JPH07135020A - ニッケル電極を備えたアルカリ蓄電池の製造方法 - Google Patents

ニッケル電極を備えたアルカリ蓄電池の製造方法

Info

Publication number
JPH07135020A
JPH07135020A JP5281138A JP28113893A JPH07135020A JP H07135020 A JPH07135020 A JP H07135020A JP 5281138 A JP5281138 A JP 5281138A JP 28113893 A JP28113893 A JP 28113893A JP H07135020 A JPH07135020 A JP H07135020A
Authority
JP
Japan
Prior art keywords
nickel
electrode
storage battery
battery
alkaline storage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP5281138A
Other languages
English (en)
Japanese (ja)
Other versions
JPH07135020A5 (enExample
Inventor
Hajime Konishi
始 小西
Takashi Yao
剛史 八尾
Michio Ito
道雄 伊藤
Michiyo Akimoto
道代 秋元
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Holdings Corp
Original Assignee
Matsushita Electric Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Matsushita Electric Industrial Co Ltd filed Critical Matsushita Electric Industrial Co Ltd
Priority to JP5281138A priority Critical patent/JPH07135020A/ja
Publication of JPH07135020A publication Critical patent/JPH07135020A/ja
Publication of JPH07135020A5 publication Critical patent/JPH07135020A5/ja
Pending legal-status Critical Current

Links

Classifications

    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10—Energy storage using batteries
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P70/00—Climate change mitigation technologies in the production process for final industrial or consumer products
    • Y02P70/50—Manufacturing or production processes characterised by the final manufactured product

Landscapes

  • Secondary Cells (AREA)
  • Battery Electrode And Active Subsutance (AREA)
JP5281138A 1993-11-10 1993-11-10 ニッケル電極を備えたアルカリ蓄電池の製造方法 Pending JPH07135020A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP5281138A JPH07135020A (ja) 1993-11-10 1993-11-10 ニッケル電極を備えたアルカリ蓄電池の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP5281138A JPH07135020A (ja) 1993-11-10 1993-11-10 ニッケル電極を備えたアルカリ蓄電池の製造方法

Publications (2)

Publication Number Publication Date
JPH07135020A true JPH07135020A (ja) 1995-05-23
JPH07135020A5 JPH07135020A5 (enExample) 1999-01-22

Family

ID=17634900

Family Applications (1)

Application Number Title Priority Date Filing Date
JP5281138A Pending JPH07135020A (ja) 1993-11-10 1993-11-10 ニッケル電極を備えたアルカリ蓄電池の製造方法

Country Status (1)

Country Link
JP (1) JPH07135020A (enExample)

Similar Documents

Publication Publication Date Title
JP2730121B2 (ja) アルカリ二次電池およびその製造方法
JP3097347B2 (ja) ニッケル・水素蓄電池
JP4747233B2 (ja) アルカリ蓄電池
JPH0447676A (ja) 密閉型蓄電池の製造法
JP2001266867A (ja) アルカリ蓄電池とそれに用いるアルカリ蓄電池用正極
JP3156485B2 (ja) アルカリ蓄電池用ニッケル極
JPH08264174A (ja) 水素貯蔵合金陰極およびその製造方法
JP2926732B2 (ja) アルカリ二次電池
JP3048953B2 (ja) 非水電解質二次電池
JP3182790B2 (ja) 水素吸蔵合金電極およびその製造法
JP4531874B2 (ja) ニッケル・金属水素化物電池
JP3384109B2 (ja) ニッケル極板
JPH06333568A (ja) 密閉型金属酸化物−水素電池およびその製造方法
JP3136688B2 (ja) ニッケル−水素蓄電池
JP2568967B2 (ja) 密閉型ニッケル−水素二次電池の製造方法
JPH0465067A (ja) ニッケル―水素蓄電池の化成法
JPS6097560A (ja) 密閉形アルカリ蓄電池
JP3490858B2 (ja) アルカリ蓄電池用非焼結式カドミウム負極
JPH04237951A (ja) アルカリ蓄電池用ニッケル極の製造法
JPH04163861A (ja) 非水電解質二次電池
JPS6220258A (ja) 密閉形ニツケル−カドミウム蓄電池
JPH0620717A (ja) 密閉形ニッケル−カドミウム蓄電池の製造法
JPH0737587A (ja) アルカリ蓄電池用の非焼結式ニッケル極
JP2005183339A (ja) アルカリ蓄電池用ニッケル極及びアルカリ蓄電池
JPH07130369A (ja) 電池用電極