JPS6316402B2 - - Google Patents
Info
- Publication number
- JPS6316402B2 JPS6316402B2 JP23811084A JP23811084A JPS6316402B2 JP S6316402 B2 JPS6316402 B2 JP S6316402B2 JP 23811084 A JP23811084 A JP 23811084A JP 23811084 A JP23811084 A JP 23811084A JP S6316402 B2 JPS6316402 B2 JP S6316402B2
- Authority
- JP
- Japan
- Prior art keywords
- polymer gel
- acrylamide
- polymer
- fine particles
- active hydrogen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Crushing And Pulverization Processes (AREA)
- Disintegrating Or Milling (AREA)
- Processes Of Treating Macromolecular Substances (AREA)
- Processing And Handling Of Plastics And Other Materials For Molding In General (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23811084A JPS61115909A (ja) | 1984-11-12 | 1984-11-12 | アクリルアミド残量の少ないアクリルアミド系重合体細粒状物の製法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23811084A JPS61115909A (ja) | 1984-11-12 | 1984-11-12 | アクリルアミド残量の少ないアクリルアミド系重合体細粒状物の製法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61115909A JPS61115909A (ja) | 1986-06-03 |
| JPS6316402B2 true JPS6316402B2 (ca) | 1988-04-08 |
Family
ID=17025322
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP23811084A Granted JPS61115909A (ja) | 1984-11-12 | 1984-11-12 | アクリルアミド残量の少ないアクリルアミド系重合体細粒状物の製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61115909A (ca) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6262141B1 (en) | 1999-10-06 | 2001-07-17 | Cytec Technology Corporation | Process for the preparation of polymers having low residual monomer content |
| JP2001121013A (ja) * | 1999-10-26 | 2001-05-08 | Kousha:Kk | 粗リンターの粉砕方法 |
| JP5311360B2 (ja) * | 2000-05-17 | 2013-10-09 | 三菱レイヨン株式会社 | 水溶性重合体の製造方法 |
| JP4495834B2 (ja) * | 2000-06-19 | 2010-07-07 | ダイヤニトリックス株式会社 | アクリルアミド系重合体組成物およびその製造方法 |
| JP5072514B2 (ja) * | 2007-09-26 | 2012-11-14 | ダイヤニトリックス株式会社 | 水溶性重合体の製造方法 |
-
1984
- 1984-11-12 JP JP23811084A patent/JPS61115909A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61115909A (ja) | 1986-06-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4690788A (en) | Process for preparing water-soluble polymer gel particles | |
| DE69813484T9 (de) | Verfahren zur Herstellung eines hydrophiles Harz | |
| CN104822735B (zh) | 聚丙烯酸(盐)系吸水性树脂的制造方法 | |
| CN85104823A (zh) | 水溶性丙烯酸类聚合物的制备方法 | |
| JPH0457682B2 (ca) | ||
| WO1998017453A1 (en) | Method of production of water-absorbing resin | |
| DE102004026787A1 (de) | Verfahren zur Herstellung von wasserabsorbierendem Material | |
| EP2535369A1 (en) | Process for producing water-absorbing resin powder | |
| JPS6316402B2 (ca) | ||
| JP5298288B2 (ja) | 粉末状重合体の製造方法 | |
| JP2023064963A (ja) | 吸水性樹脂の製造方法及び吸水性樹脂 | |
| JPH032042B2 (ca) | ||
| JPH047887B2 (ca) | ||
| JP2000189794A (ja) | 吸水材の製造方法 | |
| CN110713566B (zh) | 细粉再造粒料和高吸水性树脂的制造方法 | |
| JPS6316401B2 (ca) | ||
| JP2847249B2 (ja) | 顆粒状水溶性ポリマーの製造方法 | |
| JP2004330143A (ja) | 水溶性重合体ゲルの細粒化方法 | |
| JP2799889B2 (ja) | 水溶性高分子物質の造粒方法 | |
| JP2003251106A (ja) | 粒状高分子凝集剤の製造法 | |
| JPH02123102A (ja) | 部分加水分解アクリルアミド系ポリマー粉粒体の製造方法 | |
| JPS61155406A (ja) | 高分子量アクリル係重合体の製法 | |
| JPS63273609A (ja) | 高分子量カチオン性アクリル系重合体の製造方法 | |
| JPS63270708A (ja) | カチオン性(メタ)アクリル系水溶性ポリマ−の製法 | |
| JPS61155405A (ja) | アクリル系重合体の製法 |