SE456057B - Elektokemisk cell med gelad anod samt forfarande for framstellning av en sadan cell - Google Patents
Elektokemisk cell med gelad anod samt forfarande for framstellning av en sadan cellInfo
- Publication number
- SE456057B SE456057B SE8008924A SE8008924A SE456057B SE 456057 B SE456057 B SE 456057B SE 8008924 A SE8008924 A SE 8008924A SE 8008924 A SE8008924 A SE 8008924A SE 456057 B SE456057 B SE 456057B
- Authority
- SE
- Sweden
- Prior art keywords
- cell
- anode
- water
- starch
- electrolyte solution
- Prior art date
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M6/00—Primary cells; Manufacture thereof
- H01M6/22—Immobilising of electrolyte
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/06—Electrodes for primary cells
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M4/621—Binders
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
- Primary Cells (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US10699679A | 1979-12-26 | 1979-12-26 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| SE8008924L SE8008924L (sv) | 1981-06-27 |
| SE456057B true SE456057B (sv) | 1988-08-29 |
Family
ID=22314320
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| SE8008924A SE456057B (sv) | 1979-12-26 | 1980-12-18 | Elektokemisk cell med gelad anod samt forfarande for framstellning av en sadan cell |
Country Status (18)
| Country | Link |
|---|---|
| US (1) | US4455358A (instruction) |
| JP (1) | JPS5699975A (instruction) |
| AU (1) | AU539315B2 (instruction) |
| BE (1) | BE886842A (instruction) |
| BR (1) | BR8008481A (instruction) |
| CA (1) | CA1149866A (instruction) |
| CH (1) | CH649174A5 (instruction) |
| DE (1) | DE3048126A1 (instruction) |
| DK (1) | DK160451C (instruction) |
| ES (2) | ES8301065A1 (instruction) |
| FR (1) | FR2472845B1 (instruction) |
| GB (1) | GB2066555B (instruction) |
| GR (1) | GR72307B (instruction) |
| HK (1) | HK71688A (instruction) |
| IL (1) | IL61673A (instruction) |
| IT (1) | IT1142163B (instruction) |
| NL (1) | NL8006858A (instruction) |
| SE (1) | SE456057B (instruction) |
Families Citing this family (32)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4563404A (en) * | 1984-06-18 | 1986-01-07 | Duracell Inc. | Cell gelling agent |
| US4871428A (en) * | 1988-03-24 | 1989-10-03 | C & D Charter Power Systems, Inc. | Method for in situ forming lead-acid batteries having absorbent separators |
| US5401596A (en) * | 1991-10-14 | 1995-03-28 | Stoilov; Georgi T. | Hermetically sealed dry accumulator |
| US5851695A (en) * | 1992-02-10 | 1998-12-22 | C & D Technologies, Inc. | Recombinant lead-acid cell and long life battery |
| US5401590A (en) * | 1992-12-07 | 1995-03-28 | Duracell Inc. | Additives for electrochemical cells having zinc anodes |
| DE4333181C2 (de) * | 1993-04-30 | 1995-09-14 | Siemens Ag | Elektrische Batterie, insbesondere Zink-Brom-Batterie und deren Verwendung als Speisebatterie für ein Elektroauto |
| US6087030A (en) * | 1995-05-05 | 2000-07-11 | Rayovac Corporation | Electrochemical cell anode and high discharge rate electrochemical cell employing same |
| US5837397A (en) * | 1996-11-08 | 1998-11-17 | Gould Electronics Inc. | Laminar (flat or paper-type) lithium-ion battery with slurry anodes and slurry cathodes |
| US5968325A (en) * | 1997-01-07 | 1999-10-19 | A.T.S. Electro-Lube Holdings Ltd. | Auto-electrolytic hydrogen generator |
| US6284410B1 (en) | 1997-08-01 | 2001-09-04 | Duracell Inc. | Zinc electrode particle form |
| US6472103B1 (en) | 1997-08-01 | 2002-10-29 | The Gillette Company | Zinc-based electrode particle form |
| US6521378B2 (en) | 1997-08-01 | 2003-02-18 | Duracell Inc. | Electrode having multi-modal distribution of zinc-based particles |
| US6833217B2 (en) * | 1997-12-31 | 2004-12-21 | Duracell Inc. | Battery cathode |
| CA2243219A1 (en) | 1998-07-14 | 2000-01-14 | A.T.S. Electro-Lube Holdings Ltd. | Electrolytic generation of nitrogen |
| US6379835B1 (en) * | 1999-01-12 | 2002-04-30 | Morgan Adhesives Company | Method of making a thin film battery |
| CA2362754A1 (en) | 1999-02-26 | 2000-08-31 | The Gillette Company | High performance alkaline battery |
| JP4259778B2 (ja) * | 2001-08-02 | 2009-04-30 | パナソニック株式会社 | 非水系二次電池用正極の製造方法 |
| SG104277A1 (en) * | 2001-09-24 | 2004-06-21 | Inst Of Microelectronics | Circuit for measuring changes in capacitor gap using a switched capacitor technique |
| JP2007524190A (ja) * | 2003-06-17 | 2007-08-23 | ザ ジレット カンパニー | 電池用アノード |
| US8722235B2 (en) * | 2004-04-21 | 2014-05-13 | Blue Spark Technologies, Inc. | Thin printable flexible electrochemical cell and method of making the same |
| US8029927B2 (en) | 2005-03-22 | 2011-10-04 | Blue Spark Technologies, Inc. | Thin printable electrochemical cell utilizing a “picture frame” and methods of making the same |
| US8722233B2 (en) | 2005-05-06 | 2014-05-13 | Blue Spark Technologies, Inc. | RFID antenna-battery assembly and the method to make the same |
| WO2008039808A2 (en) | 2006-09-25 | 2008-04-03 | Board Of Regents, The University Of Texas System | Cation-substituted spinel oxide and oxyfluoride cathodes for lithium ion batteries |
| US8441411B2 (en) * | 2007-07-18 | 2013-05-14 | Blue Spark Technologies, Inc. | Integrated electronic device and methods of making the same |
| CN101946347A (zh) * | 2007-12-19 | 2011-01-12 | 蓝色火花科技有限公司 | 高电流薄电化学电池单元及其制造方法 |
| US9027242B2 (en) | 2011-09-22 | 2015-05-12 | Blue Spark Technologies, Inc. | Cell attachment method |
| WO2013177202A1 (en) | 2012-05-21 | 2013-11-28 | Blue Spark Technologies, Inc. | Multi-cell battery |
| JP6316305B2 (ja) | 2012-11-01 | 2018-04-25 | ブルー スパーク テクノロジーズ,インク. | 体温ロギング用パッチ |
| US9444078B2 (en) | 2012-11-27 | 2016-09-13 | Blue Spark Technologies, Inc. | Battery cell construction |
| EP2972001A4 (en) | 2013-03-15 | 2016-11-23 | Warmilu Llc | HEAT PACKAGING WITH PHASE CHANGE |
| US9693689B2 (en) | 2014-12-31 | 2017-07-04 | Blue Spark Technologies, Inc. | Body temperature logging patch |
| US10849501B2 (en) | 2017-08-09 | 2020-12-01 | Blue Spark Technologies, Inc. | Body temperature logging patch |
Family Cites Families (19)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR854064A (fr) * | 1938-12-07 | 1940-04-04 | électrode pour accumulateur et son procédé de fabrication | |
| US2593893A (en) * | 1947-04-14 | 1952-04-22 | Mallory & Co Inc P R | Primary cell |
| BE525034A (instruction) * | 1952-12-13 | |||
| NL113994C (instruction) * | 1957-10-09 | |||
| US3265632A (en) * | 1963-04-09 | 1966-08-09 | Corn Products Co | Aqueous thermally reversible rigid sodium hydroxide gel and process for preparing same |
| ES377820A1 (es) * | 1969-04-22 | 1972-11-01 | Accumulateurs Fixes | Perfeccionamientos en la construccion de baterias. |
| US3918989A (en) * | 1971-01-18 | 1975-11-11 | Gates Rubber Co | Flexible electrode plate |
| FR2143595B1 (instruction) * | 1971-06-30 | 1974-10-31 | Accumulateurs Fixes | |
| BE789556A (fr) * | 1971-10-01 | 1973-03-29 | Union Carbide Corp | Element alcain de pile au zinc |
| FR2186741B1 (instruction) * | 1972-05-30 | 1978-03-03 | Cipel | |
| US3884722A (en) * | 1974-03-18 | 1975-05-20 | Union Carbide Corp | Alkaline galvanic cells |
| JPS50157835A (instruction) * | 1974-06-11 | 1975-12-20 | ||
| US4047289A (en) * | 1974-10-15 | 1977-09-13 | Polaroid Corporation | Method for forming a slurry battery cell |
| JPS53129825A (en) * | 1977-04-19 | 1978-11-13 | Hitachi Maxell | Zinc alkali battery |
| JPS5445746A (en) * | 1977-09-17 | 1979-04-11 | Hitachi Maxell | Alkaline battery |
| JPS5450830A (en) * | 1977-09-29 | 1979-04-21 | Shin Kobe Electric Machinery | Method of producing negative electrode of alkaline battery |
| JPS5468930A (en) * | 1977-11-10 | 1979-06-02 | Hitachi Maxell | Preparation of alkaline battery |
| US4209577A (en) * | 1978-03-31 | 1980-06-24 | Union Carbide Corporation | Alkaline-MnO2 cell having a zinc powder-gel anode containing methyl cellulose |
| US4175052A (en) * | 1978-03-31 | 1979-11-20 | Union Carbide Corporation | Alkaline-MnO2 cell having a zinc powder-gel anode containing P-N-V-P or PMA |
-
1979
- 1979-12-26 US US06/106,996 patent/US4455358A/en not_active Expired - Lifetime
-
1980
- 1980-11-19 GB GB8040413A patent/GB2066555B/en not_active Expired
- 1980-12-09 IL IL61673A patent/IL61673A/xx not_active IP Right Cessation
- 1980-12-10 CA CA000366488A patent/CA1149866A/en not_active Expired
- 1980-12-11 AU AU65286/80A patent/AU539315B2/en not_active Ceased
- 1980-12-17 NL NL8006858A patent/NL8006858A/nl not_active Application Discontinuation
- 1980-12-18 SE SE8008924A patent/SE456057B/sv not_active IP Right Cessation
- 1980-12-19 DE DE19803048126 patent/DE3048126A1/de active Granted
- 1980-12-22 CH CH9456/80A patent/CH649174A5/de unknown
- 1980-12-23 DK DK550180A patent/DK160451C/da not_active IP Right Cessation
- 1980-12-23 ES ES498115A patent/ES8301065A1/es not_active Expired
- 1980-12-23 BR BR8008481A patent/BR8008481A/pt not_active IP Right Cessation
- 1980-12-23 GR GR63753A patent/GR72307B/el unknown
- 1980-12-23 JP JP18271580A patent/JPS5699975A/ja active Granted
- 1980-12-23 IT IT26934/80A patent/IT1142163B/it active
- 1980-12-24 BE BE2/58927A patent/BE886842A/fr not_active IP Right Cessation
- 1980-12-24 FR FR8027555A patent/FR2472845B1/fr not_active Expired
-
1982
- 1982-06-25 ES ES513451A patent/ES8304714A1/es not_active Expired
-
1988
- 1988-09-08 HK HK716/88A patent/HK71688A/xx not_active IP Right Cessation
Also Published As
| Publication number | Publication date |
|---|---|
| IT8026934A0 (it) | 1980-12-23 |
| ES498115A0 (es) | 1982-11-01 |
| AU6528680A (en) | 1981-07-02 |
| BR8008481A (pt) | 1981-07-14 |
| GB2066555A (en) | 1981-07-08 |
| ES8301065A1 (es) | 1982-11-01 |
| DE3048126C2 (instruction) | 1989-01-05 |
| SE8008924L (sv) | 1981-06-27 |
| CA1149866A (en) | 1983-07-12 |
| ES513451A0 (es) | 1983-03-01 |
| DK160451C (da) | 1991-09-16 |
| BE886842A (fr) | 1981-04-16 |
| JPH0348615B2 (instruction) | 1991-07-25 |
| DE3048126A1 (de) | 1981-08-27 |
| ES8304714A1 (es) | 1983-03-01 |
| US4455358A (en) | 1984-06-19 |
| FR2472845B1 (fr) | 1985-06-28 |
| HK71688A (en) | 1988-09-16 |
| NL8006858A (nl) | 1981-07-16 |
| FR2472845A1 (fr) | 1981-07-03 |
| DK550180A (da) | 1981-06-27 |
| GB2066555B (en) | 1983-08-17 |
| IL61673A (en) | 1985-11-29 |
| JPS5699975A (en) | 1981-08-11 |
| AU539315B2 (en) | 1984-09-20 |
| IT1142163B (it) | 1986-10-08 |
| GR72307B (instruction) | 1983-10-19 |
| IL61673A0 (en) | 1981-01-30 |
| DK160451B (da) | 1991-03-11 |
| CH649174A5 (de) | 1985-04-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| SE456057B (sv) | Elektokemisk cell med gelad anod samt forfarande for framstellning av en sadan cell | |
| US4681698A (en) | Electrochemical cells having a gelled anode-electrolyte mixture | |
| US4288913A (en) | Method of forming in situ gelled anode | |
| JPS6113561A (ja) | アルカリ電池の陰極をゲル化する方法及び陰極ブレンド | |
| JPH07114126B2 (ja) | 一次電池の安定化方法 | |
| WO2011007761A1 (ja) | アルカリ電池用電解液のゲル化剤 | |
| US4380578A (en) | Electrochemical cell with gelled anode | |
| US4332870A (en) | Cell having a gelled anode containing a polyhydric alcohol | |
| JPS58166650A (ja) | アルカリ電池アノ−ドのゲル化方法 | |
| JPWO2022034900A5 (instruction) | ||
| JPH02119053A (ja) | アルカリ電池のゲル状陰極用ゲル化剤 | |
| EP3882278A1 (en) | Polymer composition | |
| CN116216711A (zh) | 一种含c=c键有机酸盐改性石墨材料及其制备方法和应用 | |
| CN109817981B (zh) | 一种碱性电池负极合成凝胶剂 | |
| JPH0317181B2 (instruction) | ||
| JPS6113580A (ja) | 空気電池 | |
| JPS61243654A (ja) | アルカリ電池 | |
| JPH09161781A (ja) | アルカリ電池用負極活物質 | |
| JPH0521056A (ja) | 亜鉛アルカリ電池の製造法 | |
| JPS6164072A (ja) | 電池用亜鉛粉 | |
| JPS61198555A (ja) | アルカリ電池 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| NAL | Patent in force |
Ref document number: 8008924-6 Format of ref document f/p: F |
|
| NUG | Patent has lapsed |
Ref document number: 8008924-6 Format of ref document f/p: F |