JPS6210276B2 - - Google Patents
Info
- Publication number
- JPS6210276B2 JPS6210276B2 JP53073685A JP7368578A JPS6210276B2 JP S6210276 B2 JPS6210276 B2 JP S6210276B2 JP 53073685 A JP53073685 A JP 53073685A JP 7368578 A JP7368578 A JP 7368578A JP S6210276 B2 JPS6210276 B2 JP S6210276B2
- Authority
- JP
- Japan
- Prior art keywords
- less
- particle size
- injection
- cement
- powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Soil Conditioners And Soil-Stabilizing Materials (AREA)
- Consolidation Of Soil By Introduction Of Solidifying Substances Into Soil (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7368578A JPS5523110A (en) | 1978-06-20 | 1978-06-20 | Grout and grouting method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7368578A JPS5523110A (en) | 1978-06-20 | 1978-06-20 | Grout and grouting method |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5523110A JPS5523110A (en) | 1980-02-19 |
JPS6210276B2 true JPS6210276B2 (enrdf_load_stackoverflow) | 1987-03-05 |
Family
ID=13525306
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7368578A Granted JPS5523110A (en) | 1978-06-20 | 1978-06-20 | Grout and grouting method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5523110A (enrdf_load_stackoverflow) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60125288A (ja) * | 1983-12-09 | 1985-07-04 | Yks Co Ltd | 汚水浄化装置 |
FR2598407A1 (fr) * | 1986-05-07 | 1987-11-13 | Lelong Bernard | Procede pour ameliorer la stabilite dimensionnelle de compositions de platre et de ciment en presence d'eau et produits obtenus |
JP2624270B2 (ja) * | 1987-11-18 | 1997-06-25 | 電気化学工業株式会社 | セメントミルク工法用材料 |
JP2525330B2 (ja) * | 1993-06-25 | 1996-08-21 | 強化土エンジニヤリング株式会社 | 地盤注入用薬液 |
JP6578316B2 (ja) * | 2017-04-21 | 2019-09-18 | 花王株式会社 | 地盤の改良工法 |
-
1978
- 1978-06-20 JP JP7368578A patent/JPS5523110A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS5523110A (en) | 1980-02-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPH10504514A (ja) | 改良粉砕助剤組成物およびセメント製品 | |
KR101917513B1 (ko) | 페로니켈 슬래그 분쇄조제, 페로니켈 슬래그를 포함하는 수화열 저감 콘트리트 조성물 및 이의 제조방법 | |
JP4560887B2 (ja) | 製鋼スラグを原料とする水中硬化体 | |
JP5896057B2 (ja) | 人工石材の製造方法 | |
CN106673541A (zh) | 糜棱岩破碎带盾构施工防突涌注浆材料及其制备方法 | |
CN108439907A (zh) | 一种水泥基渣土混凝土的制备工艺 | |
CN109293289B (zh) | 混凝土浮浆回收利用制备同等强度混凝土的方法 | |
JPS6210276B2 (enrdf_load_stackoverflow) | ||
CN103274648A (zh) | 掺花岗岩石粉的高强混凝土管桩及其生产方法 | |
EP2085366A2 (en) | Method for producing hydraulic binding agent in a form of activated fly ash, activated fly ash, hydraulic binding agent, sulfur or cement concrete, mineral-asphalt mixture and application of the activated fly ash | |
JP2007131804A (ja) | 地盤埋戻し材 | |
KR100415641B1 (ko) | 수재슬래그사를이용한성형재료 | |
WO2011136395A1 (ja) | 人工石材の製造方法 | |
CN109020353B (zh) | 混凝土浮浆回收利用制备高于原强度混凝土的方法 | |
CN107512885A (zh) | 一种带有人工砂和细河砂的预拌混凝土及生产方法 | |
KR20100090999A (ko) | 개흙을 이용한 고형물과 그 제조방법 | |
JP3101129B2 (ja) | 重量コンクリートの製造方法 | |
JP2514576B2 (ja) | 炭酸カルシウムを主成分とした岩石粉mpグラウトを用いたエア―モルタルにより目的個所を充填固結する工法 | |
JPS5841751A (ja) | 水硬性混練物の調整法 | |
JPH04219353A (ja) | 注入材 | |
JPS58176155A (ja) | 空洞充填材の調製方法 | |
JPS635243B2 (enrdf_load_stackoverflow) | ||
JP3820301B2 (ja) | 地盤改良工法及びこれに用いられる地盤改良材 | |
JP4150135B2 (ja) | ノロ低減剤及びそれを用いた遠心力成形製品の製造方法 | |
CN109231901A (zh) | 高钛型高炉渣混凝土浮浆回收利用方法 |