RU98123003A - Способ получения безводного сульфида натрия - Google Patents

Способ получения безводного сульфида натрия

Info

Publication number
RU98123003A
RU98123003A RU98123003/12A RU98123003A RU98123003A RU 98123003 A RU98123003 A RU 98123003A RU 98123003/12 A RU98123003/12 A RU 98123003/12A RU 98123003 A RU98123003 A RU 98123003A RU 98123003 A RU98123003 A RU 98123003A
Authority
RU
Russia
Prior art keywords
sodium sulfide
dryer
plates
temperature
flakes
Prior art date
Application number
RU98123003/12A
Other languages
English (en)
Other versions
RU2201891C2 (ru
Inventor
Роберт МАГИРА
Ханс Кристиан АЛЬТ
Герхард РАЗИГ
Йерг МЮНЦЕНБЕРГ
Кристоф Батц-Зон
Ральф ГЕДЕККЕ
Ульрих Дешлер
Фолкер КНАПП
Карл-Хайнц РЮТЦЕЛЬ
Original Assignee
Дегусса Акциенгезельшафт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from DE19755760A external-priority patent/DE19755760A1/de
Application filed by Дегусса Акциенгезельшафт filed Critical Дегусса Акциенгезельшафт
Publication of RU98123003A publication Critical patent/RU98123003A/ru
Application granted granted Critical
Publication of RU2201891C2 publication Critical patent/RU2201891C2/ru

Links

Claims (9)

1. Способ получения безводного сульфида натрия путем нагрева водосодержащего сульфида натрия при пониженном давлении, отличающийся тем, что сульфид натрия с содержанием воды 35-45% при перемешивании пропускают через установку, в которой температура высушиваемого материала постоянно возрастает от приблизительно 20°С на входе до ≥180°С на выходе, причем одновременно поддерживают пониженное давление на уровне <20 торр, предпочтительно <11 торр.
2. Способ по п. 1, отличающийся тем, что в качестве сушильной установки применяют контактную сушилку.
3. Способ по пп. 1 и 2, отличающийся тем, что применяют гребковую сушилку.
4. Способ по пп. 1 и 2, отличающийся тем, что в качестве сушильной установки применяют тарельчатую сушилку.
5. Способ по п. 4, отличающийся тем, что тарелки набирают в три или более групп, предназначенные для зон с различным температурным режимом, и при этом в первой группе тарелок (за местом подачи высушиваемого материала) температура продукта составляет 20 - 70°С, а температура продукта перед выходом из сушилки составляет более 180°С.
6. Способ по любому или нескольким пп. 1-5, отличающийся тем. что водосодержащий сульфид натрия применяют в измельченном виде, предпочтительно в форме чешуек, пластинок либо хлопьев с характерной длиной 5 - 8 мм.
7. Способ по любому или нескольким пп. 1-6, отличающийся тем, что получают безводный сульфид натрия с содержанием Nа2S по меньшей мере 98, предпочтительно 99 мас.%.
8. Способ по пп. 1 и 4, отличающийся тем, что способ осуществляют в непрерывном режиме.
9. Способ по пп. 1 и 3, отличающийся тем, что способ осуществляют в периодическом режиме.
RU98123003/12A 1997-12-16 1998-12-16 Способ получения безводного сульфида натрия RU2201891C2 (ru)