JPS61291922A - 連続焼鈍による軟質表面処理原板の製造法 - Google Patents
連続焼鈍による軟質表面処理原板の製造法Info
- Publication number
- JPS61291922A JPS61291922A JP13503585A JP13503585A JPS61291922A JP S61291922 A JPS61291922 A JP S61291922A JP 13503585 A JP13503585 A JP 13503585A JP 13503585 A JP13503585 A JP 13503585A JP S61291922 A JPS61291922 A JP S61291922A
- Authority
- JP
- Japan
- Prior art keywords
- less
- temperature
- rolled
- rolling
- steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13503585A JPS61291922A (ja) | 1985-06-20 | 1985-06-20 | 連続焼鈍による軟質表面処理原板の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13503585A JPS61291922A (ja) | 1985-06-20 | 1985-06-20 | 連続焼鈍による軟質表面処理原板の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61291922A true JPS61291922A (ja) | 1986-12-22 |
| JPH0210854B2 JPH0210854B2 (en:Method) | 1990-03-09 |
Family
ID=15142419
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13503585A Granted JPS61291922A (ja) | 1985-06-20 | 1985-06-20 | 連続焼鈍による軟質表面処理原板の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61291922A (en:Method) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0273916A (ja) * | 1988-09-07 | 1990-03-13 | Nisshin Steel Co Ltd | 極低炭素Tiキルド冷延鋼板のフクレ疵の防止方法 |
| JPH0328324A (ja) * | 1989-06-23 | 1991-02-06 | Nippon Steel Corp | アルミ添加による軟質容器材料用鋼板の製造法 |
Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59173222A (ja) * | 1983-03-24 | 1984-10-01 | Nippon Steel Corp | 軟質表面処理用原板の製造法 |
| JPS6123719A (ja) * | 1984-07-09 | 1986-02-01 | Nippon Steel Corp | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法 |
| JPS6126724A (ja) * | 1984-07-18 | 1986-02-06 | Nippon Steel Corp | 連続焼鈍による極軟質表面処理用原板の製造方法 |
| JPS61207520A (ja) * | 1985-03-13 | 1986-09-13 | Kawasaki Steel Corp | 軟質の非時効性表面処理用鋼板の製造方法 |
-
1985
- 1985-06-20 JP JP13503585A patent/JPS61291922A/ja active Granted
Patent Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59173222A (ja) * | 1983-03-24 | 1984-10-01 | Nippon Steel Corp | 軟質表面処理用原板の製造法 |
| JPS6123719A (ja) * | 1984-07-09 | 1986-02-01 | Nippon Steel Corp | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法 |
| JPS6126724A (ja) * | 1984-07-18 | 1986-02-06 | Nippon Steel Corp | 連続焼鈍による極軟質表面処理用原板の製造方法 |
| JPS61207520A (ja) * | 1985-03-13 | 1986-09-13 | Kawasaki Steel Corp | 軟質の非時効性表面処理用鋼板の製造方法 |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0273916A (ja) * | 1988-09-07 | 1990-03-13 | Nisshin Steel Co Ltd | 極低炭素Tiキルド冷延鋼板のフクレ疵の防止方法 |
| JPH0328324A (ja) * | 1989-06-23 | 1991-02-06 | Nippon Steel Corp | アルミ添加による軟質容器材料用鋼板の製造法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0210854B2 (en:Method) | 1990-03-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| WO2018180404A1 (ja) | 2ピース缶用鋼板及びその製造方法 | |
| US4698102A (en) | Process for producing, by continuous annealing, soft blackplate for surface treatment | |
| JPS5827933A (ja) | 連続焼鈍による耐食性に優れるt−3軟質ぶりき原板の製造方法 | |
| JPH0770650A (ja) | 極めて深絞り性に優れる冷延鋼板の製造方法 | |
| JPS6169928A (ja) | 連続焼鈍によるしごき加工用鋼板の製造方法 | |
| JPS631374B2 (en:Method) | ||
| JPS61291922A (ja) | 連続焼鈍による軟質表面処理原板の製造法 | |
| JPS6234804B2 (en:Method) | ||
| JPH1036917A (ja) | 伸びフランジ性に優れた高強度熱延鋼板の製造方法 | |
| JPH09104919A (ja) | 絞り成形性に優れる缶用鋼板の製造方法 | |
| JPS59173222A (ja) | 軟質表面処理用原板の製造法 | |
| JP2971192B2 (ja) | 深絞り用冷延鋼板の製造方法 | |
| JPH06271943A (ja) | 成形性および耐リジング性に優れ、しかも異方性の小さいフェライト系ステンレス鋼板の製造方法 | |
| RU2815949C1 (ru) | Способ получения горячекатаных листов из низколегированной стали | |
| JPH06306536A (ja) | 耐圧強度とネックドイン性に優れたdi缶用表面処理原板及び製造方法 | |
| JPH0583609B2 (en:Method) | ||
| JPH02129319A (ja) | 表面処理鋼板用原板の製造方法 | |
| JP3028969B2 (ja) | 表面処理鋼板用原板の製造方法 | |
| JP3257390B2 (ja) | 面内異方性の小さい2ピース缶用鋼板の製造方法 | |
| JPH05171351A (ja) | 焼付硬化性に優れた非時効性深絞り用冷延鋼板とその製造方法 | |
| JP2816595B2 (ja) | 連続焼鈍による軟質表面処理用原板の製造方法 | |
| JPH0142329B2 (en:Method) | ||
| JPH04107218A (ja) | 連続焼鈍による耐ストレッチャーストレイン性に優れた軟質ブリキ・tfs原板の製造方法 | |
| JPS61204325A (ja) | 耐リジング性と強度−伸びバランスに優れる加工用アズロ−ルド薄鋼板の製造方法 | |
| JPS6354048B2 (en:Method) |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |