KR970704525A - 다중-피복 작용 페인트물을 제조 및 복구시키는 방법(process for producing and repairing multi-coat effect painting) - Google Patents
다중-피복 작용 페인트물을 제조 및 복구시키는 방법(process for producing and repairing multi-coat effect painting) Download PDFInfo
- Publication number
- KR970704525A KR970704525A KR1019970700415A KR19970700415A KR970704525A KR 970704525 A KR970704525 A KR 970704525A KR 1019970700415 A KR1019970700415 A KR 1019970700415A KR 19970700415 A KR19970700415 A KR 19970700415A KR 970704525 A KR970704525 A KR 970704525A
- Authority
- KR
- South Korea
- Prior art keywords
- coating
- shear
- apparent viscosity
- period
- shear rate
- Prior art date
Abstract
본 발명은 베이스코우트의 정전기적 분무에 의해 유일하게 도포되는 다중-피복 작용 페인트물을 제조하고 복구시키는 방법에 관한 것으로서,제공된 유동적 성질을 가지는 페인트물이 베이스코우트로서 사용되고 복구는 분무가 이루어지고 하기를 특징으로 하는 분무 도포 방법을 사용하여 수행된다; 분무의 중앙 및 노즐로부터 300㎜에의 측정 지점을 통과하는 페인트 방울의 40%가 20㎛이하의 직경을 갖고 페인트 방울의 5% 이상은 60㎛이상의 직경을 가지며, 상기 측정 지점을 통과하는 페인트 방울의 20%이상은 6m/s 이하의 속도를 갖고 페인트 방울의 30%는 10m/s 이상의 속도를 가지며, 페인트 방울의 운동량은 4×10-5g㎝s-1이고, 상기 직경 및 속도는 도플러 상 풍력 측정법으로 측정된다.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
Claims (4)
- (1)기판 표면 상에, 베이스코우트를 1가지 이상의 플레이틀릿형 안료를 함유하는 피복 재료를 사용하여 생성시키는 단계, (2)상기 베이스코우트를 1가지 이상의 플레이틀릿형 안료를 함유하는 피복 재료를 분무함으로써 복구시키는 단계, (3) 상기 단계 (1) 또는 (2)에서 생성되는 피복물을 투명한 피복 재료로 피복시키는 단계, (4) 상기 방식으로 생성되는 다중피복 피복물을 베이킹시키는 단계, (5) 베이킹된 다중피복 피복물이 1가지 이상의 플레이틀릿형 안료를 함유하는 피복 재료를 분무함으로써 복구시키는 단계, (6)상기 단계 (5)에서 생성된 피복물을 투명한 피복 재료로 피복시키는 단계, 및 (7) 상기 방식으로 생성된 다중피복 피복물을 베이킹시키는 단계 모두로 이루어지는 방법, 또는 단계 (1), (2), (3)및 (4)로 이루어지는 방법 또는 단계 (1), (3), (4), (5), (6) 및 (7)로 이루어지는 다중피복 특수 작용 피복물을 제조 및 복구시키는 방법으로서, (ⅰ)상기 단계(1)에서 18중량%의 고체 함량 및 23℃의 온도 및 6초의 전단주기 후에 100s-1의 전단 속도에서는 40 내지 200mP s의 겉보기 점도, 300초의 전단기간 후에 1000s-1의 전단 속도에서는 40 내지 200mP s의 겉보기 점도, 10초의 전단기간 후에 5s-1의 전단 속도에서는 100 내지 2000mP s의 겉보기 점도 및 300초의 전단기간 후에 5s-1의 전단 속도에서는 100 내지 2000mP s의 겉보기 점도를 가지는 피복 재료를 사용하고, 1000s-1의 전단 속도에서 300초 동안사전-전단화 직후에 5sec-1의 전단 속도에서 측정 수행되고, 300초의 전단기간 후에 5s-1의 전단 속도에서 측정되는 겉보기 점도는 10초의 전단 기간 후의 5s-1의 전단 속도에서 측정되는 겉보기 점도보다 0 내지 1000mPa s 더 높고 (ⅱ)상기 단계(1)에서 제조된 베이스코우는 유일하게 정전기적 분무에 의해 제조되며,(ⅲ) 상기 단계(2) 및/또는 (5)에서 수행되는 복구는 피복 방울로 구성되고-분무 제트의 중앙에 위치하고 노즐로부터 300mm떨어져 있는 측정 지점을 통과하는 피복방울의 40% 이하가 20㎛미만의 직경을 갖고 상기 측정 지점을 통과하는 피복 방울의 5%이상이 60㎛이상의 직경을 갖고, -분무 제트의 중앙에 위치하고 노즐로부터 300mm떨어져 있는 측정 지점을 통과하는 피복 방울의 20%이상이 6m/s 미만의 속도를 갖고 상기 측정 지점을 통과하는 피복 방울의 30%이하가 10m/s 이상의 속도를 갖고 -분무 제트의 중앙에 위치하고 노즐로부터 300mm 떨어져 있는 측정 지점을 통과하는 피복 방울의 운동량은 4×10-5g ㎝ s-1이상이며, 피복 방울의 직경 및 속도는 도플러 상 풍력 측정법에 의해 측정되는 점에서 구별되는 분무 제트가 제조되는 분무 도포 방법으로 수행되는 것을 특징으로 하는 방법.
- 제1항에 있어서, 상기단계(1)에서 사용되는 피복 재료가 6초의 전단기간 후에 1000s-1의 전단 속도에서는 60 내지 150mPa s의 겉보기 점도, 300초의 전단기간 후에 1000s-1의 전단 속도에서는 60 내지 150mPa s의 겉보기 점도, 10초의 전단기간 후에 5s-1의 전단 속도에서는 200 내지 800mP s의 겉보기 점도, 및 300초의 전단기간 후에 5s-1의 전단 속도에서는 500 내지 1500mPas의 겉보기 점도를 가지고, 300초의 전단기간 후에 5s-1의 전단 속도에서 측정되는 겉보기 점도는 10초 후의 전단기간 후에 5s-1의 전단 속도에서 측정되는 겉보기 점도보다 높은 200내지 600mP as인 것을 특징으로 하는 방법.
- 제1항 또는 제2항에 있어서, 상기 단계(2) 및/또는 단계(5)에서 수행되는 복구가 피복 방울로 구성되고 하기로 구별되는 분무 제트가 제조되며 피목 방울의 직경 및 속도는 도플러 상 풍력 측정법에 따라 측정되는 분무 도포 방법으로 수행되는 것을 특징으로 하는 방법.:-분무 제트의 중앙에 위치하고 노즐로부터 300mm떨어져 있는 측정 지점을 통과하는 피복 방울의 10 내지 30%가 20㎛미만의 직경을 갖고 상기 측정 지점을 통과하는 피복 방울의 10내지 30%이상이 60㎛이상의 직경을 갖고, -분무 중앙에 위치하고 노즐로부터 300mm떨어져 있는 측정 지점을 통과하는 피복 방울의 30 내지 50%가 6m/s 미만의 속도를 갖고 상기 측정 지점을 통과하는 피복 방울의 10 내지 20%가 10m/s 의 속도를 갖고, -분무제트의 중앙에 위치하고 노즐로부터 300mm 떨어져 있는 측정 지점을 통과하는 피복 방울의 운동량은 6×10-5g ㎝ s-1내지 8×10-5g ㎝ s-1과 동등하다.
- 제1항 내지 3항 중 어느 한 항에 따른 방법에 위해 제조될 수 있는 다중 피복 특수 작용 피복물.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.