JPS62270290A - スリ−ピ−ス缶用アルミニウム合金製缶胴体の製造方法 - Google Patents
スリ−ピ−ス缶用アルミニウム合金製缶胴体の製造方法Info
- Publication number
- JPS62270290A JPS62270290A JP11299286A JP11299286A JPS62270290A JP S62270290 A JPS62270290 A JP S62270290A JP 11299286 A JP11299286 A JP 11299286A JP 11299286 A JP11299286 A JP 11299286A JP S62270290 A JPS62270290 A JP S62270290A
- Authority
- JP
- Japan
- Prior art keywords
- welding
- aluminum alloy
- seam welding
- deformation
- overlapping part
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 229910000838 Al alloy Inorganic materials 0.000 title claims abstract description 37
- 238000004519 manufacturing process Methods 0.000 title claims description 23
- 238000003466 welding Methods 0.000 claims abstract description 89
- 238000005304 joining Methods 0.000 claims description 5
- 230000015572 biosynthetic process Effects 0.000 abstract 2
- 230000002093 peripheral effect Effects 0.000 abstract 1
- 238000000034 method Methods 0.000 description 33
- 229910045601 alloy Inorganic materials 0.000 description 6
- 239000000956 alloy Substances 0.000 description 6
- 238000007796 conventional method Methods 0.000 description 5
- 239000000463 material Substances 0.000 description 5
- XAGFODPZIPBFFR-UHFFFAOYSA-N aluminium Chemical compound [Al] XAGFODPZIPBFFR-UHFFFAOYSA-N 0.000 description 3
- 229910052782 aluminium Inorganic materials 0.000 description 3
- 230000008901 benefit Effects 0.000 description 3
- 238000010586 diagram Methods 0.000 description 3
- 235000008331 Pinus X rigitaeda Nutrition 0.000 description 2
- 235000011613 Pinus brutia Nutrition 0.000 description 2
- 241000018646 Pinus brutia Species 0.000 description 2
- 229910000831 Steel Inorganic materials 0.000 description 2
- 235000014171 carbonated beverage Nutrition 0.000 description 2
- 230000000052 comparative effect Effects 0.000 description 2
- 238000002474 experimental method Methods 0.000 description 2
- 238000010409 ironing Methods 0.000 description 2
- 239000010959 steel Substances 0.000 description 2
- 229910000914 Mn alloy Inorganic materials 0.000 description 1
- 235000013405 beer Nutrition 0.000 description 1
- 238000005452 bending Methods 0.000 description 1
- 235000013353 coffee beverage Nutrition 0.000 description 1
- 238000005336 cracking Methods 0.000 description 1
- 230000000694 effects Effects 0.000 description 1
- 238000005516 engineering process Methods 0.000 description 1
- 238000003384 imaging method Methods 0.000 description 1
- 230000013011 mating Effects 0.000 description 1
- 239000000203 mixture Substances 0.000 description 1
- 238000005096 rolling process Methods 0.000 description 1
- 238000009751 slip forming Methods 0.000 description 1
Landscapes
- Pressure Welding/Diffusion-Bonding (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11299286A JPS62270290A (ja) | 1986-05-17 | 1986-05-17 | スリ−ピ−ス缶用アルミニウム合金製缶胴体の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11299286A JPS62270290A (ja) | 1986-05-17 | 1986-05-17 | スリ−ピ−ス缶用アルミニウム合金製缶胴体の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62270290A true JPS62270290A (ja) | 1987-11-24 |
JPH0354033B2 JPH0354033B2 (enrdf_load_stackoverflow) | 1991-08-16 |
Family
ID=14600711
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11299286A Granted JPS62270290A (ja) | 1986-05-17 | 1986-05-17 | スリ−ピ−ス缶用アルミニウム合金製缶胴体の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62270290A (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH02142686A (ja) * | 1988-11-24 | 1990-05-31 | Daiwa Can Co Ltd | アルミニウム合金製溶接缶胴体の製造方法 |
WO1998026897A1 (en) * | 1996-12-16 | 1998-06-25 | Carnaudmetalbox Plc | Measurement of welds |
-
1986
- 1986-05-17 JP JP11299286A patent/JPS62270290A/ja active Granted
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH02142686A (ja) * | 1988-11-24 | 1990-05-31 | Daiwa Can Co Ltd | アルミニウム合金製溶接缶胴体の製造方法 |
WO1998026897A1 (en) * | 1996-12-16 | 1998-06-25 | Carnaudmetalbox Plc | Measurement of welds |
Also Published As
Publication number | Publication date |
---|---|
JPH0354033B2 (enrdf_load_stackoverflow) | 1991-08-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US6037559A (en) | Process for lap joining two kinds of metallic members having different melting points | |
US5115963A (en) | Superplastic forming of panel structures | |
EP0303837A2 (en) | Container closure with increased strength | |
JPS61206576A (ja) | 金属板等から成る缶胴のラツプ継手の溶接方法 | |
CN113613822B (zh) | 铝材的点焊方法和铝材 | |
JP3767191B2 (ja) | 集合ブランクおよびサイドメンバー | |
JPS62270290A (ja) | スリ−ピ−ス缶用アルミニウム合金製缶胴体の製造方法 | |
JP2002178170A (ja) | 差厚ブランク材及びその製造方法 | |
JP7188121B2 (ja) | 接合装置 | |
JP4415729B2 (ja) | プレス成形方法およびプレス成形装置 | |
JPS606273A (ja) | 連続処理用鋼帯の製造方法 | |
JP2004130315A (ja) | 突合せ溶接継手の疲労強度向上方法 | |
JPS6297785A (ja) | アルミニウム薄板の超音波シ−ム溶接法 | |
JPH079169A (ja) | 金属薄板の溶接方法および装置 | |
JPH0518673B2 (enrdf_load_stackoverflow) | ||
JPH0464797B2 (enrdf_load_stackoverflow) | ||
JPH06170558A (ja) | ティンフリースチール製缶胴の溶接方法 | |
JP3181802B2 (ja) | ピアス加工方法 | |
JP2000167673A (ja) | テーラードブランク材およびその製造方法 | |
JP2020110831A (ja) | フランジ付き板巻きレーザー溶接鋼管及びフランジ付き板巻きレーザー溶接鋼管の製造方法 | |
JPH07232223A (ja) | スポット溶接部のプレス成形方法 | |
JPS62263836A (ja) | アルミニウム合金製接合缶胴体の製造方法 | |
JP2001225114A (ja) | ハイドロフォーム加工方法 | |
SU812475A1 (ru) | Способ холодной сварки металлов внахлестку | |
JP2005305461A (ja) | 疲労強度に優れたレーザ溶接重ね継手の製造方法およびそのレーザ溶接重ね継手 |