JPS5994699A - 両性重合体よりなる紙力増強剤 - Google Patents
両性重合体よりなる紙力増強剤Info
- Publication number
- JPS5994699A JPS5994699A JP19923982A JP19923982A JPS5994699A JP S5994699 A JPS5994699 A JP S5994699A JP 19923982 A JP19923982 A JP 19923982A JP 19923982 A JP19923982 A JP 19923982A JP S5994699 A JPS5994699 A JP S5994699A
- Authority
- JP
- Japan
- Prior art keywords
- paper strength
- acid
- reaction
- add
- acrylamide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
- Paper (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19923982A JPS5994699A (ja) | 1982-11-12 | 1982-11-12 | 両性重合体よりなる紙力増強剤 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19923982A JPS5994699A (ja) | 1982-11-12 | 1982-11-12 | 両性重合体よりなる紙力増強剤 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5994699A true JPS5994699A (ja) | 1984-05-31 |
| JPH0147598B2 JPH0147598B2 (enrdf_load_stackoverflow) | 1989-10-16 |
Family
ID=16404472
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP19923982A Granted JPS5994699A (ja) | 1982-11-12 | 1982-11-12 | 両性重合体よりなる紙力増強剤 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5994699A (enrdf_load_stackoverflow) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5756646A (en) * | 1995-03-17 | 1998-05-26 | Japan Pmc Corporation | Agent for improving surface quality of paper |
-
1982
- 1982-11-12 JP JP19923982A patent/JPS5994699A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5756646A (en) * | 1995-03-17 | 1998-05-26 | Japan Pmc Corporation | Agent for improving surface quality of paper |
| CN1080792C (zh) * | 1995-03-17 | 2002-03-13 | 日本匹爱姆西株式会社 | 纸表面品质改良剂 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0147598B2 (enrdf_load_stackoverflow) | 1989-10-16 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH08253537A (ja) | 共重合されたビニルアミドモノマーおよびその加水分解生成物を含む水性エマルジョン物質 | |
| CN107849185B (zh) | 水溶性聚合物组合物及其制造方法、以及其利用 | |
| WO2012142425A1 (en) | Process to produce an acylated vinylamine-containing polymer and its application as a papermaking additive | |
| JPH06299494A (ja) | 製紙用サイズ剤組成物およびそれを用いる紙の製造方法 | |
| US4122071A (en) | Water-soluble thermosetting resins and use thereof | |
| JP4370020B2 (ja) | 表面紙質向上剤 | |
| JPS5994699A (ja) | 両性重合体よりなる紙力増強剤 | |
| JPH0149839B2 (enrdf_load_stackoverflow) | ||
| USRE30259E (en) | Water-soluble thermosetting resins and use thereof | |
| EP0282081A1 (en) | Method for increasing paper strength | |
| JP2794414B2 (ja) | カチオン性ポリアクリルアミド並びにz軸紙力及び層間紙力用紙力増強剤及び濾水向上剤 | |
| JP2605330B2 (ja) | 紙力増強方法 | |
| JP2000129590A (ja) | アニオン性アクリルアミド重合体、及びその用途 | |
| JP2979741B2 (ja) | 製紙用添加剤の製造法 | |
| JP2004162201A (ja) | 紙の製造方法 | |
| JPH0860593A (ja) | 紙力増強剤およびその製造方法 | |
| JPH0261493B2 (enrdf_load_stackoverflow) | ||
| JPS6392800A (ja) | 紙力増強剤 | |
| JPH0457991A (ja) | 製紙用添加剤 | |
| JP3173113B2 (ja) | 製紙用添加剤の製造法 | |
| JP2863275B2 (ja) | 製紙用添加剤及び紙の抄造方法 | |
| JPH06192993A (ja) | 製紙用添加剤 | |
| JPS62299599A (ja) | 製紙用添加剤 | |
| JP2665968B2 (ja) | Z軸紙力及び層間紙力用紙力増強剤及び増強方法、濾水向上剤並びに抄紙 | |
| JPH08188982A (ja) | 製紙用添加剤 |