WO2016052968A1 - 친환경 탄약포장용 지관통 - Google Patents

친환경 탄약포장용 지관통 Download PDF

Info

Publication number
WO2016052968A1
WO2016052968A1 PCT/KR2015/010266 KR2015010266W WO2016052968A1 WO 2016052968 A1 WO2016052968 A1 WO 2016052968A1 KR 2015010266 W KR2015010266 W KR 2015010266W WO 2016052968 A1 WO2016052968 A1 WO 2016052968A1
Authority
WO
WIPO (PCT)
Prior art keywords
paper
rosin
adhesive
polysol
paperboard
Prior art date
Application number
PCT/KR2015/010266
Other languages
English (en)
French (fr)
Inventor
장주현
Original Assignee
장주현
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 장주현 filed Critical 장주현
Publication of WO2016052968A1 publication Critical patent/WO2016052968A1/ko

Abstract

내구성이 뛰어나면서 방수 및 방습기능 뿐만 아니라 지환통 내부에 존재하는 습기도 배출이 가능하도록 하는 발수기능이 뛰어난 지환통이 개시되어 있으며, 이러한 기능을 수행하는 지관통이 친환경적인 구성요소로 이루어짐에 따라서 재활용이 가능한 지관통이 제공되어있다. 상기 목적을 달성하기 위해서 본 발명의 바람직한 일 실시예에 따르면, 본 발명인 지관통은 제1 바디(B1) 안쪽에 내삽되며 상부가 제2바디(B2)와 결합하는 제3 바디(B3)로 이루어진 지관통에 있어서, 상기 제1 바디(B1)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30%이상 함침되도록 처리한 제1지(10); 은박지로 구성된 제2지(20); 상기 제1지(10)와 상기 제2지(20)사이에 도포되며, 로진을 알콜에 희석하여 녹인 로진점착제(30); 하나 이상의 판지로 구성된 제3지(40); 상기 제2지(20)와 최초로 접하는 판지(40) 사이에 도포되는 로진점착제(30); 및 상기 제3지(40)의 판지(40)와 판지(40)사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로 이루어지며, 상기 제2 바디(B2)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30% 이상 함침되도록 처리한 제1지(10); 은박지로 구성된 제2지(20); 상기 제1지(10)와 상기 제2지(20) 사이에 도포되며, 로진을 알콜에 희석하여 녹인 로진점착제(30); 하나 이상의 판지로 구성된 제3지(40); 상기 제2지(20)와 최초로 접하는 판지(40) 사이에 도포되는 로진점착제(30); 및 상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이혼합된 로진폴리졸접착제(50)로 이루어지고, 상기 제3 바디(B3)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30%이상 함침되도록 처리한 제1지(10); 하나 이상의 판지로 구성된 제3지(40); 상기 제1지(10)와 최초로 접하는 판지(40)사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50); 상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸90~95%이 혼합된 로진폴리졸접착제(50)로 이루어진다.

Description

친환경 탄약포장용 지관통
본 발명은 로진을 포함하는 절연지 및 접착제들로 구성된 탄약을 보관하는 지관통에 관한 것으로, 더욱 상세하게는 종래의 지관통에 사용되던 아스팔트 또는 파라핀 함침지를 사용하지 않더라도, 내용물의 중량에 따른 내구성을 겸비하면서 방습·방수 및 발수기능을 수행하여 내용물의 부식을 방지하면서 내용물을 보관할 수 있도록하면서도, 작업환경과 위생을 강화하고 환경오염을 예방하며 지관통의 재활용이 가능하도록 함으로써 친환경적으로 구성된 지관통에 관한 것이다.
내용물의 성능을 유지하면서 장기간 내용물을 보관하기 위한 방법으로 종래에는 목재 재질의 보관용기를 사용하다가, 성능과 보관의 취약성으로 인하여 종이를 여러겹으로 중첩하여 만드는 지관통이 사용되고 있다. 지관통에는 다양한 내용물이 수납되어 보관될 수 있지만, 특히 탄약 및 포탄을 보관하기 위한 탄약보관용 지환통은 다른 어떤 보관용기보다도 탄약의 부식을 방지할 수 있는 성능이 요구된다.
지관통은 원지 및 특수한 처리과정을 거친 재료를 중첩하여 만들며, 지관통 내부에 포탄을 수용할 수 있는 보관실과 그 상부를 덮을 수 있는 덮개구조로 이루어진다. 지관의 내피 및 외피가 모두 종이 재질을 바탕으로 한 요소로 이루어지기 때문에 종이의 종류와 그에 따른 두께 및 무게, 종이 코팅 방식의 상이성, 그의 적체 순서에 따른 방수·방습 및 발수처리 효과, 종이의 종류에 대응하는 접착제의 선택이 지관통의 내구성과 기능을 결정하는데 중요한 역할을 한다.
이러한 역할을 수행하기 위하여 공개특허 10-2010-0045958에서는 외피에 해당하는 종이에 아스팔트를 함침시켜 방수 및 방습효과를 높이고자 하였으나, 이는 친환경적이지 못한 한계가 있으며, 등록특허 10-1282484에서는 친환경적인 지관통을 개시함을 발명의 목적으로 하면서 파라핀왁스로 함침시키는 지관통 및 폴리비닐아세테이트접착제를 사용하는 기술적 사상을 청구하고 있으나, 핵심구성인 파라핀 및 폴리비닐아세테이트 접착제는 친환경물질이 아님은 너무나 자명하다. 더구나 파라핀왁스로 종이를 코팅할 경우에는 파라핀의 특성상 종이 위에 코팅된 파라핀 왁스에 크랙이 생겨 방수력 및 방습력을 저하시키는 문제가 발생하며, 파라핀 코팅으로 인하여 크랙이 생기기 때문에 등록특허 10-1282484의 공보상의 방법처럼 로빈으로 롤링하여 제작하는 방법은 현실적으로 수행 불가능한 문제점이 있다. 또한 이러한 유해물질로 구성된 지관통은 인체에 유해한 성분들로 이루어져 있기때문에 작업자 및 사용자가 유해물질에 노출되는 위험성이 있으며, 폐기시에도 환경오염을 발생시키고, 폐기처리비용을 증대시키는 문제점이 있다.
탄약의 야적시 장기간 보관되는 탄약은 공기 중의 수분으로 인하여 탄약의 부식 및 불발의 불량품이 발생하는 확률이 높아지므로, 탄약 및 포탄을 보관하는 지관통은 방수·방습 및 발수기능을 구비해야 할 뿐만 아니라, 그 위험성으로 인하여 일정 강도를 지닌 내구성도 요구된다.
본 발명의 제1 목적은 내구성이 뛰어나면서 방수 및 방습기능 뿐만 아니라 지환통 내부에 존재하는 습기도 배출이 가능하도록 하는 발수기능이 뛰어난 지환통 을 제공하는 것이며, 이러한 기능을 수행하는 지관통이 친환경적인 구성요소로 이루어짐에 따라서 재활용이 가능한 지관통을 제공하는 것이다. 이러한 목적을 수행하기 위한 지관통을 제공하기 위하여 선택되어진 재료 및 그 재료의 적체순서가 개시된다.
본 발명의 제2 목적은 선택되어진 재료에 따른 접착제의 선별이 지관통의 내구성을 결정하는데 중요한 역할을 하므로, 각 재료별로 대응하는 개별 접착제도 개시하는데 있다.
어떠한 재질을 어떠한 순서로 적체시키고, 각 적체 단계에서 어떠한 접착제를 사용하느냐에 따라서 다양한 내용물을 수용할 수 있는 다양한 지관통이 생성되므로, 본 발명을 통하여 내구성 뿐만 아니라 방수 및 방습기능과 지관통 내부에 존재하는 습기도 배출이 용이하도록 하는 발수 기능이 뛰어난 친환경적인 지관통을 제공하고자한다.
상기 목적을 달성하기 위해서 본 발명의 바람직한 일 실시예에 따르면, 본 발명인 지관통은 제1 바디(B1) 안쪽에 내삽되며 상부가 제2바디(B2)와 결합하는 제3 바디(B3)로 이루어진 지관통에 있어서, 상기 제1 바디(B1)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30%이상 함침되도록 처리한 제1지(10);
은박지로 구성된 제2지(20); 상기 제1지(10)와 상기 제2지(20) 사이에 도포되며, 로진을 알콜에 희석하여 녹인 로진점착제(30); 하나 이상의 판지로 구성된 제3지(40); 상기 제2지(20)와 최초로 접하는 판지(40) 사이에 도포되는 로진점착제(30); 및 상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로 이루어지며, 상기 제2 바디(B2)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30% 이상 함침되도록 처리한 제1지(10); 은박지로 구성된 제2지(20); 상기 제1지(10)와 상기 제2지(20) 사이에 도포되며, 로진을 알콜에 희석하여 녹인 로진점착제(30); 하나 이상의 판지로 구성된 제3지(40); 상기 제2지(20)와 최초로 접하는 판지(40) 사이에 도포되는 로진점착제(30); 및 상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로 이루어지고, 상기 제3 바디(B3)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30%이상 함침되도록 처리한 제1지(10); 하나 이상의 판지로 구성된 제3지(40); 상기 제1지(10)와 최초로 접하는 판지(40)사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50); 상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로 이루어진다.
본 발명의 다른 실시예에 따르면, 본 발명인 지관통은 상기 제1지(20)의 함침시 및 상기 로진점착제(30)의 희석시에는 원하는 색상을 띄도록 안료가 첨가된다.
탄약과 같은 내용물을 보관함에 있어서, 내용물의 부식을 방지할 뿐만 아니라 무게가 나가는 내용물도 장기간 보관이 가능한 내구성을 겸비하면서도 친환경적인 지관통을 제공한다.
상술한 지환통으로 활용되기 위해서는 지환통을 구성하는 재질의 종류, 두께, 평량, 선택된 재질의 적체순서 및 그 재질의 상호결합을 위한 접착이 중요한 역할을 하므로, 본 발명에서 개시하는 재료와 그 재료의 적체순서,
이에 대응하는 접착제를 통하여 탄약을 안전하게 보관하면서도 친환경적으로 재활용할 수 있는 지관통을 제공할수 있다.
지관통은 어떠한 재질을 어떠한 순서로 적체시키고, 각 적체단계에서 어떠한 접착제를 사용하느냐에 따라서 내구성이 상이한 지환통이 생성되므로, 본 발명을 통하여 친환경적이면서도 내구성 뿐만 아니라 방수 및 방습기능과 지환통 내부에 존재하는 습기도 배출이 용이하도록 하는 발수기능이 뛰어난 지환통을 제공할 수 있다.
본 발명에서 사용된 로진폴리졸접착제는 건조속도가 빠른 장점으로 인하여 수분적체율이 감소하므로, 접착제로서의 강도가 강해질 뿐만 아니라, 점착력이 강하므로 접착으로 인하여 방수역할을 증대시키는 특징이 있으며,
본 발명에서 사용된 또 다른 접착제인 로진점착제는 경화속도가 빨라서 기포가 생기지 않으므로 강도가 세지며,
방수력이 강화되고, 인화점이 높아서 방수효과 및 방열효과가 증대되는 강점이 있다.
또한, 본 발명에서 사용된 제1지를 구성하는 절연지는 로진을 흡수한 절연지로 구성함에 따라서 친환경적인데다가, 방수 및 방열효과를 도모할 수 있는 이점이 있다.
도 1은 본 발명인 친환경 탄약 포장용 지관통의 외부 사시도이다.
도 2는 본 발명의 구조를 도시하기 위한 단면도이다.
도 1 및 도 2를 참고하여 본 발명의 바람직한 일 실시 예를 설명하면, 본 발명인 친환경 탄약 포장용 지관통은 국방규격에 맞는 종래의 제품과 같이 탄약이 수용되도록 몸통부를 이루는 제1바디(B1), 제3바디(B3) 및 제3바디(B3)와 결합하여 덮개를 이루는 제2바디(B2)로 구성되며, 제1바디(B1) 하단과 제2바디(B2)상단 및 제3바디(B3)상단에는 캡(CAP)이 씌워져 마무리 처리된다. 이러한 외관적인 구성은 국방부의 규격에 명시되어 있는 것으로서 탄약을 수용하기 위한 지관통은 이러한 일반적인 외부 구조를 지니고 있다. 단지 이러한 지관통의 기술적인 차별화를 가져오는 요소들은 탄약을 보관하기 위한 방수, 방습, 내열기능을 수행하기 위하여 각 지관통의 구성요소를 어떠한 구성으로 배치하고 설계하느냐에 달려 있다. 본 발명에서는 지관통의 상술한 기능들을 수행하면서도 친환경적으로 구성하여 재활용이 가능한 차별화된 친환경 탄약 포장용 지관통을 이하 개시한다.
본 발명인 지관통은 크게 3부분으로 분별되는데, 바깥 몸통을 이루는 제1 바디(B1), 제1바디(B1) 안쪽에 내삽되는 제3바디(B3), 제3바디(B3)와 결합하여 덮개부를 형성하는 제2 바디(B2)로 이루어진다.
상기 제1 바디(B1)는 제1지(10)가 외부에 노출되게 되는데, 제1지(10)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜서, 절연지 상에 로진이 30%이상 함침되도록 처리한다. 로진(Rosin)은 소나무 에서 추출되는 천연물 화합물로 1개의 카르복시기를 갖는 불포화 이클로 화합물이며, 주로 ABS(Acrylonitrile Butadiene styrene Copolymer)수지 제조용 유화제 및 기타 점접착제 에스테르(ester)수지, 잉크용 로진 변성 수지, 제지공업용 등의 원료로 사용되고 있다. 본 지관통에 사용되는 로진은 검로진이며, 로진산(Rosin acid)의 에스테르 반응으로 제조한다. 제1지(10)의 제조에 투여되는 로진 함량은 함침시킬 종이의 양에 따라서 가감을 하게 되며, 알콜도 로진을 녹일 만큼만 투여하게 된다. 기호에 따라 색상을 나타내기 위하여 안료를 첨가하기도 하는데, 안료와 로진과 알콜이 희석된 용액에 로진이 흡수되도록 절연지를 함침시키며, 함침률이 30%이상 나오도록 한다. 친환경적으로 제조된 제1지(10)를 통하여 지관통의 정전기를 방지하게 되며, 불꽃을 가까이 대었을 때 인화되는 최저의 온도도 높이게 되어 지관통의 인화점이 증대되는 효과가 있다.
제2지(20)는 제1지(10)의 바로 안쪽에 위치하게 되며, 내열성 강화를 위하여 은박지로 구성된다. 상기 제1지(10)와 상기 제2지(20) 사이에는 로진을 알콜에 희석하여 녹인 로진점착제(30)가 도포된다. 로진점착제(30)는 제2지(20)인 은박지를 제1지(10)와 강하게 접착함으로써 기포가 생기지 않고, 건조를 빠르게 함으로써 강도 및 방수력을 강화시키는 역할을 수행한다. 또한, 인화점도 높아지기 때문에 지관통 전체의 내열성도 증대되는 효과가 있다.
제3지(40)는 하나 이상의 판지로 구성되며, 제2지(20)의 안쪽에 부착된다. 상기 제2지(20)와 최초로 접하는 판지(40) 사이에는 로진점착제(30)가 도포되며, 상기 제3지(40)의 판지(40)와 판지(40) 사이에는 로진폴리졸접착제(50)가 도포된다. 로진폴리졸 접착제(50)는 로진 5~10%과 폴리졸(90~95%)이 혼합된 것으로서 건조속도가 빠른 장점으로 인하여 수분적체율이 감소하므로, 접착제로서의 강도가 강해질 뿐만 아니라, 점착력이 강하므로 접착으로 인하여 방수역할을 증대시키는 특징이 있다. 도 2에는 설명상의 편의를 위하여 로진점착제(30) 및 로진폴리졸접착제(50)가 도포되는 부분을 굵고 짧게 표기하였으나, 이 부분만 도포되는 것이 아니라, 접착제는 접촉면 전체에 골고루 도포된다.
제2 바디(B2)는 덮개부의 역할을 수행하는 부분으로서, 제1지(10)가 외부에 노출되게 되는데, 제1지(10)는 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜서, 절연지 상에 로진이 30%이상 함침되도록 처리한다. 이 때의 로진 함량은 함침시킬 종이의 양에 따라서 가감을 하게 되며, 알콜도 로진을 녹일만큼만 투여하게 된다. 기호에 따라 색상을 나타내기 위하여 안료를 첨가하기도 하는데, 안료와 로진과 알콜이 희석된 용액에 로진이 흡수되도록 절연지를 함침시키며, 함침률이 30%이상 나오도록 한다.
제2 바디(B2)의 제2지(20)는 제1지(10)의 바로 안쪽에 위치하게 되며, 내열성 강화를 위하여 은박지로 구성된다. 상기 제1지(10)와 상기 제2지(20) 사이에는 로진을 알콜에 희석하여 녹인 로진점착제(30)가 도포된다. 로진 점착제(30)는 제2지(20)인 은박지를 제1지(10)와 강하게 접착함으로써 기포가 생기지 않고, 건조를 빠르게 함으로써 강도 및 방수력을 강화시키는 역할을 수행한다. 또한, 인화점도 높아지기 때문에 지관통 전체의 내열성도 증대되는 효과가 있다.
제2 바디(B2)의 제3지(40)는 하나 이상의 판지로 구성되며, 제2지(20)의 안쪽에 부착된다. 상기 제2지(20)와 최초로 접하는 판지(40) 사이에는 로진점착제(30)가 도포되며, 상기 제3지(40)의 판지(40)와 판지(40) 사이에는 로진폴리졸접착제(50)가 도포된다. 로진폴리졸 접착제(50)는 로진 5~10%과 폴리졸(90~95%)이 혼합된 것으로서 건조속도가 빠른 장점으로 인하여 수분적체율이 감소하므로, 접착제로서의 강도가 강해질 뿐만 아니라, 점착력이 강하므로 접착으로 인하여 방수역할을 증대시키는 특징이 있다.
제3 바디(B3)는 제1 바디(B1)의 안쪽에 내삽되어 있는 부분으로서, 제1지(10)가 바깥부분에 위치하며, 제1지(10)는 상술한 바와 같이 절연지를 로진 및 알콜이 혼합된 희석액에 함침시켜 절연지 상에 로진이 30%이상 함침되도록 처리한다.
제3바디(B3)의 제1지(10) 안쪽에는 하나 이상의 판지로 구성된 제3지(40) 위치한다. 상기 제1지(10)와 최초로 접하는 판지(40)사이에는 로진폴리졸접착제(50)가 도호되며, 상기 제3지(40)의 판지(40)와 판지(40) 사이에도 로진 5~10%과 폴리졸(90~95%)이 혼합된 로진폴리졸접착제(50)가 도포된다.
상술한 구성에 사용된 상기 제1지(10) 및 상기 로진점착제(30)에는 제1지(10)의 함침과정 및 로진점착제(30)의 희석과정에서 국방색 등의 원하는 색상을 띄도록 안료가 첨가되는 것이 가능하다.
앞서 설명한 본 발명을 실시하기 위한 구체적인 내용에는 본 발명의 바람직한 실시 예를 참조하여 설명하였지만, 해당 기술분야의 당업자라면 후술 될 특허청구범위에 기재된 발명의 사상 및 기술 영역으로부터 벗어나지 않는 범위 내에서 본 발명을 다양하게 수정 및 변형시킬 수 있음을 이해할 수 있을 것이다.
[부호의 설명]
CAP:캡
B1:제1바디
B2:제2바디
B3:제3바디
10:제1지
20:제2지
30:로진점착제
40:제3지
50:로진폴리졸접착제

Claims (2)

  1. 제1 바디(B1) 안쪽에 내삽되며 상부가 제2바디(B2)와 결합하는 제3 바디(B3)로 이루어진 지관통에 있어서,
    상기 제1 바디(B1)는
    상기 제1 바디의 외부로 노출되며 절연지 상에 로진이 30%이상 함침된 제1지(10);
    은박지로 구성된 제2지(20);
    상기 제1지(10)와 상기 제2지(20) 사이에 도포되는 로진점착제(30);
    하나 이상의 판지로 구성된 제3지(40);
    상기 제2지(20)와 최초로 접하는 판지(40) 사이에 도포되는 로진점착제(30); 및
    상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로 이루어지며
    상기 제2 바디(B2)는
    상기 제2 바디의 외부로 노출되며 절연지 상에 로진이 30%이상 함침된 제1지(10);
    은박지로 구성된 제2지(20);
    상기 제1지(10)와 상기 제2지(20) 사이에 도포되는 로진점착제(30);
    하나 이상의 판지로 구성된 제3지(40);
    상기 제2지(20)와 최초로 접하는 판지(40) 사이에 도포되는 로진점착제(30); 및
    상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로 이루어지고
    상기 제3 바디(B3)는
    상기 제3 바디의 외부로 노출되며 절연지 상에 로진이 30%이상 함침된 제1지(10);
    하나 이상의 판지로 구성된 제3지(40);
    상기 제1지(10)와 최초로 접하는 판지(40)사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50);
    상기 제3지(40)의 판지(40)와 판지(40) 사이에 도포되며, 로진 5~10%과 폴리졸 90~95%이 혼합된 로진폴리졸접착제(50)로
    이루어지는 것을 특징으로 하는 친환경 탄약포장용 지관통.
  2. 제1항에 있어서,
    상기 제1지(10)의 함침시 및 상기 로진점착제(30)의 희석시에는 원하는 색상을 띄도록 안료가 첨가되는 것을 특징으로 하는 친환경 탄약포장용 지관통.
PCT/KR2015/010266 2014-10-02 2015-09-30 친환경 탄약포장용 지관통 WO2016052968A1 (ko)