JPS61155406A - 高分子量アクリル係重合体の製法 - Google Patents
高分子量アクリル係重合体の製法Info
- Publication number
- JPS61155406A JPS61155406A JP28171484A JP28171484A JPS61155406A JP S61155406 A JPS61155406 A JP S61155406A JP 28171484 A JP28171484 A JP 28171484A JP 28171484 A JP28171484 A JP 28171484A JP S61155406 A JPS61155406 A JP S61155406A
- Authority
- JP
- Japan
- Prior art keywords
- monomer
- aqueous solution
- polymer
- manufacturing
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Polymerisation Methods In General (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (8)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28171484A JPS61155406A (ja) | 1984-12-27 | 1984-12-27 | 高分子量アクリル係重合体の製法 |
| CA474603A CA1268732C (en) | 1984-12-27 | 1985-02-19 | POLYMERIZATION BY RADIATION AND OBTAINING PARTICLES BY CASTING A LAYER OF WATER-SOLUBLE VINYL MONOMER |
| US06/704,414 US4612336A (en) | 1984-12-27 | 1985-02-22 | Process for preparing water-soluble acrylic polymers by irradiating aqueous monomer solutions containing a surfactant |
| DE3506534A DE3506534C3 (de) | 1984-12-27 | 1985-02-25 | Verfahren zur Herstellung von teilchenförmigen Polymeren mit ausgezeichneter Wasserlöslichkeit und hohem Molekulargewicht |
| FI850794A FI85153C (fi) | 1984-12-27 | 1985-02-27 | Foerfarande foer framstaellning av vattenloesliga akrylpolymerer. |
| FR8502928A FR2575476B1 (fr) | 1984-12-27 | 1985-02-28 | Procede de preparation de polymeres acryliques hydrosolubles |
| CN85104823A CN85104823B (zh) | 1984-12-27 | 1985-06-22 | 水溶性丙烯酸类聚合物的制备方法 |
| GB8530947A GB2170811B (en) | 1984-12-27 | 1985-12-16 | Process for preparing water-soluble acrylic polymers |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28171484A JPS61155406A (ja) | 1984-12-27 | 1984-12-27 | 高分子量アクリル係重合体の製法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61155406A true JPS61155406A (ja) | 1986-07-15 |
| JPH0532410B2 JPH0532410B2 (enExample) | 1993-05-17 |
Family
ID=17642958
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP28171484A Granted JPS61155406A (ja) | 1984-12-27 | 1984-12-27 | 高分子量アクリル係重合体の製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61155406A (enExample) |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2002338630A (ja) * | 2001-05-17 | 2002-11-27 | Mitsubishi Rayon Co Ltd | ノニオン性又はアニオン性の水溶性アクリルアミド系重合体およびその製造方法 |
| US7230061B2 (en) | 2001-12-06 | 2007-06-12 | Nippon Shokubai Co., Ltd. | Process for production of water-soluble (meth)acrylic polymers, water-soluble (meth)acrylic polymers, and use thereof |
| JP2007533808A (ja) * | 2004-04-21 | 2007-11-22 | ストックハウゼン ゲーエムベーハー | 拡散乾燥による吸収性ポリマーの製造方法 |
| JP2009298903A (ja) * | 2008-06-12 | 2009-12-24 | Daiyanitorikkusu Kk | 重合ゲルシートの製造方法及び粉末状重合体の製造方法並びに光重合用反応装置 |
| JP2014173004A (ja) * | 2013-03-08 | 2014-09-22 | Sumitomo Rubber Ind Ltd | 立体形状物の表面改質方法及び注射器用ガスケット |
| JP2015506400A (ja) * | 2012-01-12 | 2015-03-02 | エボニック デグサ ゲーエムベーハーEvonik De | 吸水性ポリマーの連続的な製造方法 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5285283A (en) * | 1976-01-09 | 1977-07-15 | Nitto Chem Ind Co Ltd | Preparation of acrylamide polymers |
| JPS57115409A (en) * | 1980-09-04 | 1982-07-17 | Rhone Poulenc Ind | Manufacture of water-soluble high molecular polymer |
| JPS59133212A (ja) * | 1983-01-21 | 1984-07-31 | Nitto Chem Ind Co Ltd | 残存モノマ−の少ないカチオン性ポリマ−の製造方法 |
-
1984
- 1984-12-27 JP JP28171484A patent/JPS61155406A/ja active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5285283A (en) * | 1976-01-09 | 1977-07-15 | Nitto Chem Ind Co Ltd | Preparation of acrylamide polymers |
| JPS57115409A (en) * | 1980-09-04 | 1982-07-17 | Rhone Poulenc Ind | Manufacture of water-soluble high molecular polymer |
| JPS59133212A (ja) * | 1983-01-21 | 1984-07-31 | Nitto Chem Ind Co Ltd | 残存モノマ−の少ないカチオン性ポリマ−の製造方法 |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2002338630A (ja) * | 2001-05-17 | 2002-11-27 | Mitsubishi Rayon Co Ltd | ノニオン性又はアニオン性の水溶性アクリルアミド系重合体およびその製造方法 |
| US7230061B2 (en) | 2001-12-06 | 2007-06-12 | Nippon Shokubai Co., Ltd. | Process for production of water-soluble (meth)acrylic polymers, water-soluble (meth)acrylic polymers, and use thereof |
| JP2007533808A (ja) * | 2004-04-21 | 2007-11-22 | ストックハウゼン ゲーエムベーハー | 拡散乾燥による吸収性ポリマーの製造方法 |
| JP2009298903A (ja) * | 2008-06-12 | 2009-12-24 | Daiyanitorikkusu Kk | 重合ゲルシートの製造方法及び粉末状重合体の製造方法並びに光重合用反応装置 |
| JP2015506400A (ja) * | 2012-01-12 | 2015-03-02 | エボニック デグサ ゲーエムベーハーEvonik De | 吸水性ポリマーの連続的な製造方法 |
| JP2014173004A (ja) * | 2013-03-08 | 2014-09-22 | Sumitomo Rubber Ind Ltd | 立体形状物の表面改質方法及び注射器用ガスケット |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0532410B2 (enExample) | 1993-05-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS62235305A (ja) | 高分子量アクリル系重合体の製法 | |
| US4612336A (en) | Process for preparing water-soluble acrylic polymers by irradiating aqueous monomer solutions containing a surfactant | |
| US5380808A (en) | Process for producing water-absorbing resins | |
| JP6312680B2 (ja) | 吸水性ポリマー粒子の製造方法 | |
| EP3252097B1 (en) | Superabsorbent polymer and preparation method therefor | |
| JP2005015787A (ja) | 吸水材の製造方法 | |
| US10894867B2 (en) | Manufacturing method of super absorbent polymer | |
| CN106459236A (zh) | 用于制备超吸收性聚合物的方法和由此制备的超吸收性聚合物 | |
| US11680142B2 (en) | Process for producing superabsorbent polymer particles | |
| WO2005007713A1 (en) | Method for production of water-soluble porous polymer and water-soluble porous polymer | |
| JPS61155406A (ja) | 高分子量アクリル係重合体の製法 | |
| JP2023064963A (ja) | 吸水性樹脂の製造方法及び吸水性樹脂 | |
| WO2018174175A1 (ja) | 吸水性樹脂の製造方法 | |
| KR102528637B1 (ko) | 초흡수제의 제조 방법 | |
| JPH0553804B2 (enExample) | ||
| JPS61110510A (ja) | 水溶性重合体ゲルの破砕方法 | |
| JPS61110511A (ja) | 水溶性重合体ゲルの細粒化方法 | |
| JP2003251106A (ja) | 粒状高分子凝集剤の製造法 | |
| JP2003514963A (ja) | 多孔質架橋ポリマー材料の製造方法 | |
| CN103502324A (zh) | 制备吸水聚合物颗粒的方法 | |
| JPH04255701A (ja) | 含水ゲル状重合体の製造方法 | |
| JPS63273609A (ja) | 高分子量カチオン性アクリル系重合体の製造方法 | |
| JPS63270708A (ja) | カチオン性(メタ)アクリル系水溶性ポリマ−の製法 | |
| KR102186939B1 (ko) | 고흡수성 수지의 제조 방법 | |
| JP6934281B2 (ja) | 粉末状水溶性重合体の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |