sheet suitable for forming |
DE3270379D1 (en) * | 1981-08-19 | 1986-05-15 | Pennwalt Corp | Cold forming lubricants and process |
-
1985
- 1985-05-24 JP JP60111590A patent/JPS61269929A/ja active Granted
-
1986
- 1986-04-29 NZ NZ215988A patent/NZ215988A/en unknown
- 1986-05-05 AU AU57103/86A patent/AU580408B2/en not_active Expired - Fee Related
- 1986-05-15 CA CA000509291A patent/CA1284930C/fr not_active Expired - Fee Related
- 1986-05-22 BR BR8602325A patent/BR8602325A/pt unknown
- 1986-05-23 GB GB8612650A patent/GB2175611B/en not_active Expired
Also Published As
Publication number | Publication date |
---|---|
JPS61269929A (ja) | 1986-11-29 |
AU5710386A (en) | 1986-11-27 |
NZ215988A (en) | 1988-04-29 |
GB8612650D0 (en) | 1986-07-02 |
BR8602325A (pt) | 1987-01-21 |
GB2175611A (en) | 1986-12-03 |
JPH0355204B2 (fr) | 1991-08-22 |
AU580408B2 (en) | 1989-01-12 |
GB2175611B (en) | 1989-07-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA1284930C (fr) | Methode de preparation d'un metal allant a la mise en forme a froid | |
CN106687571B (zh) | 硫酸盐的用途及通过在成型机中的成型制造钢构件的方法 | |
US20030130137A1 (en) | Aqueous lubricant for plactic working of metallic material and method of lubricant film processing | |
JPWO2003035929A1 (ja) | 塑性加工用金属線材の製造方法 | |
EP0412788A1 (fr) | Méthode de lubrification pour traitement de matériaux mÀ©talliques lors du travail plastique à froid | |
Taha-Tijerina et al. | Tribological evaluation of electroless Ni–B coating on metal-working tool steel | |
US4944813A (en) | Process for phosphating metal surfaces | |
Tomala et al. | Tool–solid lubricant–workpiece interactions in high temperatures applications | |
Patil et al. | Tin layer as a solid lubricant for cold tube drawing processes | |
CN108138327B (zh) | 耐腐蚀性和加工后的外观优异的钢线材 | |
US10914009B2 (en) | Method for manufacturing non-phosphate coated metal material for cold heading-plastic working process | |
CA1154745A (fr) | Compose de trefilage, et mode d'emploi connexe | |
Devaneyan et al. | Enhanced corrosion and wear behavior of nano titanium carbide reinforced polyurethane PMC coating on aluminium 7075 | |
CA2652478C (fr) | Methode de travail a froid de tuyau d'acier | |
JP3778026B2 (ja) | 冷間伸線加工用潤滑剤、冷間伸線材およびその製造方法 | |
Sharma et al. | Corrosion and wear study of Ni-P-PTFE-Al2O3 coating: the effect of heat treatment | |
JPH0872197A (ja) | 深絞り性に優れた潤滑鋼板 | |
US5493886A (en) | Elevated temperature metal forming lubrication method | |
Jayaraj et al. | INVESTIGATION ON THE DISTRIBUTION AND CONCENTRATION OF NYLON 6, 6 PARTICLES ON THE WEAR BEHAVIOUR OF ELECTROLESS NICKEL PHOSPHORUS NYLON COMPOSITE COATING. | |
US2329731A (en) | Drawing lubricant | |
JP4113000B2 (ja) | コイリング加工性に優れたオイルテンパー線およびその製造方法 | |
WO2021065025A1 (fr) | Tôle d'acier galvanise traitee en surface et procede de fabrication de celle-ci | |
JPH07164042A (ja) | 潤滑性及び耐食性にすぐれる冷間鍛造用棒鋼線材の製造方法 | |
US6231687B1 (en) | Lubrication treatment method for cold working of steel | |
DE60000228T2 (de) | Verfahren zum verformen metallischer werkstücke durch kaltverformen |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MKLA | Lapsed |