JPS6410564B2 - - Google Patents
Info
- Publication number
- JPS6410564B2 JPS6410564B2 JP19863284A JP19863284A JPS6410564B2 JP S6410564 B2 JPS6410564 B2 JP S6410564B2 JP 19863284 A JP19863284 A JP 19863284A JP 19863284 A JP19863284 A JP 19863284A JP S6410564 B2 JPS6410564 B2 JP S6410564B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- less
- temperature
- quenching
- hardness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19863284A JPS6176615A (ja) | 1984-09-25 | 1984-09-25 | 耐摩耗鋼の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19863284A JPS6176615A (ja) | 1984-09-25 | 1984-09-25 | 耐摩耗鋼の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6176615A JPS6176615A (ja) | 1986-04-19 |
JPS6410564B2 true JPS6410564B2 (enrdf_load_stackoverflow) | 1989-02-22 |
Family
ID=16394426
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP19863284A Granted JPS6176615A (ja) | 1984-09-25 | 1984-09-25 | 耐摩耗鋼の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6176615A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103233171A (zh) * | 2013-05-10 | 2013-08-07 | 武汉钢铁(集团)公司 | 一种nm400级抗裂纹高强度耐磨钢及生产方法 |
Families Citing this family (12)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6318019A (ja) * | 1986-07-10 | 1988-01-25 | Kobe Steel Ltd | 耐摩耗用鋼板の製造方法 |
JPS6431928A (en) * | 1987-07-27 | 1989-02-02 | Kawasaki Steel Co | Manufacture of wear-resistant steel stock by direct hardening |
JP2578449B2 (ja) * | 1987-12-04 | 1997-02-05 | 川崎製鉄株式会社 | 耐遅れ割れ性の優れた直接焼入れ型高強度鋼の製造方法 |
JPH01172550A (ja) * | 1987-12-25 | 1989-07-07 | Nippon Steel Corp | 耐熱亀裂性に優れた高硬度高靭性耐摩耗鋼 |
JP2867626B2 (ja) * | 1990-06-14 | 1999-03-08 | 株式会社東郷製作所 | 板ばねホースバンドおよびその製造方法 |
JP2924592B2 (ja) * | 1993-09-13 | 1999-07-26 | 日本鋼管株式会社 | 耐磨耗性に優れた鋼管 |
CN1293222C (zh) * | 2003-12-11 | 2007-01-03 | 杨军 | 一种高硬度高韧性易火焰切割的耐磨钢板及其制备方法 |
CN102747282B (zh) * | 2012-07-31 | 2015-04-22 | 宝山钢铁股份有限公司 | 一种高硬度高韧性耐磨钢板及其制造方法 |
PE20241792A1 (es) * | 2017-03-13 | 2024-09-06 | Jfe Steel Corp | Placa de acero resistente a la abrasion y metodo de fabricacion de la misma |
CN107130172B (zh) * | 2017-05-27 | 2019-03-19 | 江阴兴澄特种钢铁有限公司 | 布氏硬度400hbw级整体硬化型高韧性易焊接特厚耐磨钢板及其制造方法 |
CN107881417B (zh) * | 2017-11-29 | 2019-08-27 | 东北大学 | 一种低屈强比马氏体-铁素体-奥氏体复相耐磨钢板及其制造方法 |
CN108707824A (zh) * | 2018-05-25 | 2018-10-26 | 山东钢铁股份有限公司 | 一种抗氢致延迟开裂耐磨钢板及其制备方法 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5789426A (en) * | 1980-11-19 | 1982-06-03 | Nippon Steel Corp | Manufacture of high-hardness and wear resistant steel having excellent weldability |
-
1984
- 1984-09-25 JP JP19863284A patent/JPS6176615A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103233171A (zh) * | 2013-05-10 | 2013-08-07 | 武汉钢铁(集团)公司 | 一种nm400级抗裂纹高强度耐磨钢及生产方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS6176615A (ja) | 1986-04-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP2397570B1 (en) | Steel plate for line pipes with excellent strength and ductility and process for production of same | |
JP7339339B2 (ja) | 冷間加工性及びssc抵抗性に優れた超高強度鋼材及びその製造方法 | |
KR101908818B1 (ko) | 저온에서의 파괴 개시 및 전파 저항성이 우수한 고강도 강재 및 그 제조방법 | |
JP7508469B2 (ja) | せん断加工性に優れた超高強度鋼板及びその製造方法 | |
JP2020510749A (ja) | 低温での破壊開始及び伝播抵抗性に優れた高強度鋼材及びその製造方法 | |
JP3550726B2 (ja) | 低温靱性に優れた高張力鋼の製造方法 | |
JP2017179596A (ja) | 高炭素鋼板およびその製造方法 | |
JPS6410564B2 (enrdf_load_stackoverflow) | ||
JP2005139517A (ja) | 高強度高靭性厚鋼板の製造方法 | |
JP7221476B2 (ja) | 水素誘起割れ抵抗性に優れた鋼材及びその製造方法 | |
JPS63286517A (ja) | 低降状比高張力鋼の製造方法 | |
JP2004027334A (ja) | 高周波焼もどし用鋼およびその製造方法 | |
KR102164110B1 (ko) | 황화물 응력부식 균열 저항성이 우수한 고강도 강재 및 이의 제조방법 | |
JPH0413406B2 (enrdf_load_stackoverflow) | ||
JP7265008B2 (ja) | 水素誘起割れ抵抗性に優れた圧力容器用鋼材及びその製造方法 | |
JP7197699B2 (ja) | 水素誘起割れ抵抗性に優れた圧力容器用鋼材及びその製造方法 | |
JP2004124190A (ja) | ねじり特性に優れる高周波焼もどし鋼 | |
JP3327065B2 (ja) | 脆性亀裂伝播停止特性に優れた調質型高張力鋼板の製造方法 | |
KR20200047081A (ko) | 황화물 응력부식 균열 저항성이 우수한 고강도 강재의 제조방법 | |
JPS6358906B2 (enrdf_load_stackoverflow) | ||
KR102326109B1 (ko) | 황화물 응력부식 균열 저항성이 우수한 강재 및 이의 제조방법 | |
JPH0741865A (ja) | 高炭素鋼板の連続焼鈍による球状化焼鈍方法 | |
JP4803077B2 (ja) | 浸炭焼入用鋼板およびその製造方法 | |
KR100368241B1 (ko) | 플랜지 가공성이 우수한 열연변태유기 소성강 제조방법 | |
JPS6117885B2 (enrdf_load_stackoverflow) |