TW241314B - In-situ palladium doping or coating of stainless steel surfaces - Google Patents
In-situ palladium doping or coating of stainless steel surfacesInfo
- Publication number
- TW241314B TW241314B TW083104137A TW83104137A TW241314B TW 241314 B TW241314 B TW 241314B TW 083104137 A TW083104137 A TW 083104137A TW 83104137 A TW83104137 A TW 83104137A TW 241314 B TW241314 B TW 241314B
- Authority
- TW
- Taiwan
- Prior art keywords
- stainless steel
- reactor
- coating
- compound
- steel surfaces
- Prior art date
Links
Classifications
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21C—NUCLEAR REACTORS
- G21C17/00—Monitoring; Testing ; Maintaining
- G21C17/02—Devices or arrangements for monitoring coolant or moderator
- G21C17/022—Devices or arrangements for monitoring coolant or moderator for monitoring liquid coolants or moderators
- G21C17/0225—Chemical surface treatment, e.g. corrosion
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/10—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using organic inhibitors
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B01—PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
- B01J—CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01J37/00—Processes, in general, for preparing catalysts; Processes, in general, for activation of catalysts
- B01J37/02—Impregnation, coating or precipitation
- B01J37/03—Precipitation; Co-precipitation
- B01J37/031—Precipitation
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/18—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using inorganic inhibitors
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N17/00—Investigating resistance of materials to the weather, to corrosion, or to light
- G01N17/02—Electrochemical measuring systems for weathering, corrosion or corrosion-protection measurement
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21C—NUCLEAR REACTORS
- G21C17/00—Monitoring; Testing ; Maintaining
- G21C17/02—Devices or arrangements for monitoring coolant or moderator
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21C—NUCLEAR REACTORS
- G21C19/00—Arrangements for treating, for handling, or for facilitating the handling of, fuel or other materials which are used within the reactor, e.g. within its pressure vessel
- G21C19/28—Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21C—NUCLEAR REACTORS
- G21C19/00—Arrangements for treating, for handling, or for facilitating the handling of, fuel or other materials which are used within the reactor, e.g. within its pressure vessel
- G21C19/28—Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core
- G21C19/30—Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core with continuous purification of circulating fluent material, e.g. by extraction of fission products deterioration or corrosion products, impurities, e.g. by cold traps
- G21C19/307—Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core with continuous purification of circulating fluent material, e.g. by extraction of fission products deterioration or corrosion products, impurities, e.g. by cold traps specially adapted for liquids
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21C—NUCLEAR REACTORS
- G21C17/00—Monitoring; Testing ; Maintaining
- G21C17/02—Devices or arrangements for monitoring coolant or moderator
- G21C17/022—Devices or arrangements for monitoring coolant or moderator for monitoring liquid coolants or moderators
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E30/00—Energy generation of nuclear origin
- Y02E30/30—Nuclear fission reactors
Landscapes
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Chemical & Material Sciences (AREA)
- Plasma & Fusion (AREA)
- General Engineering & Computer Science (AREA)
- High Energy & Nuclear Physics (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Life Sciences & Earth Sciences (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Biodiversity & Conservation Biology (AREA)
- Biochemistry (AREA)
- Ecology (AREA)
- Environmental & Geological Engineering (AREA)
- Environmental Sciences (AREA)
- Health & Medical Sciences (AREA)
- Analytical Chemistry (AREA)
- Inorganic Chemistry (AREA)
- General Health & Medical Sciences (AREA)
- General Physics & Mathematics (AREA)
- Immunology (AREA)
- Pathology (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Catalysts (AREA)
- Chemically Coating (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US14351393A | 1993-10-29 | 1993-10-29 |
Publications (1)
Publication Number | Publication Date |
---|---|
TW241314B true TW241314B (en) | 1995-02-21 |
Family
ID=22504415
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW083104137A TW241314B (en) | 1993-10-29 | 1994-05-06 | In-situ palladium doping or coating of stainless steel surfaces |
Country Status (8)
Country | Link |
---|---|
EP (1) | EP0651397B1 (zh) |
JP (1) | JP3066265B2 (zh) |
KR (1) | KR100264466B1 (zh) |
CA (1) | CA2118062C (zh) |
DE (2) | DE69404112T2 (zh) |
FI (1) | FI103993B (zh) |
IL (1) | IL111203A0 (zh) |
TW (1) | TW241314B (zh) |
Families Citing this family (16)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US5608766A (en) | 1993-10-29 | 1997-03-04 | General Electric Company | Co-deposition of palladium during oxide film growth in high-temperature water to mitigate stress corrosion cracking |
US5818893A (en) * | 1993-10-29 | 1998-10-06 | General Electric Company | In-situ palladium doping or coating of stainless steel surfaces |
US5602888A (en) * | 1993-10-29 | 1997-02-11 | General Electric Company | Radiation-induced palladium doping of metals to protect against stress corrosion cracking |
US5600691A (en) * | 1993-10-29 | 1997-02-04 | General Electric Company | Noble metal doping or coating of crack interior for stress corrosion cracking protection of metals |
US5600692A (en) * | 1993-10-29 | 1997-02-04 | General Electric Company | Method for improving tenacity and loading of palladium on palladium-doped metal surfaces |
TW253058B (en) * | 1994-03-10 | 1995-08-01 | Gen Electric | Method of doping or coating metal surfaces with metallic elements to improve oxide film insulating characteristics |
JP3749731B2 (ja) * | 1994-06-24 | 2006-03-01 | ゼネラル・エレクトリック・カンパニイ | 高温水中で低腐食電位を保つための酸化物皮膜導電率の調整 |
JP3550544B2 (ja) * | 1997-11-28 | 2004-08-04 | ゼネラル・エレクトリック・カンパニイ | 腐食及び応力腐食割れを減少するために金属酸化物表面に加える金属の量を制御する温度に基づく方法 |
US6714618B1 (en) | 1997-11-28 | 2004-03-30 | General Electric Company | Temperature-based method for controlling the amount of metal applied to metal oxide surfaces to reduce corrosion and stress corrosion cracking |
JP2001124891A (ja) | 1999-07-09 | 2001-05-11 | Hitachi Ltd | 原子力プラント構造物の表面処理方法および原子力プラント |
JP3923705B2 (ja) * | 2000-04-24 | 2007-06-06 | 株式会社日立製作所 | 原子力プラントの運転方法および原子力プラント並びに原子力プラントの水質制御方法 |
JP4437256B2 (ja) * | 2004-03-31 | 2010-03-24 | 日立Geニュークリア・エナジー株式会社 | 炭素鋼の腐食減肉防止方法 |
US20100246745A1 (en) * | 2006-12-29 | 2010-09-30 | Samson Hettiarachchi | Methods for operating and methods for reducing post-shutdown radiation levels of nuclear reactors |
KR100968744B1 (ko) | 2007-02-20 | 2010-07-08 | 한국원자력연구원 | 가압경수로용 배관재의 백금분말 담지에 의한 표면처리방법 |
JP5572592B2 (ja) * | 2011-06-16 | 2014-08-13 | 日立Geニュークリア・エナジー株式会社 | ウォータージェットピーニング方法及びその装置 |
CN109524136B (zh) * | 2018-11-22 | 2022-05-20 | 西南石油大学 | 一种高能管断裂甩击行为的试验装置及方法 |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US5130080A (en) * | 1990-04-02 | 1992-07-14 | General Electric Company | Method of providing extended life expectancy for components of boiling water reactors |
US5130081A (en) * | 1990-04-02 | 1992-07-14 | General Electric Company | Operation life of on-life boiling water reactors |
US5135709A (en) * | 1991-05-13 | 1992-08-04 | General Electric Company | Method for reducing corrosion of components exposed to high-temperature water |
-
1994
- 1994-05-06 TW TW083104137A patent/TW241314B/zh not_active IP Right Cessation
- 1994-10-07 IL IL11120394A patent/IL111203A0/xx unknown
- 1994-10-13 CA CA002118062A patent/CA2118062C/en not_active Expired - Fee Related
- 1994-10-27 DE DE69404112T patent/DE69404112T2/de not_active Expired - Fee Related
- 1994-10-27 DE DE0651397T patent/DE651397T1/de active Pending
- 1994-10-27 EP EP94307893A patent/EP0651397B1/en not_active Expired - Lifetime
- 1994-10-28 KR KR1019940027850A patent/KR100264466B1/ko not_active IP Right Cessation
- 1994-10-28 FI FI945083A patent/FI103993B/fi not_active IP Right Cessation
- 1994-10-28 JP JP6264762A patent/JP3066265B2/ja not_active Expired - Fee Related
Also Published As
Publication number | Publication date |
---|---|
KR100264466B1 (ko) | 2000-08-16 |
FI945083A0 (fi) | 1994-10-28 |
CA2118062C (en) | 2000-03-28 |
EP0651397A1 (en) | 1995-05-03 |
FI945083A (fi) | 1995-04-30 |
CA2118062A1 (en) | 1995-04-30 |
FI103993B1 (fi) | 1999-10-29 |
DE651397T1 (de) | 1996-10-10 |
JP3066265B2 (ja) | 2000-07-17 |
KR950011650A (ko) | 1995-05-15 |
DE69404112T2 (de) | 1998-01-15 |
EP0651397B1 (en) | 1997-07-09 |
FI103993B (fi) | 1999-10-29 |
IL111203A0 (en) | 1995-01-24 |
DE69404112D1 (de) | 1997-08-14 |
JPH07198893A (ja) | 1995-08-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
TW241314B (en) | In-situ palladium doping or coating of stainless steel surfaces | |
CA2221002A1 (en) | In situ palladium doping or coating of stainless steel surfaces | |
NO950882L (no) | Fremgangsmåte for å dempe initiering eller forplantning av en sprekk i en overflate til en metallkomponent i en vannkjölt kjernereaktor eller tilknyttet utstyr | |
CA1124008A (en) | Bath for electroless depositing tin on substrates | |
US5608766A (en) | Co-deposition of palladium during oxide film growth in high-temperature water to mitigate stress corrosion cracking | |
SE8006172L (sv) | Passivering av kromfria eller lagkromhaltiga ytor | |
MY151335A (en) | Electroplating solution containing organic acid complexing agent | |
WO1994015001A3 (fr) | Procede de dissolution d'oxydes deposes sur un substrat metallique | |
ES8603589A1 (es) | Procedimiento de tratar substratos a base de hierro para impedir su corrosion superficial | |
ES8206660A1 (es) | Procedimiento para pasivar superficies de hierro y de acero | |
HK1028907A1 (en) | Pretreating agent for metal plating, and method for metal plating using the same. | |
NO984240D0 (no) | Korrosjonsbestandighet av h°ytemperaturlegeringer | |
TW253058B (en) | Method of doping or coating metal surfaces with metallic elements to improve oxide film insulating characteristics | |
MY130189A (en) | Aqueous composition and solution and process for metallic surface-treating an aluminum-containing metal material | |
NZ508503A (en) | Methods of inhibiting corrosion using isomers of chloro- methylbenzotriazole | |
GB2271107A (en) | Method and composition for inhibiting general and pitting corrosion in cooling tower water | |
Hettiarachchi | Palladium acetylacetonate solution | |
US5678232A (en) | Lead decontamination method | |
TW429379B (en) | Application of noble metals to internal surfaces of operating boiling water reactors in the presence of zinc in reactor water | |
CA1182953A (en) | Method and bath for the electroless plating of gold | |
ES8406565A1 (es) | Procedimiento para la proteccion del aluminio, previamente anodizado. | |
JPS57181394A (en) | Preventing method for contamination of steel plate zinc electroplated on one side | |
Brusic | Corrosion Inhibition With Cu-BTA | |
Josso et al. | Hydrazine Bath for Chemical Deposition of Platinum and/or Palladium, and Method of Manufacturing Such a Bath | |
JPS56136966A (en) | Electroless plating method |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |