JPS6333518A - 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 - Google Patents
鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法Info
- Publication number
- JPS6333518A JPS6333518A JP15881987A JP15881987A JPS6333518A JP S6333518 A JPS6333518 A JP S6333518A JP 15881987 A JP15881987 A JP 15881987A JP 15881987 A JP15881987 A JP 15881987A JP S6333518 A JPS6333518 A JP S6333518A
- Authority
- JP
- Japan
- Prior art keywords
- flux density
- magnetic flux
- less
- iron loss
- oriented electrical
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacturing Of Steel Electrode Plates (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15881987A JPS6333518A (ja) | 1987-06-27 | 1987-06-27 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15881987A JPS6333518A (ja) | 1987-06-27 | 1987-06-27 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Related Parent Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58009398A Division JPS59157259A (ja) | 1982-01-27 | 1983-01-25 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6333518A true JPS6333518A (ja) | 1988-02-13 |
| JPH0419297B2 JPH0419297B2 (enrdf_load_stackoverflow) | 1992-03-30 |
Family
ID=15680063
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15881987A Granted JPS6333518A (ja) | 1987-06-27 | 1987-06-27 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6333518A (enrdf_load_stackoverflow) |
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01219126A (ja) * | 1988-02-26 | 1989-09-01 | Nkk Corp | 表面性状の優れた無方向性電磁鋼板の製造方法 |
| JPH01219124A (ja) * | 1988-02-26 | 1989-09-01 | Nkk Corp | 酸洗性に優れた無方向性電磁鋼板の製造方法 |
| JPH03274247A (ja) * | 1990-03-22 | 1991-12-05 | Sumitomo Metal Ind Ltd | 磁気特性に優れた無方向性電磁鋼板 |
| KR100501000B1 (ko) * | 1997-11-25 | 2005-10-12 | 주식회사 포스코 | 응력제거소둔후철손이낮은무방향성전기강판및그제조방법 |
| US7759412B2 (en) | 2006-02-27 | 2010-07-20 | The Yokohama Rubber Co., Ltd. | Tire puncture sealant |
-
1987
- 1987-06-27 JP JP15881987A patent/JPS6333518A/ja active Granted
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01219126A (ja) * | 1988-02-26 | 1989-09-01 | Nkk Corp | 表面性状の優れた無方向性電磁鋼板の製造方法 |
| JPH01219124A (ja) * | 1988-02-26 | 1989-09-01 | Nkk Corp | 酸洗性に優れた無方向性電磁鋼板の製造方法 |
| JPH03274247A (ja) * | 1990-03-22 | 1991-12-05 | Sumitomo Metal Ind Ltd | 磁気特性に優れた無方向性電磁鋼板 |
| KR100501000B1 (ko) * | 1997-11-25 | 2005-10-12 | 주식회사 포스코 | 응력제거소둔후철손이낮은무방향성전기강판및그제조방법 |
| US7759412B2 (en) | 2006-02-27 | 2010-07-20 | The Yokohama Rubber Co., Ltd. | Tire puncture sealant |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0419297B2 (enrdf_load_stackoverflow) | 1992-03-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS6256225B2 (enrdf_load_stackoverflow) | ||
| EP0334224A2 (en) | Ultra-rapid annealing of nonoriented electrical steel | |
| JPS6323262B2 (enrdf_load_stackoverflow) | ||
| JP3855554B2 (ja) | 無方向性電磁鋼板の製造方法 | |
| JPH0713266B2 (ja) | 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法 | |
| JPH0753886B2 (ja) | 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法 | |
| JP3430794B2 (ja) | 磁気特性に優れる無方向性電磁鋼板およびその製造方法 | |
| JP3483265B2 (ja) | 磁束密度が高くかつ鉄損が低い無方向性電磁鋼板の製造方法 | |
| JP3037878B2 (ja) | 歪取焼鈍後鉄損に優れる無方向性電磁鋼板およびその製造方法 | |
| JPS6333518A (ja) | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 | |
| JPH055126A (ja) | 無方向性電磁鋼板の製造方法 | |
| JPS6256922B2 (enrdf_load_stackoverflow) | ||
| JPH04325629A (ja) | 磁気特性の優れた無方向性電磁鋼板の製造方法 | |
| JPH0949023A (ja) | 鉄損が優れた一方向性電磁鋼板の製造方法 | |
| JPH0657332A (ja) | 磁束密度が高くかつ鉄損が低い無方向性電磁鋼板の製造方法 | |
| JP3294367B2 (ja) | 磁束密度が高くかつ鉄損が低い無方向性電磁鋼板およびその製造方法 | |
| JPH0797628A (ja) | 磁束密度が高く、鉄損の低い無方向性電磁鋼板の製造方法 | |
| JPH06256847A (ja) | 磁気特性の優れた一方向性電磁鋼板の製造方法 | |
| JPH0477067B2 (enrdf_load_stackoverflow) | ||
| JP2784661B2 (ja) | 高磁束密度薄手一方向性電磁鋼板の製造方法 | |
| JP3331402B2 (ja) | 全周磁気特性の優れたセミプロセス無方向性電磁鋼板の製造方法 | |
| JPH0261031A (ja) | 磁気特性の優れた無方向性電磁鋼板およびその製造方法 | |
| JPH03294422A (ja) | 磁気特性の優れた無方向性電磁鋼板の製造方法 | |
| JP4320794B2 (ja) | 圧延方向の磁気特性に優れた電磁鋼板の製造方法 | |
| JPH046220A (ja) | 磁束密度が高くかつ鉄損が低い無方向性電磁鋼板の製造方法 |