JPH0762434A - 方向性電磁鋼板の一次再結晶粒径制御方法 - Google Patents
方向性電磁鋼板の一次再結晶粒径制御方法Info
- Publication number
- JPH0762434A JPH0762434A JP21159893A JP21159893A JPH0762434A JP H0762434 A JPH0762434 A JP H0762434A JP 21159893 A JP21159893 A JP 21159893A JP 21159893 A JP21159893 A JP 21159893A JP H0762434 A JPH0762434 A JP H0762434A
- Authority
- JP
- Japan
- Prior art keywords
- temperature
- grain size
- primary recrystallized
- average primary
- annealing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Links
Landscapes
- Manufacturing Of Steel Electrode Plates (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21159893A JPH0762434A (ja) | 1993-08-26 | 1993-08-26 | 方向性電磁鋼板の一次再結晶粒径制御方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21159893A JPH0762434A (ja) | 1993-08-26 | 1993-08-26 | 方向性電磁鋼板の一次再結晶粒径制御方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0762434A true JPH0762434A (ja) | 1995-03-07 |
| JPH0762434A5 JPH0762434A5 (enExample) | 1998-10-20 |
Family
ID=16608419
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP21159893A Ceased JPH0762434A (ja) | 1993-08-26 | 1993-08-26 | 方向性電磁鋼板の一次再結晶粒径制御方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0762434A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN117778704A (zh) * | 2023-12-15 | 2024-03-29 | 同济大学 | 一种基于在线铁损检测的电工钢机械性能在线控制方法 |
| CN119351680A (zh) * | 2024-09-11 | 2025-01-24 | 江阴兴澄特种钢铁有限公司 | 一种低碳齿轮钢材温锻或热锻后消除锻件混晶的热处理工艺 |
-
1993
- 1993-08-26 JP JP21159893A patent/JPH0762434A/ja not_active Ceased
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN117778704A (zh) * | 2023-12-15 | 2024-03-29 | 同济大学 | 一种基于在线铁损检测的电工钢机械性能在线控制方法 |
| CN119351680A (zh) * | 2024-09-11 | 2025-01-24 | 江阴兴澄特种钢铁有限公司 | 一种低碳齿轮钢材温锻或热锻后消除锻件混晶的热处理工艺 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP2025767B2 (en) | Process for producing grain-oriented electrical steel sheet with high magnetic flux density | |
| US12644164B2 (en) | Production method for grain-oriented electrical steel sheet | |
| JP2519615B2 (ja) | 磁気特性の優れた方向性電磁鋼板の製造方法 | |
| JP2005226111A (ja) | 磁気特性に優れた一方向性電磁鋼板の製造方法 | |
| JP2000129352A (ja) | 磁束密度の高い一方向性電磁鋼板の製造方法 | |
| JPH10140297A (ja) | 高磁束密度方向性電磁鋼板用一次再結晶焼鈍板 | |
| JP2003041320A (ja) | 鉄損の良好な鏡面方向性電磁鋼板の製造方法 | |
| JP2826903B2 (ja) | グラス被膜の良好な高磁束密度方向性電磁鋼板の製造方法 | |
| JP6946846B2 (ja) | 方向性電磁鋼板の製造方法 | |
| KR100940720B1 (ko) | 자기특성이 우수한 방향성 전기강판의 제조방법 | |
| JP4268277B2 (ja) | 一方向性電磁鋼板の製造方法 | |
| JPH06256847A (ja) | 磁気特性の優れた一方向性電磁鋼板の製造方法 | |
| JPH10273727A (ja) | 高磁束密度一方向性電磁鋼板の製造方法 | |
| JP7670948B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JPH07305116A (ja) | 高磁束密度一方向性電磁鋼板の製造方法 | |
| JPH10219359A (ja) | 方向性電磁鋼板の脱炭焼鈍の管理方法 | |
| JP2580403B2 (ja) | 一方向性電磁鋼板用連続鋳造スラブの熱間圧延方法 | |
| JPH04346622A (ja) | 磁気特性の優れた方向性電磁鋼板の製造方法 | |
| JP3072401B2 (ja) | 磁気特性、被膜特性の優れた方向性電磁鋼板の製造方法 | |
| JP6946847B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JP3885264B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JPH0673509A (ja) | 磁気特性の優れた一方向性電磁鋼板及びその製造方法 | |
| JP4021503B2 (ja) | 方向性電磁鋼板の1次再結晶粒径制御方法 | |
| JPH05255753A (ja) | 無方向性電磁鋼板の製造方法 | |
| JP2003268452A (ja) | 磁気特性の良好な鏡面方向性電磁鋼板の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A02 | Decision of refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A02 Effective date: 20010313 |