JPS57207149A - Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance - Google Patents
Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistanceInfo
- Publication number
- JPS57207149A JPS57207149A JP9317281A JP9317281A JPS57207149A JP S57207149 A JPS57207149 A JP S57207149A JP 9317281 A JP9317281 A JP 9317281A JP 9317281 A JP9317281 A JP 9317281A JP S57207149 A JPS57207149 A JP S57207149A
- Authority
- JP
- Japan
- Prior art keywords
- cracking resistance
- stress corrosion
- corrosion cracking
- precipitation hardening
- hardening type
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Nonferrous Metals Or Alloys (AREA)
- Rigid Pipes And Flexible Pipes (AREA)
Priority Applications (6)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9317281A JPS57207149A (en) | 1981-06-17 | 1981-06-17 | Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance |
US06/383,803 US4400209A (en) | 1981-06-10 | 1982-06-01 | Alloy for making high strength deep well casing and tubing having improved resistance to stress-corrosion cracking |
GB08216703A GB2103655B (en) | 1981-06-10 | 1982-06-09 | Alloy for making high strength deep well casing and tubing having improved resistance to stress-corrosion cracking |
DE3221878A DE3221878A1 (de) | 1981-06-10 | 1982-06-09 | Legierung, insbesondere zur herstellung von hochbelastbaren verrohrungen von tiefbohrungen oder dergleichen |
FR8210116A FR2507628A1 (fr) | 1981-06-10 | 1982-06-10 | Alliage pour la realisation de chemisages et de tubes pour puits profonds |
SE8203627A SE452477B (sv) | 1981-06-10 | 1982-06-10 | Legering for framstellning av hoghallfasta foder och ror for djupborrstal, anvendning av legeringen och hoghallfast ror framstellt av denna legering |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9317281A JPS57207149A (en) | 1981-06-17 | 1981-06-17 | Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57207149A true JPS57207149A (en) | 1982-12-18 |
JPS6144133B2 JPS6144133B2 (zh) | 1986-10-01 |
Family
ID=14075146
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9317281A Granted JPS57207149A (en) | 1981-06-10 | 1981-06-17 | Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57207149A (zh) |
Cited By (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60224764A (ja) * | 1984-04-24 | 1985-11-09 | Sumitomo Metal Ind Ltd | 高温用n含有オ−ステナイトステンレス鋼 |
JPS63100152A (ja) * | 1986-10-15 | 1988-05-02 | Kubota Ltd | 高耐食性鋳造合金 |
US4911886A (en) * | 1988-03-17 | 1990-03-27 | Allegheny Ludlum Corporation | Austentitic stainless steel |
JP2008528806A (ja) * | 2005-01-25 | 2008-07-31 | ハンチントン、アロイス、コーポレーション | 延性低下割れ耐性を有する被覆された溶接電極、およびそれから製造された溶着物 |
WO2009044758A1 (ja) | 2007-10-03 | 2009-04-09 | Sumitomo Metal Industries, Ltd. | 高強度Cr-Ni合金材およびそれを用いた油井用継目無管 |
WO2010113843A1 (ja) | 2009-04-01 | 2010-10-07 | 住友金属工業株式会社 | 高強度Cr-Ni合金継目無管の製造方法 |
WO2015072458A1 (ja) | 2013-11-12 | 2015-05-21 | 新日鐵住金株式会社 | Ni-Cr合金材およびそれを用いた油井用継目無管 |
WO2017037851A1 (ja) * | 2015-08-31 | 2017-03-09 | 株式会社日立製作所 | Cr基二相合金および該二相合金を用いた製造物 |
EP3441492A4 (en) * | 2016-03-30 | 2019-09-25 | Hitachi, Ltd. | TWO-PHASE CHROMIUM-BASED ALLOY AND PRODUCT USING SAID TWO PHASE ALLOY |
WO2021070735A1 (ja) | 2019-10-10 | 2021-04-15 | 日本製鉄株式会社 | 合金材および油井用継目無管 |
-
1981
- 1981-06-17 JP JP9317281A patent/JPS57207149A/ja active Granted
Non-Patent Citations (4)
Title |
---|
ALLOYS FOR EIGHTIES=1980 * |
JOURNAL OF METALS=1951 * |
JOURNAL OF METALS=1969 * |
PROCEEDINGS OF MATERIALS AND CORROSION PROBLEMS IN ENERGY SYSTEMS=1980 * |
Cited By (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60224764A (ja) * | 1984-04-24 | 1985-11-09 | Sumitomo Metal Ind Ltd | 高温用n含有オ−ステナイトステンレス鋼 |
JPS63100152A (ja) * | 1986-10-15 | 1988-05-02 | Kubota Ltd | 高耐食性鋳造合金 |
US4911886A (en) * | 1988-03-17 | 1990-03-27 | Allegheny Ludlum Corporation | Austentitic stainless steel |
JP2008528806A (ja) * | 2005-01-25 | 2008-07-31 | ハンチントン、アロイス、コーポレーション | 延性低下割れ耐性を有する被覆された溶接電極、およびそれから製造された溶着物 |
US8071020B2 (en) | 2007-10-03 | 2011-12-06 | Sumitomo Metal Industries, Ltd. | High strength Cr-Ni alloy material and seamless pipe for oil well |
WO2009044758A1 (ja) | 2007-10-03 | 2009-04-09 | Sumitomo Metal Industries, Ltd. | 高強度Cr-Ni合金材およびそれを用いた油井用継目無管 |
WO2010113843A1 (ja) | 2009-04-01 | 2010-10-07 | 住友金属工業株式会社 | 高強度Cr-Ni合金継目無管の製造方法 |
WO2015072458A1 (ja) | 2013-11-12 | 2015-05-21 | 新日鐵住金株式会社 | Ni-Cr合金材およびそれを用いた油井用継目無管 |
KR20160082534A (ko) | 2013-11-12 | 2016-07-08 | 신닛테츠스미킨 카부시키카이샤 | Ni-Cr 합금재 및 그것을 이용한 유정용 이음매 없는 관 |
US10557574B2 (en) | 2013-11-12 | 2020-02-11 | Nippon Steel Corporation | Ni—Cr alloy material and seamless oil country tubular goods using the same |
WO2017037851A1 (ja) * | 2015-08-31 | 2017-03-09 | 株式会社日立製作所 | Cr基二相合金および該二相合金を用いた製造物 |
EP3441492A4 (en) * | 2016-03-30 | 2019-09-25 | Hitachi, Ltd. | TWO-PHASE CHROMIUM-BASED ALLOY AND PRODUCT USING SAID TWO PHASE ALLOY |
WO2021070735A1 (ja) | 2019-10-10 | 2021-04-15 | 日本製鉄株式会社 | 合金材および油井用継目無管 |
Also Published As
Publication number | Publication date |
---|---|
JPS6144133B2 (zh) | 1986-10-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS57203740A (en) | Precipitation hardening alloy of high stress corrosion cracking resistance for high strength oil well pipe | |
JPS57207149A (en) | Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance | |
JPS5521547A (en) | Austenite stainless steel having high strength and pitting corrosion resistance | |
JPS57134542A (en) | Ferrite stainless steel with superior corrosion resistance | |
JPS57210938A (en) | Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance | |
JPS57203738A (en) | Precipitation hardening alloy of high stress corrosion cracking resistance for high-strength oil well pipe | |
JPS57207150A (en) | Precipitation hardening type alloy for high strength oil well pipe with superior stress corrosion cracking resistance | |
JPS5616653A (en) | Soft magnetic material having superior workability and machinability | |
JPS57207148A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance and hydrogen cracking resistance | |
JPS572865A (en) | P-containing corrosion resistant steel with high weldability | |
JPS57210939A (en) | Alloy for high strength oil well pipe with superior stress corrosion cracking resistance | |
JPS57210941A (en) | Alloy for high-strength oil well pipe with superior stress corrosion cracking resistance | |
JPS57210940A (en) | Alloy for high-strength oil well pipe with superior stress corrosion cracking resistance | |
JPS57207147A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance and hydrogen cracking resistance | |
JPS57203736A (en) | Alloy of high stress corrosion cracking resistance for high-strength oil well pipe | |
JPS57203739A (en) | Precipitation hardening alloy of high stress corrosion cracking resistance for high strength oil well pipe | |
JPS57207160A (en) | Low thermal expansion invar type fe-ni alloy with superior rust resistance | |
JPS57207146A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance and hydrogen cracking resistance | |
JPS5747852A (en) | High-cr low-ni two-phase stainless steel | |
JPS57203735A (en) | Alloy of high stress corrosion cracking resistance for high-strength oil well pipe | |
JPS57131340A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance | |
JPS57134544A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance | |
JPS5726146A (en) | Nonmagnetic mn-ni steel with superior stress corrosion cracking resistance | |
JPS57207143A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance and hot workability | |
JPS57207144A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance and hot workability |