JPS6017100A - 溶接性の優れた表面処理鋼板の製造方法 - Google Patents

溶接性の優れた表面処理鋼板の製造方法

Info

Publication number
JPS6017100A
JPS6017100A JP12464783A JP12464783A JPS6017100A JP S6017100 A JPS6017100 A JP S6017100A JP 12464783 A JP12464783 A JP 12464783A JP 12464783 A JP12464783 A JP 12464783A JP S6017100 A JPS6017100 A JP S6017100A
Authority
JP
Japan
Prior art keywords
nickel
tin
plating
steel sheet
nickel plating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP12464783A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6342718B2 (enrdf_load_stackoverflow
Inventor
Terunori Fujimoto
輝則 藤本
Yasuhiko Nakagawa
泰彦 中川
Ichiro Onoda
斧田 一郎
Tsuneo Inui
乾 恒夫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toyo Kohan Co Ltd
Original Assignee
Toyo Kohan Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toyo Kohan Co Ltd filed Critical Toyo Kohan Co Ltd
Priority to JP12464783A priority Critical patent/JPS6017100A/ja
Publication of JPS6017100A publication Critical patent/JPS6017100A/ja
Publication of JPS6342718B2 publication Critical patent/JPS6342718B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Electrochemical Coating By Surface Reaction (AREA)
  • Electroplating Methods And Accessories (AREA)
JP12464783A 1983-07-11 1983-07-11 溶接性の優れた表面処理鋼板の製造方法 Granted JPS6017100A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP12464783A JPS6017100A (ja) 1983-07-11 1983-07-11 溶接性の優れた表面処理鋼板の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP12464783A JPS6017100A (ja) 1983-07-11 1983-07-11 溶接性の優れた表面処理鋼板の製造方法

Publications (2)

Publication Number Publication Date
JPS6017100A true JPS6017100A (ja) 1985-01-28
JPS6342718B2 JPS6342718B2 (enrdf_load_stackoverflow) 1988-08-25

Family

ID=14890579

Family Applications (1)

Application Number Title Priority Date Filing Date
JP12464783A Granted JPS6017100A (ja) 1983-07-11 1983-07-11 溶接性の優れた表面処理鋼板の製造方法

Country Status (1)

Country Link
JP (1) JPS6017100A (enrdf_load_stackoverflow)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH01171812U (enrdf_load_stackoverflow) * 1988-05-23 1989-12-05

Also Published As

Publication number Publication date
JPS6342718B2 (enrdf_load_stackoverflow) 1988-08-25

Similar Documents

Publication Publication Date Title
KR101108312B1 (ko) 캔용 도금 강판 및 그 제조 방법
US4601957A (en) Method for producing a thin tin and nickel plated steel sheet for welded can material
JPS6326200B2 (enrdf_load_stackoverflow)
CA1226240A (en) Method of producing tin-free steel sheets having improved resistance to retorting treatment
JPS6046199B2 (ja) 耐錆性の高い溶接缶用表面処理鋼板の製造方法
GB2071699A (en) Production of tin plated steel sheet
JPS6017100A (ja) 溶接性の優れた表面処理鋼板の製造方法
JP2576570B2 (ja) 電解クロメート処理鋼板の前処理方法
JPS6335797A (ja) 溶接性の優れた電解クロメ−ト処理鋼板の製造方法
JPH0214438B2 (enrdf_load_stackoverflow)
JPS58210197A (ja) 耐レトルト処理性にすぐれたテインフリ−鋼の製造方法
JPH0243835B2 (enrdf_load_stackoverflow)
JPH01219195A (ja) 電解クロメート処理鋼板の製造方法
JPS582597B2 (ja) すずめつき鋼板の製造方法
KR960012183B1 (ko) 용접캔용 표면처리강판
JPH11106954A (ja) 溶接性、耐食性、外観に優れた溶接缶用表面処理鋼板
JPS6376897A (ja) 溶接性の優れた電解クロメ−ト処理鋼板およびその製造方法
KR850001134B1 (ko) 용접용 극박(極薄)주석 도금강판의 후처리법
JPH0425350B2 (enrdf_load_stackoverflow)
JPS6366399B2 (enrdf_load_stackoverflow)
JPS6123795A (ja) 塗料2次密着性のすぐれたテインフリ−スチ−ルの製造方法
JPS59205494A (ja) 溶接缶用鋼板の製造法
JPS6318676B2 (enrdf_load_stackoverflow)
JPH0215640B2 (enrdf_load_stackoverflow)
JPS5974296A (ja) 耐レトルト処理性のすぐれたテインフリ−スチ−ルの製造方法