WO2014136336A1 - センサ装置 - Google Patents

センサ装置 Download PDF

Info

Publication number
WO2014136336A1
WO2014136336A1 PCT/JP2013/082671 JP2013082671W WO2014136336A1 WO 2014136336 A1 WO2014136336 A1 WO 2014136336A1 JP 2013082671 W JP2013082671 W JP 2013082671W WO 2014136336 A1 WO2014136336 A1 WO 2014136336A1
Authority
WO
WIPO (PCT)
Prior art keywords
resin
chip package
chip
sensor device
housing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2013/082671
Other languages
English (en)
French (fr)
Japanese (ja)
Inventor
裕樹 中土
河野 務
翼 渡辺
忍 田代
徳安 昇
暁 上ノ段
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Astemo Ltd
Original Assignee
Hitachi Automotive Systems Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Automotive Systems Ltd filed Critical Hitachi Automotive Systems Ltd
Publication of WO2014136336A1 publication Critical patent/WO2014136336A1/ja
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Links

Images

Classifications

    • G—PHYSICS
    • G01—MEASURING; TESTING
    • G01L—MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE
    • G01L19/00—Details of, or accessories for, apparatus for measuring steady or quasi-steady pressure of a fluent medium insofar as such details or accessories are not special to particular types of pressure gauges
    • G01L19/0007—Fluidic connecting means
    • G01L19/0023—Fluidic connecting means for flowthrough systems having a flexible pressure transmitting element
    • G—PHYSICS
    • G01—MEASURING; TESTING
    • G01F—MEASURING VOLUME, VOLUME FLOW, MASS FLOW OR LIQUID LEVEL; METERING BY VOLUME
    • G01F1/00—Measuring the volume flow or mass flow of fluid or fluent solid material wherein the fluid passes through a meter in a continuous flow
    • G01F1/68—Measuring the volume flow or mass flow of fluid or fluent solid material wherein the fluid passes through a meter in a continuous flow by using thermal effects
    • G01F1/684—Structural arrangements; Mounting of elements, e.g. in relation to fluid flow
    • G01F1/6842—Structural arrangements; Mounting of elements, e.g. in relation to fluid flow with means for influencing the fluid flow
    • G—PHYSICS
    • G01—MEASURING; TESTING
    • G01F—MEASURING VOLUME, VOLUME FLOW, MASS FLOW OR LIQUID LEVEL; METERING BY VOLUME
    • G01F1/00—Measuring the volume flow or mass flow of fluid or fluent solid material wherein the fluid passes through a meter in a continuous flow
    • G01F1/68—Measuring the volume flow or mass flow of fluid or fluent solid material wherein the fluid passes through a meter in a continuous flow by using thermal effects
    • G01F1/684—Structural arrangements; Mounting of elements, e.g. in relation to fluid flow
    • G01F1/6845—Micromachined devices
    • G—PHYSICS
    • G01—MEASURING; TESTING
    • G01L—MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE
    • G01L19/00—Details of, or accessories for, apparatus for measuring steady or quasi-steady pressure of a fluent medium insofar as such details or accessories are not special to particular types of pressure gauges
    • G01L19/14—Housings
    • G01L19/141—Monolithic housings, e.g. molded or one-piece housings
    • G—PHYSICS
    • G01—MEASURING; TESTING
    • G01L—MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE
    • G01L19/00—Details of, or accessories for, apparatus for measuring steady or quasi-steady pressure of a fluent medium insofar as such details or accessories are not special to particular types of pressure gauges
    • G01L19/14—Housings
    • G01L19/148—Details about the circuit board integration, e.g. integrated with the diaphragm surface or encapsulation
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W74/00—Encapsulations, e.g. protective coatings
    • H10W74/01—Manufacture or treatment
    • H10W74/016—Manufacture or treatment using moulds
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W72/00—Interconnections or connectors in packages
    • H10W72/851—Dispositions of multiple connectors or interconnections
    • H10W72/874—On different surfaces
    • H10W72/884—Die-attach connectors and bond wires
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W74/00—Encapsulations, e.g. protective coatings
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W74/00—Encapsulations, e.g. protective coatings
    • H10W74/10—Encapsulations, e.g. protective coatings characterised by their shape or disposition
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W74/00—Encapsulations, e.g. protective coatings
    • H10W74/10—Encapsulations, e.g. protective coatings characterised by their shape or disposition
    • H10W74/111—Encapsulations, e.g. protective coatings characterised by their shape or disposition the semiconductor body being completely enclosed
    • H10W74/114—Encapsulations, e.g. protective coatings characterised by their shape or disposition the semiconductor body being completely enclosed by a substrate and the encapsulations
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W90/00—Package configurations
    • H10W90/701—Package configurations characterised by the relative positions of pads or connectors relative to package parts
    • H10W90/751—Package configurations characterised by the relative positions of pads or connectors relative to package parts of bond wires
    • H10W90/753—Package configurations characterised by the relative positions of pads or connectors relative to package parts of bond wires between laterally-adjacent chips

Definitions

  • the present invention relates to the technology of a sensor device such as a flow rate sensor module.
  • the present invention also relates to the molding technology of the chip package and housing of the sensor device.
  • an internal control engine such as a car is provided with an electronically controlled fuel injection device.
  • This device has the role of operating the internal combustion engine efficiently by appropriately adjusting the amounts of gas and fuel flowing into the internal combustion engine. Therefore, in the electronically controlled fuel injection device, it is necessary to accurately grasp the gas flowing into the internal combustion engine. From this, the electronically controlled fuel injection device is provided with a flow rate sensor (also referred to as an air flow sensor or the like) that measures the flow rate of gas.
  • a flow rate sensor also referred to as an air flow sensor or the like
  • a chip package having a structure in which a semiconductor chip including a flow rate detecting portion, a control circuit portion and the like is mounted on a substrate and sealed and molded with a first resin.
  • a sensor module having a structure in which a housing or a housing is molded with a second resin so as to cover the chip package and the periphery thereof. Further, in particular, there is a technique of integrally molding the first resin and the second resin.
  • a chip package on which a first semiconductor chip including a flow rate detection unit and a second semiconductor chip including a control circuit unit are mounted on a substrate, and a resin housing are separately manufactured. Many methods and structures are used to attach the chip package to the housing using an adhesive.
  • Patent Document 1 JP-A 2008-111859
  • Patent Document 1 semiconductor pressure sensor device
  • semiconductor pressure sensor device in a semiconductor pressure sensor device having a structure in which a sensor module containing a semiconductor pressure sensor portion is integrally molded in an outer case, the problems of air tightness and lead corrosion are prevented. And “Providing a semiconductor pressure sensor device with improved reliability of sealing performance”. “The semiconductor pressure sensor device is composed of a sensor module insert-molded with a first resin, and an outer case formed by further insert-molding the sensor module with a second resin to form a connector portion. There is a description of That is, Patent Document 1 describes an integrated structure by two-step resin molding of a sensor module molded with a first resin to expose a sensor unit and a housing molded with a second resin. . In particular, it is described that the first resin is molded with a thermosetting resin, and the second resin is molded with a thermoplastic resin.
  • Patent Document 1 there is a structure of a sensor device by a two-step resin molding or integral molding method using first and second resins. That is, a chip package formed by mounting a semiconductor chip including a detection unit and a semiconductor chip including a control circuit unit on a substrate is sealed and molded in advance with a first resin, and thereafter the periphery of the chip package is integrated with a second resin. Molding to form a housing.
  • the material cost can be greatly reduced.
  • the chip package and the housing have been separately manufactured, but in the integrated molding method described above, when molding the housing with the second resin, molding is carried out with the chip package with the first resin contained therein. Since this can be done, it is possible to reduce the number of processes, that is, to improve the manufacturing efficiency. Furthermore, since molding is performed in a state where the periphery of the chip package is fixed by a mold for molding the second resin, variations in mounting of the chip package on the housing can be suppressed more than the manufacturing method using an adhesive.
  • the structure of the housing and the chip package spatially divides the predetermined detection unit side and the control circuit unit side to form a circuit chamber or the like in the housing. And a structure that ensures airtightness and the like.
  • the adhesion is poor, for example, there is a gap between the portion of the chip package by the first resin and the portion of the housing by the second resin, airtightness in the space such as the circuit chamber inside the housing is descend.
  • a dividing wall as a part of the housing is provided to the chip package, and a space on the detection unit side and a space on the control circuit unit side are divided.
  • a circuit room is provided on the control circuit side inside the housing to protect the lead frame and the like.
  • the gas or the contaminant may flow into the circuit chamber. This reduces the protection of the lead frame and the like.
  • An object of the present invention is to provide a technology capable of reducing a load on a control circuit portion or the like in a chip package due to resin molding shrinkage with respect to the integrated molding of a chip package and a housing in a sensor device It is.
  • Another object of the present invention is to provide a technique capable of enhancing the adhesion of the resin and securing or improving the airtightness.
  • a typical embodiment of the present invention is a sensor device or the like, which is characterized by having the following configuration.
  • the first semiconductor chip including the detection unit and the second semiconductor chip including the control circuit unit are mounted on the substrate surface, and the detection unit is exposed.
  • a chip package sealed and molded with a first resin, and covering at least a part of the periphery of the chip package so that the detection unit is exposed and in contact with a part of the chip package A housing molded of a second resin, and the chip package is disposed on the first surface corresponding to the side on which the second semiconductor chip is mounted, the control circuit unit or the second semiconductor chip being disposed
  • a thick portion is provided in a third area where the first area and the second area in contact with a part of the housing are overlapped.
  • the semiconductor chip including the detection unit and the control circuit unit is mounted on the substrate surface, and the detection unit is sealed and molded with the first resin so as to be exposed.
  • a chip package, and a housing molded of a second resin so as to cover at least a part of the periphery of the chip package and expose the detection unit and to be in contact with a part of the chip package;
  • the chip package is disposed such that the first region in which the control circuit unit is disposed is in contact with a portion of the housing on a first surface corresponding to the side on which the semiconductor chip is mounted.
  • a thick portion is provided in a third area where the two areas overlap.
  • the thick portion of the chip package is provided in the entire first region on the first surface.
  • the thick-walled portion of the chip package is provided on the entire first region on the first surface.
  • the thick portion of the chip package has one or more concave portions or convex portions on the surface in contact with the second resin.
  • the control circuit portion or the like in the chip package due to resin molding shrinkage.
  • the load can be reduced.
  • the adhesion of the resin can be enhanced and the airtightness can be secured or improved.
  • FIG. 5 is a diagram showing an XY planar configuration in the vicinity of a chip package of the flow rate sensor module of the first embodiment.
  • FIG. 7 is a diagram showing an XZ cross-sectional configuration in the vicinity of a chip package of the flow rate sensor module of the first embodiment.
  • FIG. 6 is a view showing an example of the XZ cross-sectional configuration including one example of the shape of the housing of the flow rate sensor module of the first embodiment.
  • FIG. 6 is a diagram showing an XZ cross-sectional configuration of a model of a thick portion of the chip package of the first embodiment.
  • FIG. 5 is an enlarged view showing an XZ cross section of an overlap of each part including the thick part of the chip package of the first embodiment.
  • FIG. 18 is a diagram showing an XZ cross-sectional configuration in the vicinity of the chip package of the flow rate sensor module of the modification of the first embodiment. It is a figure which shows XY planar structure of the flow sensor module which is a sensor apparatus of Embodiment 2 of this invention.
  • FIG. 16 is a diagram showing an XZ cross-sectional configuration in the vicinity of the chip package of the second embodiment. It is a figure which shows XY plane structure of the vicinity of the chip package of the flow sensor module which is a sensor apparatus of Embodiment 3 of this invention.
  • FIG. 18 is a diagram showing an XZ cross-sectional configuration in the vicinity of the chip package of the third embodiment. It is a figure which shows XZ cross-sectional structure of the vicinity of the chip package of the flow sensor module which is a sensor apparatus of Embodiment 4 of this invention.
  • FIG. 18 is a diagram showing an XZ cross-sectional configuration in the vicinity of a chip package of a flow rate sensor module according to a modification of the fourth embodiment.
  • (A), (b) is a figure which shows the structure of the analysis model corresponding to the flow sensor module of a prior art example.
  • FIG. 5 is a view showing a cross-sectional configuration of an analysis model corresponding to the flow rate sensor module of the first embodiment.
  • FIG. 10 is a view showing a cross-sectional configuration of an analysis model corresponding to the flow rate sensor module of the second embodiment.
  • FIG. 18 is a view showing a cross-sectional configuration of an analysis model corresponding to the flow rate sensor module of the third embodiment.
  • FIG. 17 is a diagram showing the results of equivalent strain due to load on the second chip according to the analysis models of Embodiments 1 to 3 in comparison with the conventional example. It is a figure which shows XY plane structure of the flow sensor module which is a sensor apparatus of a prior art example. It is a figure which shows the XZ cross-section structure of the vicinity of the chip package of the flow sensor module of a prior art example.
  • FIG. 18 is a diagram showing an XZ cross-sectional configuration in the vicinity of a chip package of a flow rate sensor module according to a modification of the second embodiment.
  • the present flow rate sensor module (for example, FIG. 3) is a two-step resin molding structure having a chip package 10 of a first resin and a housing 20 of a second resin integrally molded on the outside thereof.
  • the chip package 10 has a structure in which a semiconductor chip including a flow rate detection unit and its control circuit unit is mounted on a substrate, and sealed and molded with a first resin. For example, it is sealed and formed by the first resin in a form having an opening on the side of the first chip 11 including the flow rate detection unit. Then, the flow rate sensor module is configured by integrally molding the second resin so as to cover the periphery of the chip package 10 and form the housing 20 including the dividing wall 21.
  • This flow rate sensor module can reduce the load on the control circuit unit and the like due to the molding of the first and second resins, and can increase the adhesion of the first and second resins to ensure the airtightness of the circuit chamber.
  • the control circuit unit 4 or the second chip 12 including the same on the main surface (f1 in FIG. 3) corresponding to the side on which the semiconductor chip is mounted on the chip package 10 with the first resin.
  • the thick portion 13 is provided corresponding to the third region (R5) overlapping in a plan view from the Z direction.
  • the thickness or volume of the first resin in the region (R5) is made larger than that in the other region, for example, the region where the second chip 12 is not disposed. Reduce the thickness or volume.
  • the thick portion 13 in the chip package 10 By providing the thick portion 13 in the chip package 10, the rigidity in the vicinity of the control circuit portion 4 or the second chip 12 in the chip package 10 is enhanced. Thereby, the load or stress on the control circuit unit 4 or the like through the first resin due to the molding shrinkage of the second resin, in particular, in the integral molding of the chip package 10 and the housing 20 is reduced. Further, by providing the thick portion 13 in the chip package 10, the contact area between the surface of the chip package 10 and the surface of the dividing wall 21 which is a part of the housing 20 is enlarged to improve the adhesion. Accordingly, the airtightness of the circuit chamber 6 (FIG. 1) and the like inside the housing 20 can be maintained or improved along with the reduction of the load.
  • FIG. 19 shows the entire XY plane configuration of the flow rate sensor module of the conventional example.
  • FIG. 20 shows an XZ cross-sectional configuration in the vicinity of the chip package of the flow rate sensor module of the conventional example.
  • the conventional flow sensor module has a chip package 10 and a housing 20 covering the periphery thereof.
  • A1 is an area where the first chip 11 is disposed, the diaphragm 3 is exposed, and the flow path 5 is formed.
  • a2 is an area where the second chip 12 is disposed and the lead frame 7 is exposed and becomes the circuit chamber 6;
  • a3 shows the field where dividing wall 21 which is a part of housing 20 is arranged.
  • the front surface (f1) and the back surface (f2) of the chip package 10 are flat surfaces, and a dividing wall which is a part of the housing 20 by the second resin in the upper and lower portions in the Z direction It forms in the state which 21 touches.
  • a cover or the like which is a part of the housing 20 provided further outside the dividing wall 21 is not shown.
  • the region of the second chip 12 and the region of the dividing wall 21 have a region R0 overlapping in plan view in the Z direction.
  • the X direction of the chip package 10 is shortened, so that the degree of overlap between the area of the second chip 12 and the area of the dividing wall 21 is increased.
  • the molding shrinkage force of the second resin including the dividing wall 21 is the chip package 10 as shown by arrow F in FIG. It acts as a load or stress on the control circuit unit 4 of the second chip 12 in the inside.
  • the reduction of the load on the control circuit unit 4 to the second chip 12 is the first problem.
  • the load is applied not only in the region R0 but mainly in the vicinity of the region where the housing 20 and the chip package 10 contact each other, which affects the second chip 12 and the like. In particular, when the volume and thickness of the second resin located on the outer side are larger than the first resin located on the inner side, the load due to the molding shrinkage force of the second resin is large.
  • the second problem is to ensure the airtightness of the circuit chamber 6 by the adhesion of the resin between the chip package 10 and the dividing wall 21 as described above. It is desirable that the circuit room 6 be isolated from the flow path 5 to maintain high air tightness. Therefore, in the housing 20, it is desirable that the adhesion between the resins be high because of the provision of the dividing wall 21 that shields the flow path 5 side and the circuit chamber 6 side and the performance of the division. In particular, depending on the shape and conditions of integral molding of the first resin and the second resin, the adhesion of the resin may be lowered.
  • Embodiment 1 The structure of a flow rate sensor module which is a sensor device according to the first embodiment of the present invention will be described with reference to FIGS. 1 to 6 and the like.
  • the thick package portion 13 is provided on the chip package 10 as a structure of the chip package 10 and the housing 20 of the flow rate sensor module 100A as a device for the above first and second problems. .
  • FIG. 1 shows an XY plane configuration of the flow rate sensor module 100A of the first embodiment.
  • the plane of FIG. 1 schematically shows the state of the cross section of the housing 20 at a predetermined position in the Z direction so that the chip package 10, the circuit chamber 6 and the like housed inside the housing 20 of the flow sensor module 100A can be seen Show.
  • this corresponds to the state in which the cover 22 (FIG. 4 described later) which is a part of the housing 20 is removed.
  • the laterally long direction in which two semiconductor chips (11, 12) in the chip package 10 are arranged is taken as the X direction.
  • the chip package 10 has a thick portion 13 of the first resin on the surface.
  • the housing 20 made of the second resin is a parting wall 21 formed in contact with a part of the surface of the chip package 10, and a part such as a cover 22 shown in FIG. And.
  • a single chip package 10 of the first resin and a housing 20 of the second resin covering at least a part of the periphery thereof are formed.
  • the case where two semiconductor chips (11, 12) are mounted in one chip package 10 by the first resin is shown.
  • the first chip 11 is a semiconductor chip on which a flow rate detection unit by the diaphragm 3 is mounted.
  • the second chip 12 is a semiconductor chip on which the control circuit unit 4 that controls the flow rate detection unit is mounted.
  • the chip package 10 is manufactured by the process of sealing and molding the first resin.
  • a plate 2 which is a substrate made of glass, for example, is placed on a metal lead frame 7.
  • the first chip 11 and the second chip 12 are mounted on the plate 2 by the adhesive 8.
  • the first chip 11 and the second chip are connected by the wire 9, and the second chip 12 and the lead frame 7 are connected by the wire 9.
  • the chip package 10 is configured by sealing and molding the first resin so as to cover those structures (2, 7, 8, 9, 11, 12).
  • the outer shape of the chip package 10 of the first resin is substantially flat, and the lead frame 7 extends from the end.
  • the opening B1 is formed so that the diaphragm 3 of the first chip 11 is exposed.
  • the chip package 10 includes both the case of referring to the whole including the internal structure and the case of referring to the sealing body by the first resin.
  • the housing 20 which covers the periphery of the chip package 10 is manufactured by the process of integral molding of the second resin with respect to the first resin.
  • the inside of the housing 20 made of the second resin is divided by the dividing wall 21 into the area a1 on the first chip 11 side and the area a2 on the second chip 12 side.
  • a flow path 5 for detecting a flow rate is formed in the area a1, a flow path 5 for detecting a flow rate is formed.
  • the area a2 is formed as a circuit chamber 6 of a sealed closed space including the lead frame 7 and the like.
  • the dividing wall 21 blocks and prevents gas, contaminants, and the like from the flow path 5 of the area a1 from flowing into the circuit chamber 6 of the area a2.
  • the circuit chamber 6 protects the lead frame 7 and the like from corrosion due to its airtightness.
  • the position of the dividing wall 21 in the X direction of the module is generally between the first chip 11 and the second chip 12, and the arrangement region of the dividing wall 21 partially corresponds to the arrangement region A2 of the second chip 12. And Z overlap in plan view.
  • the flow path 5 is formed by the shape of the housing 20 and the like.
  • the flow path 5 is a flow path for detecting the flow rate of gas or the like in the flow rate detection unit by the diaphragm 3.
  • the shape of the flow path 5 is an example, but in the present example, as shown by the arrow, it enters from the opening in the upper side of the drawing, turns around halfway through the diaphragm 3 and exits the lower opening in the drawing.
  • the first chip 11 is a semiconductor chip mounted with a flow rate detection unit by the diaphragm 3 and has a rectangular shape in the XY plane. The first chip 11 detects the flow rate of the gas flowing from the flow path 5 as an electrical signal by the diaphragm 3. The detection signal is sent to the control circuit unit 4 of the second chip 12 through the wiring in the chip package 10.
  • the second chip 12 disposed in A2 is a semiconductor chip on which the control circuit unit 4 is mounted, and has a rectangular shape in the XY plane.
  • the second chip 12 processes the signal detected by the flow rate detection unit of the first chip 11 by the control circuit unit 4 and exchanges signals with the outside through the lead frame 7 or the like.
  • FIG. 2 shows an XY plane configuration in the vicinity of the chip package 10 corresponding to the area a of FIG.
  • the configuration of division of the area a1 on the flow path 5 side and the area a2 on the circuit chamber 6 side by the shapes of the chip package 10 and the dividing wall 21 is shown.
  • A1 indicates an arrangement area of the first chip 11.
  • the first chip 11 has a diaphragm 3 at a position substantially in the center of the rectangular shape or near the left side in the drawing.
  • the chip package 10 is formed such that the diaphragm 3 and a part of the first chip 11 are exposed at the opening (B1 in FIG. 3).
  • A2 is an arrangement area of the second chip 12.
  • the thick portion 13 of the chip package 10 is formed in, for example, a rectangular shape so as to substantially overlap the upper side in the Z direction of the arrangement region A2 of the second chip 12. Since the second chip 12 is sealed in the chip package 10, it can not be seen from the Z direction.
  • the dividing wall 21 is disposed between the first chip 11 and the second chip 12 of the chip package 10 so as to cross in the Y direction.
  • a plurality of lead frames 7 connected from the first chip 11 extend in the X direction, and a connector portion (not shown) 23) connected.
  • FIG. 3 shows an XZ cross-sectional configuration in the vicinity of the chip package 10.
  • FIG. 3 shows a cross section taken along the line AA of FIG. 1 and FIG. As the housing 20, only the dividing wall 21 which is a part of the housing 20 is shown.
  • the chip package 10 is the same as the shape and the cross section of the conventional example (FIG. 20) except for the thick portion 13.
  • the flow sensor module 100A is a module including a flow sensor, which is mainly formed by integral molding of the chip package 10 and a housing 20 covering the periphery thereof.
  • the chip package 10 includes a plate 2 as a substrate, a lead frame 7 connected to the plate 2, a first chip 11 and a second chip 12 mounted on the surface of the plate 2 via an adhesive 8, and a first A wire 9 connecting the right end of the chip 11 to the left end of the second chip 12 and a wire 9 connecting the right end of the second chip 12 to the end of the lead frame 7 and sealing them to form an outer shape And 1 resin.
  • the diaphragm 3 and a part of the first chip 11 are formed in a state of being exposed to the flow path 5.
  • the chip package 10 formed by sealing and molding the first resin is formed to cover the chips (11, 12) and the like on the surface (f1) side with respect to the surface of the plate 2, and also on the back surface (f2) side. It is formed to cover 7 mag.
  • thick portions 13 in a shape inverted in the Z direction by the first resin are provided as a pair on both the front surface (f1) and the back surface (f2) of the chip package 10.
  • the width, thickness, etc. of the two thick portions 13 are the same.
  • the thick portion 13 may not be provided on the back surface (f2) side of the chip package 10, and the chip package 10 may have a flat shape.
  • the thick portion 13 of the chip package 10 corresponds to the entire area in the X direction in which the second chip 12 including the control circuit portion 4 on the main surface of the chip package 10 is disposed, and has a thickness rising as a convex in the Z direction. It is a meat structure. In the first embodiment, it is a condition that the thick portion 13 is provided in the region R3 so as to cover the entire arrangement region of the second chip 12. Then, the second resin is integrally molded so that a part of the right side of the dividing wall 21 is in contact with the part R5 of the left side in the area R3 of the thick portion 13.
  • the rigidity in the vicinity of the second chip 12 is enhanced, and the load on the control circuit unit 4 and the like through the first resin due to the molding shrinkage of the second resin is reduced.
  • the surface (f1) of the chip package 10 has a shape including the thick portion 13, specifically, there is a step, so the surface of the dividing wall 21 of the second resin and the surface of the chip package 10 of the first resin The adhesion of the circuit chamber 6 is improved, and the airtightness of the circuit chamber 6 is improved.
  • the region R5 indicates a region where the arrangement region of the second chip 12 in the X direction and the arrangement region of the dividing wall 21 overlap in a plan view of the Z direction.
  • the dividing wall 21 is relatively divided by the thickness of the thick portion 13 (h in FIG. 5). Is thinner than the prior art. That is, the dividing wall 21 has a thin portion or recess in contact with the thick portion 13 in the region R5, and the second chip 12 is not disposed on the lower side which is the region on the left side of the region R5. It is thinner than the area. Therefore, the load which the second chip 12 receives through the first resin can be reduced by the molding shrinkage of the second resin of the housing 20 including the dividing wall 21.
  • a step is formed in the arrangement region of the dividing wall 21 as shown, and the dividing wall 21 of the second resin and the first resin
  • the contact area of the resin with the surface of the chip package 10 is increased. Therefore, the adhesion between the second resin and the first resin in integrated molding is enhanced. That is, the airtightness of the circuit room 6 is improved.
  • FIG. 4 shows an example of an XZ sectional configuration including an example of the shape of the housing 20 of the flow rate sensor module 100A.
  • the shape of the housing 20 corresponds to the outer shape of the flow rate sensor module 100A.
  • a dividing wall 21 provided corresponding to the upper and lower sides in the Z direction via the chip package 10, and a flat cover 22 connected to the outside of the dividing wall 21; It has the connector part 23 etc. which are connected to the cover 22.
  • the housing 20 is formed to form a predetermined flow path 5 as shown in FIG. 1 in a state where the diaphragm 3 of the first chip 11 is exposed at the opening B1.
  • the cover 22 and the like by the second resin are connected to the outside of the dividing wall 21 in the upper and lower directions in the Z direction. It is covered entirely except a part.
  • FIG. 5 shows an XZ cross section of a model of the thick portion 13 of the chip package 10.
  • the thick portion 13 of the chip package 10 is provided with a thickness h in the Z direction on the main surface (shown here as s3) on the surface (f1) side of the chip package 10.
  • the thick portion 13 is substantially trapezoidal in the XZ cross section.
  • the length Lx1 in the X direction and the area S1 in the bottom surface of the trapezoidal shape of the thick portion 13 and the length Lx2 in the X direction and the area S2 in the upper surface of the trapezoidal shape are used.
  • the length Lx1 of the bottom is larger than the length Lx2 of the upper surface (Lx1> Lx2), and the area S1 of the bottom is larger than the area S2 of the upper surface (S1> S2).
  • the thick portion 13 preferably has a bottom length Lx1 greater than the thickness h (Lx1> h).
  • Lx1> h it is preferable to secure Lx1 and S1 in accordance with the width and the area of the control circuit unit 4 to the second chip 12 in the X direction.
  • the thick portion 13 of the chip package 10 is not limited to a trapezoidal shape having one step in the Z direction, and may have a trapezoidal shape having two or more steps as a modification. That is, the upper surface (s4) of the trapezoid in FIG. 6 may have a second-stage trapezoidal shape with an area smaller than the area S2.
  • FIG. 6 shows an enlarged cross section of each part including the thick part 13 of the chip package 10 of FIG. 3 and explains the relationship of overlapping / arrangement of each part, resin material, load reduction and the like.
  • R2 indicates the width and area in which the second chip 12 is disposed.
  • R3 indicates a width and an area in which the thick portion 13 (particularly, the bottom surface thereof) is disposed, and roughly overlaps the entire area R2.
  • R4 shows the width
  • R5 shows the area
  • the arrow F shows how a molding shrinkage force by the second resin is applied as a load or stress to the second chip 12 through the first resin in the region R5.
  • s1 is the surface of the plate 2
  • s2 is the upper surface of the second chip 12
  • s3 is the main surface of the chip package 10 (corresponding to the above f1)
  • s4 is the upper surface of the thick portion 13.
  • the thick portion 13 is provided in a region R3 corresponding to the entire placement region R2 of the second chip 12 and has a region R5 overlapping with the dividing wall 21 with respect to the arrangement relationship with the housing 20.
  • the housing 20 including the dividing wall 21 are possible.
  • this corresponds to the region R0.
  • a force due to molding shrinkage of the second resin acts on the second chip 12 through the first resin.
  • the control circuit unit 4 may be affected, and characteristics such as a detected flow rate data signal of the flow rate detection unit may fluctuate.
  • the thickness and volume of the housing 20 including the dividing wall 21 which is the second resin are larger than the thickness and volume of the first resin above the upper surface of the second chip 12. In that case, the influence of the load applied to the control circuit unit 4 of the second chip 12 in the Z direction due to the molding shrinkage of the second resin including the dividing wall 21 is large.
  • thick portion 13 is provided in region R3 including region R5.
  • the thickness and the volume of the first resin including the thick portion 13 on the second chip 12 are relative to the thickness and the volume of the second resin including the dividing wall 21 in the region R5, as compared with the conventional example.
  • Grow big That is, the rigidity in the vicinity of the second chip 12 is increased.
  • the strain applied to the control circuit unit 4 and the like in the second chip 12 by the molding shrinkage force of the second resin including the dividing wall 21 is reduced, and the control circuit unit 4 of the second chip 12 in the Z direction. The impact of the load on the head is reduced.
  • the first resin of the chip package 10 is made of a thermosetting resin
  • the second resin of the housing 20 is a thermoplastic resin.
  • Made of resin for example, an epoxy resin or a phenol resin can be used as the thermosetting resin.
  • the thermoplastic resin polycarbonate, polyethylene terephthalate, polybutylene terephthalate (PBT) and the like can be used. Each resin may be mixed with a filler or an additive such as glass or mica.
  • FIG. 7 shows an XZ cross-sectional configuration in the vicinity of the chip package 10 of the flow rate sensor module according to a modification of the first embodiment.
  • the width in the X direction of the region R2 of the second chip 12 on the upper side in the Z direction of the control circuit unit 4 of the second chip 12 in the chip package 10 It has area
  • region R4 on the upper side in the Z direction of the thick portion 13, there is a dividing wall 21 formed in the region R4 covering the entire region R3 of the thick portion 13 in the X direction on the main surface (f1) of the chip package 10.
  • the width of the region R4 of the dividing wall 21 in the X direction is larger than the width of the region R3 of the dividing wall 21 in the X direction.
  • the lower surface of the dividing wall 21 has a thin portion or a recess in contact with the thick portion 13 in the region R3. This thin portion is a region where the second chip 12 is not disposed on the lower side which is the left and right regions of the region R3. Thickness is thinner than.
  • the contact area between the lower surface of the dividing wall 21 and the surface including the thick portion 13 is larger than that described above (FIG. 3). Therefore, the adhesion between the first resin and the second resin is high, and the airtightness of the circuit chamber 6 can be enhanced.
  • the thick portion 13 to be a pair is not provided on the back surface (f 2) side of the chip package 10 and is flat.
  • tip 12, the thick part 13, and the dividing wall 21 are the structures laminated
  • the thickness h of the thick portion 13 may be increased to increase the rigidity in the vicinity of the second chip 12.
  • the width of the dividing wall 21 in the X direction may be narrowed to be equal to the widths of the second chip 12 and the dividing wall 21.
  • the module may be miniaturized by further shortening the arrangement distance between the first chip 11 and the second chip 12.
  • a configuration is also possible in which the thick portion 13 of the chip package 10 is provided only in the region R5 in the X direction.
  • the control circuit unit 4 in the chip package 10 of the first resin due to the molding shrinkage of the second resin in the integrated molding structure of the chip package 10 and the housing 20 is included.
  • the reduction of the load on the second chip 12 can be realized.
  • the adhesion between the first resin of the chip package 10 and the second resin of the housing 20 can be enhanced to ensure or improve the airtightness of the circuit chamber 6.
  • components such as the surface of the chip package 10 and the lead frame 7 of the metal in the circuit chamber 6 can be protected from the influence of corrosion due to gas or contaminants from the flow path 5 side, and the reliability of the flow sensor can be improved. it can. According to the first embodiment, the above two effects can be compatible.
  • the dividing wall 21 is provided in the housing 20 for fixing the chip package 10 and securing the airtightness of the circuit chamber 6 or the like. It is necessary.
  • the flow rate sensor module is configured by two steps of molding of the chip package 10 by the first resin and molding of the housing 20 including the dividing wall 21 by the second resin. Furthermore, in order to miniaturize the module, it is necessary to shorten the length of the chip package 10 in the X direction, and to arrange the chips (11, 12), the dividing wall 21 and the like within the narrow range.
  • the dividing wall 21 of the housing 20 is often provided at symmetrical positions and shapes not only on the front surface (f1) side of the chip package 10 but also on the rear surface (f2) side as shown in FIG.
  • not only the first thick portion 13 is provided on the front side (f1) of the chip package 10 but also the second thick portion corresponding to the back side (f2). 13 is provided. That is, the thick portions 13 of the pair are provided at symmetrical positions and shapes in the Z direction. In this way, the load reduction on the second chip 12 from the dividing wall 21 on the surface (f1) side is also supported from the back surface (f2) side and supported by the thick part 13 to achieve balance, thereby achieving an overall load. Increase the reduction effect.
  • the chip package with respect to the thickness and volume of the second resin of the housing It is conceivable to increase the overall thickness and volume of the first resin. That is, the rigidity is increased by securing the first resin uniformly large while providing the first resin with a flat outer shape without providing the thick portion 13 as in the present embodiment in the first resin, and the load on the control circuit portion is increased. Reduce.
  • an optimal chip package is considered in consideration of the configuration including the position and size of the second chip 12 and the configuration including the position and volume of the dividing wall 21 of the second resin. 10 thick portions 13 are provided.
  • the required amount of resin can be reduced to reduce the cost, and can also contribute to the downsizing of the entire module.
  • the flow sensor module 100B of the second embodiment is the same as the first embodiment in basic configuration and the like, and the main difference is that the thick portion 13 of the chip package 10 is an arrangement region R4 of the dividing wall 21 in the X direction. It is provided corresponding to the whole.
  • FIG. 8 shows an XY plane configuration in the vicinity of the chip package 10 of the flow rate sensor module 100B of the second embodiment.
  • A1 and A2 are arrangement areas of the first chip 11 and the second chip 12 as described above.
  • the thick portion 13 of the chip package 10 is entirely covered with the dividing wall 21 in the X direction, and a part on the right side overlaps the arrangement area A2 of the second chip 12.
  • FIG. 9 shows an XZ sectional configuration in the vicinity of the chip package 10 of the flow rate sensor module 100B of the second embodiment corresponding to FIG.
  • the thick portion 13 provided on the main surface of the chip package 10 is disposed in a region corresponding to the arrangement region R4 of the dividing wall 21 in the X direction, and the entire thick portion 13 is in contact with the dividing wall 21 and covered. ing. Further, the region R5 of a part of the thick portion 13 overlaps the upper part of the left side of the second chip 12 in the Z direction as described above.
  • the thick portion 13 is provided to match the placement region R2 of the second chip 12, but in the second embodiment, the thick portion 13 is matched to the placement region R4 of the dividing wall 21 of the housing 20.
  • the thick portion 13 of the chip package 10 is entirely covered by the dividing wall 21 as a condition and a feature.
  • the surface of the thick portion 13 on the main surface of the chip package 10 is completely covered with the second resin of the dividing wall 21 including the side surface of the trapezoid.
  • the thickness of the dividing wall 21 is relatively reduced by the thickness h of the thick portion 13 in the Z direction. That is, the lower surface of the dividing wall 21 has a thin portion or a recess.
  • the rigidity in the vicinity of the second chip 12 in the chip package 10 can be enhanced, and the load on the control circuit unit 4 through the first resin due to the molding shrinkage of the second resin can be reduced as described above.
  • the contact area of 2nd resin and 1st resin increases rather than a prior art example, the adhesiveness and fixability of 1st resin and 2nd resin become high by the anchor effect by the shape of the said contact surface. That is, the airtightness of the circuit chamber 6 can be improved.
  • effects such as load reduction and airtightness can be obtained.
  • FIG. 21 shows an XZ cross-sectional configuration in the vicinity of the chip package 10 of the flow rate sensor module of the modification of the second embodiment. As shown in this modification, even if the thick portion 13 of the chip package 10 is formed in the entire area including the arrangement area R2 of the second chip 12 in the X direction and the arrangement area R4 of the dividing wall 21 described above. Good.
  • Embodiment 3 Third Embodiment A third embodiment of the present invention will be described with reference to FIGS. 10 and 11.
  • the third embodiment has a configuration in which a groove 31 is further provided in the thick portion 13 of the chip package 10 based on the first and second embodiments.
  • the thick portion 13 of the second embodiment is used as a basis, but the thick portion 13 of the first embodiment can be basically used.
  • FIG. 10 shows an XY plane configuration in the vicinity of the chip package 10 of the flow rate sensor module 100C of the third embodiment.
  • a groove 31 is provided on the rectangular upper surface of the thick portion 13 of the chip package 10.
  • one linear groove 31 with a constant width and depth extending in the Y direction is provided at a position near the middle in the X direction of the thick portion 13.
  • FIG. 11 shows an XZ cross-sectional configuration in the vicinity of the chip package 10 of the flow rate sensor module 100C of the third embodiment corresponding to FIG.
  • a groove 31 is provided at a position indicated by a line a.
  • the depth of the groove 31 is smaller than the thickness h of the thick portion 13, and the width in the X direction of the groove 31 is smaller than the width of the thick portion 13.
  • the dividing wall 21 is formed such that the portion of the second resin corresponding to the position of the groove 31 enters the groove 31 as a protrusion.
  • the contact area between the first resin and the second resin is increased as compared with the second embodiment.
  • the anchor effect due to the second resin entering the groove 31 is increased.
  • the adhesion and fixation of the resin are enhanced, and the airtightness of the circuit chamber 6 can be improved.
  • the position and the shape of the groove 31 in the thick portion 13 of the chip package 10 can be various within the range where the function such as the above-described load reduction by the thick portion 13 can be secured.
  • the groove 31 may be provided at a position away from the second chip 12 on the left side of the line a. Further, the groove 31 may be provided at a position in the region R5 above the second chip 12 on the right side of the line a.
  • a plurality of linear grooves may be provided on the upper surface of the thick portion 13.
  • the shape of the groove 31 in the XZ cross section is not limited to a concave shape or a trapezoidal shape, and a hemispherical shape, a U shape, a triangular wedge shape, and the like are possible.
  • the groove 31 may be changed to a convex portion, that is, a convex portion or a convex portion, instead of a concave portion, that is, a concave portion.
  • the second thick portion may be provided in the Z direction.
  • the concave portion and the convex portion may be mixed.
  • the anchor effect is enhanced and the adhesion is enhanced.
  • the fourth embodiment is different from the above-described embodiment in that the chip package 10 has a configuration in which one semiconductor chip 40 is mounted.
  • FIG. 12 shows an XZ cross-sectional configuration in the vicinity of the chip package 10 of the flow rate sensor module 100D of the fourth embodiment.
  • the chip package 10 according to the fourth embodiment has a configuration in which the two functions of the flow rate detection unit by the diaphragm 3 and the control circuit unit 4 are mounted as one semiconductor chip 40 on the plate 2.
  • One semiconductor chip 40 or the like is mounted on the plate 2 by the adhesive 8, and the chip package 10 is configured by covering them and sealing and molding them with the first resin.
  • the thick portion 13 is provided on the main surface of the chip package 10 in the same manner as described above, corresponding to the region overlapping the upper side in the Z direction of the control circuit portion 4.
  • the width in the X direction of the thick portion 13 is the same as that of the first embodiment and the like.
  • the dividing wall 21 is formed in contact with at least a part of the region R ⁇ b> 5 on the upper side in the Z direction of the thick portion 13.
  • FIG. 13 shows an XZ cross-sectional configuration in the vicinity of the chip package 10 of the flow rate sensor module as a modification of the fourth embodiment.
  • one semiconductor chip 40B of the chip package 10 has a plurality of control circuits 4 (4a, 4b), in particular.
  • a plurality of, in particular, two thick portions 13 (13a, 13b) are provided on the surface of the chip package 10 corresponding to the positions.
  • the first control circuit unit 4a is mounted on the plate 2 near the flow rate detecting unit by the diaphragm 3, and the second control circuit unit 4b is mounted at the same position as described above.
  • thick portions 13a and 13b separated into two are provided corresponding to the regions above the Z direction of the control circuit portions 4a and 4b.
  • Each thick portion 13a, 13b is formed such that a part of the dividing wall 21 is in contact with the part in the upper part in the Z direction.
  • the width in the X direction of thick portion 13 (13a, 13b) of chip package 10 is matched to the width in the X direction of corresponding control circuit portion 4 (4a, 4b). And is shorter than the width of the first embodiment.
  • the present invention is not limited to the configuration with one semiconductor chip 40 described above, and each of the plurality of control circuit units 4 may be divided into a plurality of respective semiconductor chips to correspond to the plurality of respective semiconductor chips.
  • the thick portion 13 may be provided.
  • FIGS. 14A and 14B show an analysis model of a chip package corresponding to the conventional example (FIGS. 19 and 20), which is a model without the thick portion 13.
  • Reference numeral 120 denotes an area of a housing made of a second resin
  • 110 denotes an area of a chip package made of a first resin
  • 112 denotes an area corresponding to the second chip 12
  • 121 denotes an area corresponding to the dividing wall 21.
  • a shows the injection port of resin.
  • the large numbers indicate the respective dimensions [mm].
  • the area 112 of the second chip 12 has dimensions of X, Y, Z of 5 ⁇ 4 ⁇ 2 mm.
  • the chip package area 110 has a thickness in the Z direction of 2 mm.
  • the area 120 of the housing and the area 121 of the dividing wall have a thickness of 4 mm.
  • the width in the X direction is 3 mm in the region corresponding to the overlapping portion of the second chip 12 and the dividing wall 21 in particular.
  • 15 to 17 show an analysis model regarding the vicinity of the thick portion 13 of the chip package 10 in the first to third embodiments in the area b of the broken line in FIG. 14B.
  • FIG. 15 shows an analysis model in the vicinity of the thick portion 13 of the chip package 10 of the first embodiment.
  • An area 113 corresponds to the thick portion 13 and is in contact with the entire area 112 of the second chip 12 and a part of the right side of the area 121 of the dividing wall 21 in the X direction.
  • the dimensions of X and Z are 5 ⁇ 1 mm.
  • FIG. 16 shows an analysis model in the vicinity of the thick portion 13 of the second embodiment.
  • An area 113 corresponds to the thick portion 13 and is in contact with a part of the left side of the area 112 of the second chip 12 in the X direction and in contact with the whole area 121 of the dividing wall 21.
  • the dimensions of X and Z are 3 ⁇ 1 mm.
  • FIG. 17 shows an analysis model in the vicinity of the thick portion 13 of the third embodiment.
  • the region a is enlarged, in the region 113 corresponding to the thick portion 13, the region 131 corresponding to the groove 31 described above is provided on the surface of the dividing wall 21 in contact with the region 121.
  • the width in the X direction of the region 131 corresponding to the groove 31 is 0.6 mm, and the depth is 0.2 mm.
  • the second resin was injected at an injection rate of 4795 mm 3 / s and a resin temperature of 260 ° C. from the inlet of a of FIG. 14 (a).
  • the second resin was cooled to 25 ° C. at a mold temperature of 80 ° C.
  • the equivalent strain due to the load on the second chip 12 caused by the molding shrinkage of the second resin of the housing 20 at that time was calculated and compared in the conventional example and each of the first to third embodiments.
  • An epoxy resin is used as the first resin, and the Young's modulus is 2700 MPa, the Poisson's ratio is 0.3, and the linear expansion coefficient is 8.0 ⁇ 10 -6 .
  • the second resin a fibrous and spherical glass filler using PBT filled 40%, 9500MPa the fiber direction of the Young's modulus, Poisson's ratio 0.38, and the linear expansion coefficient 2.3 ⁇ 10 - 6
  • the Young's modulus in the direction orthogonal to the fibers is 4750 MPa, the Poisson's ratio is 0.38, and the linear expansion coefficient is 6.2 ⁇ 10 ⁇ 6 .
  • FIG. 18 shows the equivalent strain of each of the second chips of the conventional example and the first to third embodiments as a result of the above analysis.
  • the load reduction effect is the most -43%. It got higher. The effect is almost equal to -27% in the second embodiment of (c) and -24% in the third embodiment of (d).
  • the load reduction effect has been confirmed from the conventional example.
  • the load reduction effect relating to the first problem is the highest. Therefore, when priority is given to reducing the load on the second chip 12 to the control circuit unit 4, it is preferable to adopt the first embodiment.
  • priority is given to the effect of ensuring the airtightness of the circuit room 6 relating to the second problem, it is preferable to adopt the second and third embodiments.
  • the present flow rate sensor module can be variously configured as a combination of materials in the first resin constituting the chip package 10 and the second resin constituting the housing 20 as follows.
  • the combination of the first resin and the second resin includes at least one of a thermosetting resin and a thermoplastic resin.
  • Various materials such as the above-mentioned epoxy resin and PBT resin can be used as the thermosetting resin and thermoplastic resin to be the main resin, and in addition to the main resin material, the filler material and the additive material are used You may
  • thermosetting resin is less in thermal deformation than a thermoplastic resin, in other words, it is difficult to form and shrink, has high rigidity, and has a small load on the control circuit portion 4 of the second chip 12 in the chip package 10.
  • the housing 20 can be manufactured by injection molding, and the moldability is good. When priority is given to load reduction performance, this form may be adopted.
  • both the first resin and the second resin are thermoplastic resin:
  • the interface or the contact surface of the first resin of the chip package 10 and the second resin of the housing 20 is joined by melting Cheap.
  • the housing 20 can be manufactured by injection molding, and the moldability is good.
  • the thick portion 13 on the chip package 10 of the first resin the rigidity can be increased and the load on the second chip 12 can be reduced, and the adhesion between the resins can be enhanced.
  • a curable resin but also a thermoplastic resin can be used. In this case, the required rigidity or the like may be secured by, for example, increasing the thickness h or the like of the thick portion 13.
  • Embodiment in which the first resin is a thermoplastic resin and the second resin is a thermosetting resin Similarly, not only a thermoplastic resin but also a thermosetting resin can be adopted as the second resin. In this case, the warpage of the housing 20 can be reduced.
  • the present invention is not limited to the above-mentioned embodiment, and can be variously changed in the range which does not deviate from the gist. Needless to say.
  • the present invention is applicable as a structure of a sensor device to a structure in which a semiconductor chip package mounting a detection unit and a control circuit unit and a housing around the semiconductor chip package are resin-molded.
  • the present invention is applicable not only to flow sensors but also to other types of sensor devices having a similar module structure.
  • a mode in which a part of the plate 2, the adhesive 8, the lead frame 7, the wire 9, etc. in the chip package 10 is eliminated is also possible. Further, in the chip package 10, it is possible to additionally mount components such as a capacitor and a thermistor not shown on the first chip 11 including the flow rate detection unit by the diaphragm 3.
  • the flow sensor module which is the present sensor device, can be configured as follows.
  • This sensor device is a first-stage first resin sealing / molding structure in which the substrate, the semiconductor chip, the wire, and part of the conducting wire are made of the first resin, with the flow rate detection unit exposed.
  • the chip package is configured by being sealed with the stopper.
  • integration of the second resin is performed so as to cover at least a part of the periphery of the first resin sealing body of the chip package and to be in contact on part of the surface.
  • the molding forms a space within the housing and the housing.
  • the first resin on the upper side in the Z direction with reference to the upper surface of the control circuit portion in the sealing body of the first resin or the semiconductor chip including the same is larger than the thickness of the portion of the first resin above the reference plane in the other area in the XY plane, that is, the area where the control circuit portion or the semiconductor chip including the same is not disposed.
  • a dividing wall which is a part of the housing made of the second resin is provided on the upper side in the Z direction so as to contact the surface of the thick portion of the chip package.

Landscapes

  • Physics & Mathematics (AREA)
  • General Physics & Mathematics (AREA)
  • Fluid Mechanics (AREA)
  • Measuring Volume Flow (AREA)
PCT/JP2013/082671 2013-03-04 2013-12-05 センサ装置 Ceased WO2014136336A1 (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2013-042326 2013-03-04
JP2013042326A JP6063777B2 (ja) 2013-03-04 2013-03-04 センサ装置

Publications (1)

Publication Number Publication Date
WO2014136336A1 true WO2014136336A1 (ja) 2014-09-12

Family

ID=51490879

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2013/082671 Ceased WO2014136336A1 (ja) 2013-03-04 2013-12-05 センサ装置

Country Status (2)

Country Link
JP (1) JP6063777B2 (enExample)
WO (1) WO2014136336A1 (enExample)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
FR3030738A1 (fr) * 2014-12-19 2016-06-24 Commissariat Energie Atomique Capteur de pression adapte aux mesures de pression en milieu agressif

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR102264329B1 (ko) * 2018-11-30 2021-06-14 (주)파트론 지문인식 패키지

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH10170380A (ja) * 1996-12-10 1998-06-26 Denso Corp 半導体センサ装置
WO2003036251A1 (en) * 2001-10-18 2003-05-01 Hitachi, Ltd. Sensor
JP2009049298A (ja) * 2007-08-22 2009-03-05 Denso Corp 半導体部品
JP2009052970A (ja) * 2007-08-24 2009-03-12 Denso Corp 圧力センサ

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH10170380A (ja) * 1996-12-10 1998-06-26 Denso Corp 半導体センサ装置
WO2003036251A1 (en) * 2001-10-18 2003-05-01 Hitachi, Ltd. Sensor
JP2009049298A (ja) * 2007-08-22 2009-03-05 Denso Corp 半導体部品
JP2009052970A (ja) * 2007-08-24 2009-03-12 Denso Corp 圧力センサ

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
FR3030738A1 (fr) * 2014-12-19 2016-06-24 Commissariat Energie Atomique Capteur de pression adapte aux mesures de pression en milieu agressif
US10422713B2 (en) 2014-12-19 2019-09-24 Commissariat A L'energie Atomique Et Aux Energies Alternatives Pressure sensor suited to measuring pressure in an aggressive environment

Also Published As

Publication number Publication date
JP2014170858A (ja) 2014-09-18
JP6063777B2 (ja) 2017-01-18

Similar Documents

Publication Publication Date Title
JP6357535B2 (ja) センサおよびその製造方法
JP6032224B2 (ja) 電気コネクタおよびその製造方法
US9580303B2 (en) Flow sensor and method for manufacturing the same
WO2012124437A1 (ja) センサパッケージ
CN105466627B (zh) 用于测量流体压力的传感器模块
JP6435420B2 (ja) 樹脂成形体およびセンサ装置
US7004035B2 (en) Physical value detecting apparatus and housing for physical value detecting means
US10644423B2 (en) Semiconductor module
US9474168B2 (en) Electronic module and method for manufacturing electronic module
JP6063777B2 (ja) センサ装置
CN104600051A (zh) 半导体模块
CN111373226B (zh) 流量计
JP6373104B2 (ja) 半導体圧力センサ及び半導体圧力センサ取付構造体
US11353349B2 (en) Flow-rate sensor
US7768124B2 (en) Semiconductor sensor having a flat mounting plate with banks
JP4717088B2 (ja) 半導体圧力センサ装置の製造方法
JP2021067493A (ja) 温度センサ一体型圧力センサ装置
CN113838839B (zh) 感测组件封装结构及其封装方法
JP5912069B2 (ja) 物理量センサ装置及びその製造方法
CN122699646A (zh) 半导体装置及其制造方法
JP2018025394A (ja) 圧力センサ

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 13877316

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 13877316

Country of ref document: EP

Kind code of ref document: A1