JPS5925808A - アルカリ増粘型ラテツクスの製造方法 - Google Patents
アルカリ増粘型ラテツクスの製造方法Info
- Publication number
- JPS5925808A JPS5925808A JP13471082A JP13471082A JPS5925808A JP S5925808 A JPS5925808 A JP S5925808A JP 13471082 A JP13471082 A JP 13471082A JP 13471082 A JP13471082 A JP 13471082A JP S5925808 A JPS5925808 A JP S5925808A
- Authority
- JP
- Japan
- Prior art keywords
- latex
- parts
- polymerization
- alkali
- species
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Graft Or Block Polymers (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
- Polymerisation Methods In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13471082A JPS5925808A (ja) | 1982-08-03 | 1982-08-03 | アルカリ増粘型ラテツクスの製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13471082A JPS5925808A (ja) | 1982-08-03 | 1982-08-03 | アルカリ増粘型ラテツクスの製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5925808A true JPS5925808A (ja) | 1984-02-09 |
| JPH0149161B2 JPH0149161B2 (enExample) | 1989-10-23 |
Family
ID=15134783
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13471082A Granted JPS5925808A (ja) | 1982-08-03 | 1982-08-03 | アルカリ増粘型ラテツクスの製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5925808A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP2301986A1 (en) | 2009-09-25 | 2011-03-30 | Shin-Etsu Chemical Co., Ltd. | One-terminal reactive organopolysiloxane having a polyalkyleneoxide group at the omega-terminal and a method for the preparation thereof |
-
1982
- 1982-08-03 JP JP13471082A patent/JPS5925808A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP2301986A1 (en) | 2009-09-25 | 2011-03-30 | Shin-Etsu Chemical Co., Ltd. | One-terminal reactive organopolysiloxane having a polyalkyleneoxide group at the omega-terminal and a method for the preparation thereof |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0149161B2 (enExample) | 1989-10-23 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TW523539B (en) | Pressure sensitive adhesives composition | |
| JP2676672B2 (ja) | コアとシェルの間に改善された相結合を有するコア/シェル分散粒子のグラフト共重合体ラテックスの製造方法 | |
| CN101787231A (zh) | 憎水改性缔合型增稠剂及其制备方法 | |
| JPH07216025A (ja) | アルカリ可溶性エマルジョンコポリマーの製造方法 | |
| CN104250334A (zh) | 一种氯乙烯-丙烯酸酯类共聚物及其制备方法 | |
| EP1358217A2 (en) | Highly functional polymer latex | |
| US6852812B2 (en) | Latex having a high solids content and a low viscosity and exhibiting a bimodal distribution | |
| EP1414874B1 (en) | High solids ethylene-vinyl acetate latex | |
| JP3121818B2 (ja) | 水性アクリルポリマー分散液及びその製造方法 | |
| JPH11100404A (ja) | 水性乳化重合のための保護コロイドとしての新規コロイド分散系混合物、それの製造方法及び使用法 | |
| JPS5925808A (ja) | アルカリ増粘型ラテツクスの製造方法 | |
| JP2003514930A (ja) | イオノマー微粒子組成物 | |
| AU753757B2 (en) | New protective colloids in latices with improved film formation at low temperatures | |
| JP2001240633A (ja) | 新規な共重合体 | |
| CN103534277A (zh) | 乙烯基酯/烯属不饱和羧酸酯共聚物的皂化物及其制造方法 | |
| JP4473998B2 (ja) | ビニル系化合物の乳化重合方法 | |
| RU2299892C1 (ru) | Пластизоли на основе стирол-акрилатных латексных сополимеров и способ их получения | |
| JP4051970B2 (ja) | エチレン・ビニルエステル共重合体含有水性エマルジョン | |
| JPH05247408A (ja) | 有機溶媒を含まない水性接着剤溶液 | |
| PT1585774E (pt) | Emulsões aquosas de ésteres de polivinilo contendo hidroxipropilguar | |
| JP4265713B2 (ja) | ビニル系化合物の乳化重合方法 | |
| JP2003514932A (ja) | イオノマー微粒子を製造する方法 | |
| JPH0317870B2 (enExample) | ||
| JPS6270410A (ja) | ポリアクリレ−ト分散系とその製造方法 | |
| JPH11152302A (ja) | カルボキシル基およびカルボキシルアミド基含有ポリマーを基礎とする増粘剤およびその製造方法 |