JPH1067805A5 - - Google Patents
Info
- Publication number
- JPH1067805A5 JPH1067805A5 JP1997145216A JP14521697A JPH1067805A5 JP H1067805 A5 JPH1067805 A5 JP H1067805A5 JP 1997145216 A JP1997145216 A JP 1997145216A JP 14521697 A JP14521697 A JP 14521697A JP H1067805 A5 JPH1067805 A5 JP H1067805A5
- Authority
- JP
- Japan
- Prior art keywords
- polymerization
- crosslinked polymer
- water
- producing
- polymerization system
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14521697A JP3845177B2 (ja) | 1996-06-05 | 1997-06-03 | 吸水性樹脂 |
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14270896 | 1996-06-05 | ||
| JP8-142708 | 1996-06-05 | ||
| JP14521697A JP3845177B2 (ja) | 1996-06-05 | 1997-06-03 | 吸水性樹脂 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH1067805A JPH1067805A (ja) | 1998-03-10 |
| JPH1067805A5 true JPH1067805A5 (enExample) | 2004-12-09 |
| JP3845177B2 JP3845177B2 (ja) | 2006-11-15 |
Family
ID=26474624
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14521697A Expired - Lifetime JP3845177B2 (ja) | 1996-06-05 | 1997-06-03 | 吸水性樹脂 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3845177B2 (enExample) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6599989B2 (en) | 1998-03-03 | 2003-07-29 | Nippon Skokubai Co., Ltd. | Water-absorbent agents containing polycarboxylic amine chelating agents |
| DE10331456A1 (de) * | 2003-07-10 | 2005-02-24 | Basf Ag | (Meth)acrylsäureester alkoxilierter ungesättigter Polyolether und deren Herstellung |
| JP4743205B2 (ja) * | 2005-05-26 | 2011-08-10 | 東亞合成株式会社 | 水溶性重合体の製造方法及びその用途 |
| JP5599513B2 (ja) * | 2011-06-29 | 2014-10-01 | 株式会社日本触媒 | ポリアクリル酸(塩)系吸水性樹脂粉末及びその製造方法 |
| JP6441211B2 (ja) | 2013-03-11 | 2018-12-19 | 住友精化株式会社 | 吸水性樹脂の製造装置 |
| JP6513442B2 (ja) * | 2015-03-20 | 2019-05-15 | 株式会社日本触媒 | 酸基含有重合体、及び、酸基含有重合体の保存方法 |
| JPWO2021049467A1 (enExample) * | 2019-09-09 | 2021-03-18 |
-
1997
- 1997-06-03 JP JP14521697A patent/JP3845177B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN102911381B (zh) | 一种化学/离子/物理复配交联水凝胶及其制备方法 | |
| US4587284A (en) | Absorbent polymer material and its preparation | |
| JP2000504751A (ja) | アミノ基を含むバイオポリマーの架橋生成物 | |
| RU2005138297A (ru) | Водопоглощающая смола, способ ее получения и поглощающее изделие | |
| JP3177859B2 (ja) | 吸水性ポリマーを基礎とする水性液用の粉末状吸収剤 | |
| JP3907625B2 (ja) | 高分子ハイドロゲル | |
| JPH1067805A5 (enExample) | ||
| JP2003261601A (ja) | 吸水性樹脂およびその製造方法 | |
| JPS60135432A (ja) | 改質吸水性樹脂 | |
| JP2555159B2 (ja) | 吸水性樹脂の製造方法 | |
| JPS6360044B2 (enExample) | ||
| CN114736394A (zh) | 一种动态键自愈合功能的水凝胶组合物及其制备方法与应用 | |
| JP2001089527A5 (enExample) | ||
| JPH01292003A (ja) | 吸水性樹脂の精製方法 | |
| EP0165074B1 (en) | Absorbent polymer material and its preparation | |
| JPS58154708A (ja) | 高吸水性樹脂の製造方法 | |
| JPS6342641B2 (enExample) | ||
| CN110551298B (zh) | 一种高形状回复率水凝胶及其制备方法 | |
| JP2790322B2 (ja) | キトサン含有粒状体およびその製造方法 | |
| JP2745703B2 (ja) | 吸水性ポリマーの製造方法 | |
| JPH1135691A5 (enExample) | ||
| JPS5938242B2 (ja) | アクリルアミド系重合体の製造法 | |
| JPH0841103A (ja) | 吸水性セルロース材料の製造方法 | |
| JP3462016B2 (ja) | キチン成形体の製造方法 | |
| JPH06345980A (ja) | 耐塩性吸収剤組成物 |