JPH07130503A - セラミック抵抗体の製造法 - Google Patents
セラミック抵抗体の製造法Info
- Publication number
- JPH07130503A JPH07130503A JP5274057A JP27405793A JPH07130503A JP H07130503 A JPH07130503 A JP H07130503A JP 5274057 A JP5274057 A JP 5274057A JP 27405793 A JP27405793 A JP 27405793A JP H07130503 A JPH07130503 A JP H07130503A
- Authority
- JP
- Japan
- Prior art keywords
- mol
- resistor
- resistance
- average particle
- sio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Non-Adjustable Resistors (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5274057A JPH07130503A (ja) | 1993-11-02 | 1993-11-02 | セラミック抵抗体の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5274057A JPH07130503A (ja) | 1993-11-02 | 1993-11-02 | セラミック抵抗体の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH07130503A true JPH07130503A (ja) | 1995-05-19 |
| JPH07130503A5 JPH07130503A5 (enExample) | 1999-05-21 |
Family
ID=17536371
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP5274057A Pending JPH07130503A (ja) | 1993-11-02 | 1993-11-02 | セラミック抵抗体の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH07130503A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2012083562A1 (zh) * | 2010-12-24 | 2012-06-28 | 海洋王照明科技股份有限公司 | 一种导电膜及其制备方法和应用 |
| CN108395241A (zh) * | 2018-03-23 | 2018-08-14 | 电子科技大学 | 一种低阻氧化锌陶瓷的制备方法 |
-
1993
- 1993-11-02 JP JP5274057A patent/JPH07130503A/ja active Pending
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2012083562A1 (zh) * | 2010-12-24 | 2012-06-28 | 海洋王照明科技股份有限公司 | 一种导电膜及其制备方法和应用 |
| US20130248780A1 (en) * | 2010-12-24 | 2013-09-26 | Mingjie Zhou | Electrically conductive film, preparation method and application therefor |
| CN108395241A (zh) * | 2018-03-23 | 2018-08-14 | 电子科技大学 | 一种低阻氧化锌陶瓷的制备方法 |
| CN108395241B (zh) * | 2018-03-23 | 2021-02-05 | 电子科技大学 | 一种低阻氧化锌陶瓷的制备方法 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP1122211B1 (en) | PTC composite material | |
| JPS63136603A (ja) | 電圧非直線抵抗体の製造方法 | |
| US6300862B1 (en) | PTC composite material | |
| CA2231855C (en) | Composite ptc material | |
| JPH08259317A (ja) | セラミック抵抗体及びその製造法 | |
| JP3340643B2 (ja) | コンポジットptc材料 | |
| JPH06101401B2 (ja) | 直線抵抗体 | |
| JP3340644B2 (ja) | コンポジットptc材料 | |
| JP2816258B2 (ja) | 電圧非直線抵抗体の製造方法および避雷器 | |
| JP2985619B2 (ja) | 電圧非直線抵抗体の製造方法並びに避雷器 | |
| JPH0541302A (ja) | バルク型直線抵抗体およびその製造方法 | |
| JP2001326108A (ja) | 電圧非直線抵抗体およびその製造方法 | |
| JP3289599B2 (ja) | 酸化亜鉛バリスタの製造方法 | |
| JP2000307158A (ja) | 熱電材料の製造方法 | |
| JP2001114563A (ja) | セラミック抵抗体及びその製造方法 | |
| JPH08102404A (ja) | セラミック抵抗体 | |
| JP2786367B2 (ja) | ガス絶縁遮断器 | |
| JP2777009B2 (ja) | 中性点接地抵抗器 | |
| JPS59169104A (ja) | 金属酸化物非直線抵抗体の製造方法 | |
| JPH05205909A (ja) | バリスタ及びその製造方法 | |
| JPH06181102A (ja) | Ptc抵抗体の製造方法 | |
| JP3256673B2 (ja) | 電力用抵抗体 | |
| JP2002305105A (ja) | 電圧非直線抵抗体の製造方法 | |
| JPH03159201A (ja) | 酸化物抵抗体 | |
| JPH11121203A (ja) | 限流素子の製造方法 |