JPS6240704A - 密着性に優れた超低鉄損一方向性けい素鋼板の製造方法 - Google Patents
密着性に優れた超低鉄損一方向性けい素鋼板の製造方法Info
- Publication number
- JPS6240704A JPS6240704A JP60180164A JP18016485A JPS6240704A JP S6240704 A JPS6240704 A JP S6240704A JP 60180164 A JP60180164 A JP 60180164A JP 18016485 A JP18016485 A JP 18016485A JP S6240704 A JPS6240704 A JP S6240704A
- Authority
- JP
- Japan
- Prior art keywords
- group
- annealing
- steel sheet
- mirror
- silicon steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Soft Magnetic Materials (AREA)
Priority Applications (11)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60180164A JPS6240704A (ja) | 1985-08-16 | 1985-08-16 | 密着性に優れた超低鉄損一方向性けい素鋼板の製造方法 |
| DE8686301071T DE3666229D1 (en) | 1985-02-22 | 1986-02-17 | Extra-low iron loss grain oriented silicon steel sheets |
| EP86301071A EP0193324B1 (en) | 1985-02-22 | 1986-02-17 | Extra-low iron loss grain oriented silicon steel sheets |
| AU53747/86A AU570835B2 (en) | 1985-02-22 | 1986-02-19 | Metal nitride/carbide coated grain oriented silicon steel sheet |
| CA000502337A CA1297070C (en) | 1985-02-22 | 1986-02-20 | Extra-low iron loss grain oriented silicon steel sheets |
| DE8686904726T DE3673290D1 (de) | 1985-02-22 | 1986-02-21 | Herstellungsverfahren fuer unidirektionale siliziumstahlplatte mit aussergewoehnlichem eisenverlust. |
| US06/832,172 US4698272A (en) | 1985-02-22 | 1986-02-21 | Extra-low iron loss grain oriented silicon steel sheets |
| EP86904726A EP0215134B1 (en) | 1985-02-22 | 1986-02-21 | Process for producing unidirectional silicon steel plate with extraordinarily low iron loss |
| US06/907,734 US4713123A (en) | 1985-02-22 | 1986-02-21 | Method of producing extra-low iron loss grain oriented silicon steel sheets |
| PCT/JP1986/000087 WO1986004929A1 (fr) | 1985-02-22 | 1986-02-21 | Procede de production de plaques d'acier au silicium unidirectionnelles avec une perte de fer extremement faible |
| KR1019860001259A KR910006011B1 (ko) | 1985-02-22 | 1986-02-22 | 극저철손 결정 방향성 규소 강판 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60180164A JPS6240704A (ja) | 1985-08-16 | 1985-08-16 | 密着性に優れた超低鉄損一方向性けい素鋼板の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6240704A true JPS6240704A (ja) | 1987-02-21 |
| JPH0374486B2 JPH0374486B2 (enExample) | 1991-11-27 |
Family
ID=16078515
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60180164A Granted JPS6240704A (ja) | 1985-02-22 | 1985-08-16 | 密着性に優れた超低鉄損一方向性けい素鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6240704A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02187771A (ja) * | 1989-01-13 | 1990-07-23 | Minolta Camera Co Ltd | ポリオレフィン系樹脂被覆キャリア |
| WO2018117642A1 (ko) * | 2016-12-22 | 2018-06-28 | 주식회사 포스코 | 방향성 전기강판 및 이의 제조방법 |
-
1985
- 1985-08-16 JP JP60180164A patent/JPS6240704A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02187771A (ja) * | 1989-01-13 | 1990-07-23 | Minolta Camera Co Ltd | ポリオレフィン系樹脂被覆キャリア |
| WO2018117642A1 (ko) * | 2016-12-22 | 2018-06-28 | 주식회사 포스코 | 방향성 전기강판 및 이의 제조방법 |
| US11667984B2 (en) | 2016-12-22 | 2023-06-06 | Posco Co., Ltd | Grain-oriented electrical steel sheet and manufacturing method therefor |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0374486B2 (enExample) | 1991-11-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS63186826A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JP2000063950A (ja) | 磁気特性および被膜特性に優れた方向性電磁鋼板およびその製造方法 | |
| JP2000355717A (ja) | 被膜特性と磁気特性に優れた方向性けい素鋼板およびその製造方法 | |
| JP3268198B2 (ja) | 磁気特性・被膜特性に優れる方向性けい素鋼板の製造方法 | |
| JPS61235514A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6332849B2 (enExample) | ||
| JP3562433B2 (ja) | 磁気特性と被膜特性に優れた方向性けい素鋼板 | |
| JP2724094B2 (ja) | 方向性けい素鋼板の製造方法 | |
| JPH0374486B2 (enExample) | ||
| JPS6240703A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JP2001123229A (ja) | 被膜特性に優れた高磁束密度方向性電磁鋼板の製造方法 | |
| JPH0375354A (ja) | 歪取り焼鈍によって特性の劣化しない超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6269503A (ja) | 超低鉄損方向性けい素鋼板およびその製造方法 | |
| JPH0337846B2 (enExample) | ||
| JPH075973B2 (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPH0222421A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6263407A (ja) | 低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6270520A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6396218A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS621822A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6263408A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6223984A (ja) | 一方向性珪素鋼板の磁歪の圧縮応力特性を改善する極薄張力被膜 | |
| JPS62192581A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6240317A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPS62141706A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 |